Effect of Ti-Cr filler on microstructure, mechanical properties, and thermal shock resistance of TZM/graphite brazed joints

被引:2
作者
Liu, Dong-Guang [1 ,3 ,4 ]
Zou, Jin-Xin [1 ,2 ,5 ]
Zhang, Peng [1 ,2 ]
Zhou, Si-Wei [1 ,2 ]
Liu, Hui [1 ,2 ]
Li, Ze-Qun [1 ,2 ]
机构
[1] Hefei Univ Technol, Anhui Prov Key Lab Aerosp Struct Parts Forming Tec, Ind & Equipment Technol, Hefei 230009, Peoples R China
[2] Hefei Univ Technol, Sch Mat Sci & Engn, Hefei 230009, Peoples R China
[3] Anhui YaLan Seal Component Co Ltd, Chuzhou 233200, Peoples R China
[4] Fujian Univ Technol, Fujian Prov Key Lab Adv Mat Proc & Applicat, Fuzhou 350118, Peoples R China
[5] Hefei Univ Technol, Intelligent Mfg Inst, Hefei 230009, Peoples R China
基金
安徽省自然科学基金; 中国国家自然科学基金;
关键词
Titanium zirconium molybdenum alloy; Graphite; Brazing; Ti-40Cr filler; Microstructure; MOLYBDENUM ALLOY; W-RE; TEMPERATURE; COMPOSITES; BEHAVIOR; COPPER; DAMAGE; TZM; CT; TUNGSTEN;
D O I
10.1016/j.ijrmhm.2023.106310
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The objective of this work was to braze titanium zirconium molybdenum(TZM) alloy and graphite with Ti-40Cr filler in order to explore its practical application on computed tomography tube target. The brazed joints' microstructure, mechanical properties, and thermal shock properties were characterized by X-ray diffraction, scanning electron microscopy, and a 3D laser confocal measuring microscope. The results indicated that the interface microstructure of TZM/graphite brazed joints was graphite/Cr3C2/TiC/Ti-Cr(Mo)/Ti-Mo(Cr)/TZM, and the thickness of the brazing seam increases with increasing temperature. In contrast, the thickness of the carbide reaction layer near the graphite side gradually becomes thicker. The shear tests showed that the joint's strength increased with the temperature increase in a specific temperature range. Maximum shear strength of 26.5 MPa was reached when the joint with groove structure brazed at 1480 degrees C. The effect of holding time on the joints was similar to that of temperature, but the thickness of the carbide reaction layer did not change with holding time. The optimal brazing process for TZM/Ti-40Cr/graphite brazed joints was to hold for 20 min at 1480 degrees C. TZM/Ti40Cr/graphite brazed joints were subjected to a laser thermal shock test. The results indicated that TZM/Ti40Cr/ graphite brazed joints would not cause serious damage when subjected to 20A laser beam current. When the current rose to 40A, the joints will be broken down by the laser, and the damage depth reached -254.824 & mu;m.
引用
收藏
页数:10
相关论文
共 47 条
  • [11] Study of the microstructure and thermomechanical properties of Mo/graphite joint brazed with Ti-Zr-Nb-Be powder filler metal
    Fedotov, Ivan
    Suchkov, Alexey
    Sliva, Andrey
    Dzhumaev, Pavel
    Kozlov, Ilya
    Svetogorov, Roman
    Bachurina, Diana
    Sevryukov, Oleg
    [J]. JOURNAL OF MATERIALS SCIENCE, 2021, 56 (19) : 11557 - 11568
  • [12] Computed Tomography Imaging in Oncology
    Forrest, Lisa J.
    [J]. VETERINARY CLINICS OF NORTH AMERICA-SMALL ANIMAL PRACTICE, 2016, 46 (03) : 499 - +
  • [13] Phase-contrast THz-CT for non-destructive testing
    Fosodeder, Peter
    Hubmer, Simon
    Ploier, Alexander
    Ramlau, Ronny
    van Frank, Sandrine
    Rankl, Christian
    [J]. OPTICS EXPRESS, 2021, 29 (10) : 15711 - 15723
  • [14] Molecular dynamics simulations of high-energy radiation damage in W and W-Re alloys
    Fu, Jun
    Chen, Yangchun
    Fang, Jingzhong
    Gao, Ning
    Hu, Wangyu
    Jiang, Chao
    Zhou, Hong-Bo
    Lu, Guang-Hong
    Gao, Fei
    Deng, Huiqiu
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2019, 524 : 9 - 20
  • [15] Viability study and mechanical characterisation of copper-graphite electrical contacts produced by adhesive joining
    García-Márquez, JM
    Antón, N
    Jimenez, A
    Madrid, M
    Martinez, MA
    Bas, JA
    [J]. JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2003, 143 : 290 - 293
  • [16] Characterization of alumina-alumina/graphite/monel superalloy brazed joints
    Ghosh, S.
    Chakraborty, R.
    Dandapat, N.
    Pal, K. S.
    Datta, S.
    Basu, D.
    [J]. CERAMICS INTERNATIONAL, 2012, 38 (01) : 663 - 670
  • [17] One-step preparation, microstructure and properties of WRe/TZM gradient material for X-ray tube of CT scanner
    Han, Cuiliu
    Yang, Xinyu
    Nong, Binrong
    Zhu, Zhongwen
    Zhang, Jiuxing
    [J]. JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2021, 15 : 2646 - 2657
  • [18] High temperature fatigue characteristics of P/M and hot-forged W-Re and TZM for X-ray target of CT scanner
    Harimon, Mohd Azhar
    Miyashita, Yukio
    Otsuka, Yuichi
    Mutoh, Yoshiharu
    Yamamoto, Shinichi
    [J]. MATERIALS & DESIGN, 2018, 137 : 335 - 344
  • [19] The effects of processing variables on strength of carbon bonding between carbon/carbon composites
    Hatta, Hiroshi
    Koyama, Masashi
    Bando, Takamasa
    Kogo, Yasuo
    Fukuda, Hiroshi
    Ishida, Hatsuo
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 513-14 : 138 - 144
  • [20] He Z.L., 2022, INT J CLIN PRACT, V76, P1