Effect of polyethylene glycol on the crystallization, rheology and foamability of poly(lactic acid) containing in situ generated polyamide 6 nanofibrils
被引:8
作者:
Qiao, Yuhui
[1
,2
,3
]
Li, Qian
[3
]
Jalali, Amirjalal
[4
]
Yu, Dongsheng
[1
,2
]
He, Xichan
[1
,2
]
Wang, Xiaofeng
[3
]
Jiang, Jing
[5
]
Min, Zhiyu
[1
]
机构:
[1] Luoyang Inst Sci & Technol, Dept Mat Sci & Engn, Luoyang 471023, Peoples R China
[2] Luoyang Inst Sci & Technol, Henan Prov Int Joint Lab Mat Solar Energy Convers, Luoyang 471023, Peoples R China
[3] Natl Ctr Int Res Micronano Molding Technol, Zhengzhou 450001, Peoples R China
[4] Univ Toronto, Dept Mech & Ind Engn, Microcellular Plast Mfg Lab, Toronto, ON M5S 3G8, Canada
[5] Zhengzhou Univ, Sch Mech & Power Engn, Zhengzhou 450001, Peoples R China
关键词:
poly(lactic acid);
foaming;
microfibrillation;
rheological property;
crystallization;
MECHANICAL-PROPERTIES;
FOAMING BEHAVIOR;
COMPOSITES;
POLYPROPYLENE;
OXIDE;
D O I:
10.1007/s11705-023-2342-8
中图分类号:
TQ [化学工业];
学科分类号:
0817 ;
摘要:
In this study, the rheological properties, crystallization and foaming behavior of poly(lactic acid) with polyamide 6 nanofibrils were examined with polyethylene glycol as a compatibilizer. Polyamide 6 particles were deformed into nanofibrils during drawing. For the 10% polyamide 6 case, polyethylene glycol addition reduced the polyamide 6 fibril diameter from 365.53 to 254.63 nm, owing to the smaller polyamide 6 particle size and enhanced interface adhesion. Rheological experiments revealed that the viscosity and storage modulus of the composites were increased, which was associated with the three-dimensional entangled network of polyamide 6 nanofibrils. The presence of higher aspect ratio polyamide 6 nanofibrils substantially enhanced the melt strength of the composites. The isothermal crystallization kinetics results suggested that the polyamide 6 nanofibrils and polyethylene glycol had a synergistic effect on accelerating poly(lactic acid) crystallization. With the polyethylene glycol, the crystallization half-time reduced from 103.6 to 62.2 s. Batch foaming results indicated that owing to higher cell nucleation efficiency, the existence of polyamide 6 nanofibrils led to a higher cell density and lower expansion ratio. Furthermore, the poly(lactic acid)/polyamide 6 foams exhibited a higher cell density and expansion ratio than that of the foams without polyethylene glycol.
引用
收藏
页码:2074 / 2087