Investigations on microstructure and mechanical properties of cast Mg-Gd-Y-Zn-Zr-Nd alloy

被引:22
作者
Dang, Cong [1 ]
Dou, Xiaoxu [1 ]
Wang, Jingfeng [1 ]
Yu, Di [1 ]
Wang, Jinxing [1 ]
Lu, Ruopeng [2 ]
Hou, Hua [2 ,3 ]
Zhao, Yuhong [2 ]
机构
[1] Chongqing Univ, Coll Mat Sci & Engn, Natl Engn Res Ctr Magnesium Alloys, Chongqing 400044, Peoples R China
[2] North Univ China, Coll Mat Sci & Engn, Taiyuan 030051, Peoples R China
[3] Taiyuan Univ Sci & Technol, Coll Mat Sci & Engn, Taiyuan 030024, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2023年 / 24卷
关键词
Mg-Gd-Y-Zn-Zr-Nd alloy; Heat treatment; Precipitates; LPSO phase; Mechanical properties; STACKING ORDERED PHASE; MAGNESIUM SINGLE-CRYSTALS; AGE-HARDENING RESPONSE; HIGH-STRENGTH; HEAT-TREATMENT; TENSILE PROPERTIES; BEHAVIOR; EVOLUTION; PRECIPITATION; MORPHOLOGY;
D O I
10.1016/j.jmrt.2023.04.089
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Different solution treatments were carried out on the semi-continuously cast Mg-9.55Gd-2.27Y-1.28Zn-0.55Zr-0.11Nd (wt.%) alloy at temperatures of 480 & DEG;C, 500 & DEG;C, and 520 & DEG;C. It was found that the different solution treatment temperatures led to different phase con-stitutions of the alloy. The Mg3RE-type eutectic phases transform into long period stacking order (LPSO) phases with various morphologies after solution treatment. Increasing the solution temperature resulted in larger grain size, greater number of lamellar LPSO phases, and segregation of Zr element. Block LPSO phases also shifted to rod LPSO phase. After ageing treatment, the special spatial structure consisting of prismatic b' precipitates, basal g' precipitates, and lamellar LPSO phases hindered dislocation movement effectively, leading to high strength. However, the accumulation of massive dislocations promoted the premature formation of cracks at the grain boundary and LPSO/Mg matrix interface, resulting in a rapid decrease in ductility of the alloy. After solution treatment at 480 & DEG;C for 12 h and aged at 200 & DEG;C for 48 h, the Mg-9.55Gd-2.27Y-1.28Zn-0.55Zr-0.11Nd alloy exhibited favorable comprehensive mechanical properties at room temperature: ultimate tensile strength (UTS) of 383 MPa, tensile yield strength (TYS) of 269 MPa, and fracture elongation (EL) of 5.1%. & COPY; 2023 Published by Elsevier B.V. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).
引用
收藏
页码:4852 / 4862
页数:11
相关论文
共 50 条
[31]   Regulating microstructure and mechanical properties of the as-cast Mg-4Zn-0.5Y-0.5Nd alloy by heat treatment [J].
Zhao, Chaochao ;
Wen, Min ;
Wang, Jian ;
Xu, Daokui ;
Zheng, Yufeng ;
Sheng, Liyuan .
JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1010
[32]   Effect of Nd on microstructure and mechanical properties of Mg-7Gd-0.5Zr alloy [J].
Wang, Linghao ;
Jalar, Azman ;
Dan, Longhong .
JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 936
[33]   Effect of Nd on Microstructure and High-Temperature Mechanical Properties of As-cast Mg-Y-Nd-Zn-Zr Alloy [J].
Wang, Tao ;
Fu, Yuanke ;
Wang, Haojie ;
Feng, Yicheng ;
Guo, Erjun .
TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2024, 77 (09) :2857-2866
[34]   Effects of Nd or Zr Addition on Microstructure and Mechanical Properties of As-Cast Mg-Zn-Y Alloy [J].
Chen, Ti Jun ;
Zhang, Da Hua ;
Wang, Wei ;
Ma, Ying ;
Hao, Yuan .
MATERIALS TRANSACTIONS, 2016, 57 (08) :1287-1295
[35]   Effect of Zn addition on microstructure and mechanical properties of Mg-3Y-2Nd-0.5Zr alloy [J].
He, Fei-yu ;
Hu, Wen-xin ;
Liu, Li-juan ;
Ma, Shao-bo ;
He, Wei .
CHINA FOUNDRY, 2023, 20 (04) :299-306
[36]   Effect of Zn Addition on the Microstructure and Mechanical Properties of Cast Mg-10Gd-3.5Er-xZn-0.5Zr Alloys [J].
Zhang, Qiu ;
Liu, Wencai ;
Wu, Guohua ;
Zhang, Liang ;
Ding, Wenjiang .
ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2020, 33 (11) :1505-1517
[37]   Microstructure and mechanical properties of Mg-Gd-Y-Zn-Zr alloy after resistance butt welding [J].
Chen, Mingyang ;
Zhang, Yaqiao ;
Wang, Liqing ;
Ma, Kai ;
Wei, Shouzheng ;
Zhang, Dongdong ;
Li, Yunlong ;
Zhang, Zhen ;
Zhao, Zhanyong ;
Bai, Peikang .
JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1014
[38]   Effect of extrusion parameters on microstructure and mechanical properties of Mg-7.5Gd-2.5Y-3.5Zn-0.9Ca-0.4Zr (wt%) alloy [J].
Xu, C. ;
Nakata, T. ;
Qiao, X. G. ;
Jiang, H. S. ;
Sun, W. T. ;
Chi, Y. C. ;
Zheng, M. Y. ;
Kamado, S. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 685 :159-167
[39]   Effects of Passes on Microstructure Evolution and Mechanical Properties of Mg-Gd-Y-Zn-Zr Alloy During Multidirectional Forging [J].
Li, Bing ;
Teng, Bu-Gang ;
Luo, De-Gao .
ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2018, 31 (10) :1009-1018
[40]   Effect of heat treatment on mechanical properties and microstructure evolution of Mg-9.5Gd-4Y-2.2Zn-0.5Zr alloy [J].
Zheng, Jie ;
Yan, Zhaoming ;
Ji, Jinsheng ;
Shi, Yusha ;
Zhang, Heng ;
Zhang, Zhimin ;
Xue, Yong .