Chemical composition optimization of Al2O3-TiO2 composite coatings for enhanced wear and corrosion resistance

被引:25
作者
Eraslan, Fatma Sezgi [1 ]
Gecu, Ridvan [1 ]
机构
[1] Yildiz Tech Univ, Dept Met & Mat Engn, Istanbul, Turkiye
关键词
Chemical composition; Composite coating; Wear; Corrosion; TIO2; FILMS; MICROSTRUCTURE; PROTECTION; DEPOSITION; BEHAVIOR; STEEL;
D O I
10.1016/j.surfcoat.2023.130053
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
This study aimed to optimize the chemical composition of wear- and corrosion-resistant Al2O3-TiO2 composite coatings. 2-layered and 4-layered Al2O3-TiO2 coatings were fabricated on a 316L substrate with various Al2O3 and TiO2 content (20 %, 35 %, 50 %, 65 %, and 80 % in weight) at 900 degrees C by sol-gel technique. Wear properties were measured by dry sliding tests against an Al2O3 ball, and corrosion behavior was determined through potentiodynamic polarization and electrochemical impedance spectroscopy (EIS) tests. All Al2O3-TiO2 composite coatings consisted of alpha-Al2O3 and rutile phases, regardless of the chemical composition. Increasing TiO2 content significantly increased coating thickness at the same number of layers. The 2-layered configurations resulted in lower wear rates in low-TiO2 compositions, whereas the 4-layered configurations provided higher wear resistance in high TiO2-containing coatings. The high Al2O3 concentration caused extremely high corrosion rates compared to those consisting of high TiO2. Wear and corrosion losses were decreased with increasing TiO2 content due to its nanosized structure, allowing well-adhered, continuous, and less porous coating morphology. The maximum improvement in wear and corrosion resistance was obtained in the 4-layered 65 % TiO2-containing composite coating.
引用
收藏
页数:12
相关论文
共 48 条
  • [1] Deposition of meso-porous γ-alumina coatings on ceramic honeycombs by sol-gel methods
    Agrafiotis, C
    Tsetsekou, A
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2002, 22 (04) : 423 - 434
  • [2] Comparing the phase transformation of continuous alumina fiber and xerogels derived from the same precursor
    Cheng, Ming
    Liu, Wensheng
    Yao, Shuwei
    Wang, Juan
    Ma, Yunzhu
    [J]. JOURNAL OF SOL-GEL SCIENCE AND TECHNOLOGY, 2021, 99 (01) : 169 - 177
  • [3] The effect of calcination temperatures on structural and electrochemical properties of TiO2 film deposited on commercial pure titanium
    Comakli, O.
    Yazici, M.
    Yetim, T.
    Yetim, A. F.
    Celik, A.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2016, 285 : 298 - 303
  • [4] Al2O3-TiO2 composite coatings with enhanced anticorrosion properties for 316L stainless steel
    Dai, Jiamin
    Yang, Jiaqi
    Zhuge, Lanjian
    Wu, Xuemei
    [J]. MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2020, 71 (09): : 1512 - 1520
  • [5] Effect of voltage on microstructure and its influence on corrosion and tribological properties of TiO2 coatings
    Dhiflaoui, Hafedh
    Khlifi, Kaouther
    Barhoumi, Najoua
    Larbi, Ahmed Ben Cheikh
    [J]. JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2020, 9 (03): : 5293 - 5303
  • [6] Low-temperature atomic layer deposition of Al2O3 thin coatings for corrosion protection of steel: Surface and electrochemical analysis
    Diaz, Belen
    Harkonen, Emma
    Swiatowska, Jolanta
    Maurice, Vincent
    Seyeux, Antoine
    Marcus, Philippe
    Ritala, Mikko
    [J]. CORROSION SCIENCE, 2011, 53 (06) : 2168 - 2175
  • [7] Atomic force microscopy study on the anatase crystallization of long term stored Al2O3-TiO2-SiO2 coatings on glass
    Du, YJ
    Frischat, GH
    [J]. JOURNAL OF MATERIALS SCIENCE, 2000, 35 (10) : 2561 - 2564
  • [8] Thermal stability of sputtered Al2O3 coatings
    Edlmayr, V.
    Moser, M.
    Walter, C.
    Mitterer, C.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2010, 204 (9-10) : 1576 - 1581
  • [9] Influence of layer number and sintering temperature on microstructural, tribological, and corrosion behavior of Al2O3-TiO2 multilayer coatings
    Eraslan, Fatma Sezgi
    Turu, Irem Cemre
    Ozcan, Mucahid
    Birol, Burak
    Gecu, Ridvan
    [J]. CERAMICS INTERNATIONAL, 2023, 49 (20) : 33226 - 33235
  • [10] Improving wear and corrosion protection of AISI 304 stainless steel by Al2O3-TiO2 hybrid coating via sol-gel process
    Gecu, Ridvan
    Birol, Burak
    Ozcan, Mucahid
    [J]. TRANSACTIONS OF THE INSTITUTE OF METAL FINISHING, 2022, 100 (06): : 324 - 332