Investigation of Individual and Synergistic Effects of Salinity and Temperature on CO2 Corrosion Performance of Low Carbon API N80 Steel

被引:1
|
作者
Hoomehr, B. [1 ]
Pakshir, M. [2 ]
Rahsepar, M. [2 ]
机构
[1] Isfahan Univ Technol, Dept Mat Engn, Esfahan, Iran
[2] Shiraz Univ, Sch Engn, Dept Mat Sci & Engn, Shiraz, Iran
关键词
CO2; corrosion; electrochemical technique; low carbon steel; qualitative analysis; quantitative analysis; weight loss method; EROSION-CORROSION; BEHAVIOR; CALCIUM;
D O I
10.1007/s11665-022-07439-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The simultaneous presence of CO2-saturated water with natural oil in the transmission pipeline system, often made from steel, is inevitable. Therefore, in the present study, three brine salinities (low salinity, medium salinity, and high salinity) and six different temperatures (35, 45, 55, 65, 75, 85 degrees C) in CO2-saturated brines containing NaCl, CaCl2, MgCl2, Na2SO4 and KCl were employed to study the individual and synergistic effects of brine salinity and temperature on CO2 corrosion of low carbon API N80 steel. According to Tafel polarization tests results, in the 35-65 degrees C temperature range, increasing the brine salinity resulted in a decrease in the corrosion rate; however, from 65 to 85 degrees C, by increasing the salinity from low to high, the corrosion rate increased. In all brine salinities, increasing the temperature resulted in the corrosion rate enhancement to a maximum value and then a decrease was observed. Electrochemical impedance spectroscopy and Tafel tests results agreed. Weight loss method was also performed to validate the electrochemical technique and the results confirmed the electrochemical data. According to the quantitative analysis (using the analysis of variance experimental design method), the synergistic action of salt concentration and temperature was higher than the individual action of them and among temperature and salt concentration, the most influential parameter was temperature. Furthermore, according to qualitative analysis results, which was used to predict the direction of variations, the synergistic effect of temperature and salt concentration in all 6 temperatures and both medium and high salt concentrations was accelerating.
引用
收藏
页码:4643 / 4654
页数:12
相关论文
共 50 条
  • [21] Insight into polymer concentration, temperature, CO2 content, and Cl- content on corrosion of N80 steel tubing in polymer flooding
    Dong, Baojun
    Zeng, Dezhi
    Favero, Cedrick
    Divers, Thomas
    Boisse, Nicolas
    Xu, Qinglin
    Ling, Jing
    Xie, Kemin
    Wang, Qizhen
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2023, 74 (06): : 943 - 961
  • [22] Influence of CO2 partial pressure and flow rate on the corrosion behavior of N80 steel in 3.5% NaCl
    Chen, Xuezhong
    Yang, Xiaomin
    Zeng, Mingyou
    Wang, Hu
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2023, 18 (08):
  • [23] Modeling and experimental study on the effects of temperature on the corrosion of API carbon steel in CO2-Saturated environment
    Elgaddafi, Rida
    Ahmed, Ramadan
    Osisanya, Samuel
    JOURNAL OF PETROLEUM SCIENCE AND ENGINEERING, 2021, 196
  • [24] The Corrosion Behavior of N80 Steel in Multiple Thermal Fluid Environment Containing O2 and CO2
    Lin, Xueqiang
    Luo, Xiaokang
    Liu, Wei
    Chen, Yufan
    Pang, Bo
    Guo, Yi
    He, Qingkun
    FRONTIERS IN MATERIALS, 2021, 8
  • [25] Galvanic corrosion between N80 carbon steel and 13Cr stainless steel under supercritical CO2 conditions
    Li, Y. Y.
    Wang, Z. Z.
    Guo, X. P.
    Zhang, G. A.
    CORROSION SCIENCE, 2019, 147 : 260 - 272
  • [26] Effect of temperature on CO2 corrosion of carbon steel
    Yin, Z. F.
    Feng, Y. R.
    Zhao, W. Z.
    Bai, Z. Q.
    Lin, G. F.
    SURFACE AND INTERFACE ANALYSIS, 2009, 41 (06) : 517 - 523
  • [27] Inhibition of Carbon Steel CO2 Corrosion in High Salinity Solutions
    Kina, A. Y.
    Ponciano, J. A. C.
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2013, 8 (12): : 12600 - 12612
  • [28] Mannich Base as Corrosion Inhibitors for N80 Steel in a CO2 Saturated Solution Containing 3 wt % NaCl
    Tang, Mingjin
    Li, Jianbo
    Li, Zhida
    Fu, Luoping
    Zeng, Bo
    Lv, Jie
    MATERIALS, 2019, 12 (03)
  • [29] Unveiling the influential mechanism of O2 on the corrosion of N80 carbon steel under dynamic supercritical CO2 conditions
    Li, Y. Y.
    Jiang, Z. N.
    Zhang, Q. H.
    Lei, Y.
    Wang, X.
    Zhang, G. A.
    CORROSION SCIENCE, 2022, 205
  • [30] Inhibitive effects of inhibitors on the galvanic corrosion between N80 carbon steel and 13Cr stainless steel under dynamic supercritical CO2 conditions
    Wang, Z. Z.
    Li, Y. Y.
    Zhang, G. A.
    CORROSION SCIENCE, 2019, 146 : 121 - 133