Fatigue resistance of rib-to-bimetallic steel deck welded joints in orthotropic steel bridge decks

被引:12
作者
Liao, Xiaowei [1 ]
Wei, Hanlin [1 ]
Pan, Hongyang [1 ]
Li, Hai-Ting [2 ]
Sun, Bo [1 ]
Xin, Haohui [3 ]
机构
[1] Zhejiang Univ Technol, Coll Civil Engn, Hangzhou 310023, Peoples R China
[2] Shanghai Jiao Tong Univ, Dept Civil Engn, Key Lab Digital Maintenance Bldg & Infrastruct, 800 Dongchuan Rd, Shanghai 200240, Peoples R China
[3] Xi An Jiao Tong Univ, Dept Civil Engn, Xian 710049, Peoples R China
基金
中国国家自然科学基金;
关键词
Orthotropic steel deck; Stainless-clad bimetallic steel; Rib-to-deck joint; Fatigue test; Crack propagation simulation; STRESS-ANALYSES; CRACK-GROWTH; PERFORMANCE; BEHAVIOR;
D O I
10.1016/j.tws.2023.111318
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The stainless-cladding techniques have been applied in the top plate of the orthotropic steel decks in the highspeed railway steel bridges to improve the corrosion and wear resistance. The rib-to-deck (RD) welded joint with the stainless-clad bimetallic steel deck plate becomes a new critical fatigue detail. This study firstly examines the fatigue performance of this full-scale new RD joint through six high-cycle constant-amplitude fatigue tests and two beach-mark tests under eccentric over-rib loading. The structural hot-spot stress at the weld toe on the deck plate is obtained by strain gauges and the linear extrapolation method for each RD specimen before the cyclic loading. Experimental results indicate that five RD specimens suffer from the toe-deck failure modes, while the rests encounter root-deck cracking. The fatigue strength of these new RD joints satisfies the FAT100 hot-spot stress S-N curve based on the IIW design recommendation. Numerical simulation is further conducted to investigate the effect of different cracking modes and welding technologies on the fatigue crack propagation behavior of this new RD joint. Root-deck cracking mode shows weakly higher fatigue resistance than the toe-deck failure case. Using the double-side welds between the U-rib and deck plate, and the thickened-edge U-rib technology can slightly enhance the fatigue life in terms of toe-deck cracking mode in contrast with the traditional single-side groove welds. Experimental and numerical validation quantify the excellent fatigue performance of this new RD joint in comparison with the other types of RD welded joints.
引用
收藏
页数:10
相关论文
共 43 条
[1]  
[Anonymous], 2019, ISO 6892-1:2019
[2]  
[Anonymous], 2015, Q/CR 9211, Code for Fabrication of Railway Steel Bridge
[3]   Crack growth resistance of MAG butt-welded joints of S355JR construction steel [J].
Benedetti, M. ;
Fontanari, V. ;
Santus, C. .
ENGINEERING FRACTURE MECHANICS, 2013, 108 :305-315
[4]   Experimental study on fatigue failure of rib-to-deck welded connections in orthotropic steel bridge decks [J].
Cheng, Bin ;
Ye, Xinghan ;
Cao, Xinger ;
Mbako, Dibu Dave ;
Cao, Yishan .
INTERNATIONAL JOURNAL OF FATIGUE, 2017, 103 :157-167
[5]   Fatigue strength and crack growth of double-side welded rib-to-deck joint in orthotropic steel decks [J].
Cui, Chuang ;
Ma, Yan ;
Zhang, Qing-hua ;
Da, Le-tian ;
Han, Shao-hui .
JOURNAL OF CONSTRUCTIONAL STEEL RESEARCH, 2022, 196
[6]  
Fu Y.G., 2016, Eng. Mech., V33, P131
[7]  
[傅宇光 Fu Yuguang], 2016, [工程力学, Engineering Mechanics], V33, P93
[8]   Fatigue Performance of Roof and U-Rib Weld of Orthotropic Steel Bridge Deck with Different Penetration Rates [J].
Fu, Zhongqiu ;
Ji, Bohai ;
Zhang, Chengyi ;
Wang, Qiudong .
JOURNAL OF BRIDGE ENGINEERING, 2017, 22 (06)
[9]   Fatigue Performance of Rib-to-Deck Joints in Orthotropic Steel Decks with Thickened Edge U-Ribs [J].
Heng, Junlin ;
Zheng, Kaifeng ;
Gou, Chao ;
Zhang, Yu ;
Bao, Yi .
JOURNAL OF BRIDGE ENGINEERING, 2017, 22 (09)
[10]  
Hibbit M, 2012, ABAQUS/Standard User's Manual