Hygrothermal aging behavior and mechanism of multi-filler reinforced epoxy composites for steel structure coatings

被引:13
|
作者
Tian, Jingwei
Li, Chenggao
Qi, Xiao
Xian, Guijun
机构
[1] Harbin Inst Technol, Minist Educ, Key Lab Struct Dynam Behav & Control, Harbin 150090, Heilongjiang, Peoples R China
[2] Harbin Inst Technol, Minist Ind & Informat Technol, Key Lab Smart Prevent & Mitigat Civil Engn Disast, Harbin 150090, Heilongjiang, Peoples R China
[3] Harbin Inst Technol, Sch Civil Engn, Harbin 150090, Heilongjiang, Peoples R China
基金
中国国家自然科学基金;
关键词
Hygrothermal aging; Coating for steel structure; Moisture uptake; Mechanical properties; Degradation mechanism; Long-term life prediction; WATER-ABSORPTION; DEGRADATION; DIFFUSION; SURFACE; MATRIX; TIME;
D O I
10.1016/j.eurpolymj.2022.111780
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The long-term hygrothermal resistance of epoxy-based composites plays a key role as an anti-corrosion and anti-wear coating for steel structures when exposed to complex service environments. The hygrothermal aging will cause an irreversible damage to the service performances of composites. In the present paper, the multi-fillers reinforced epoxy composites (MFREC) had been successfully prepared and have been given higher expectations for steel coatings. Its hygrothermal aging behavior was experimentally investigated through the immersion in distilled water (DW) and saline water (SW) at 20, 40, and 60 degrees C as long as 120 days. The moisture uptake, thermal properties, mechanical properties and microstructure analysis were tested to evaluate the long-term hygrothermal evolution. The research results showed that the quasi-equilibrium moisture uptake content (3.72%) of MFREC in SW was lower than that (4.14%) in DW owing to the preferential permeation and occupation effects of small ions (Na+, Cl-). Hygrothermal exposure led to a maximum degradation of tensile strength, elongation at break and glass transition temperature of MFREC, up to 38.2%, 46.6% and 20.8% in DW, and 34.5%, 40.8% and 18.4% in SW, respectively. This was because the epoxy matrix had generated relaxation and reinforced-fillers/epoxy interfaces had been destroyed, which can be verified by hydrogen bond increasing (maximum 75.2%) from infrared test, fiber pulling out from epoxy matrix (morphology analysis), elastic modulus decreasing (maximum 37.8%) from micro-hardness measurement and pore volume increasing (maximum 53.9%) from N2 adsorption test compared to unaged samples. Based on the Arrhenius theory, the long-term life prediction of MFREC tensile strength under three typical bridge service environments was conducted to evaluate the service time as coatings. It can be found that the stable strength retentions were 63.19% and 66.03% in the simulated pure water and marine environments, respectively. Furthermore, an additional strength degradation percentage up to 11.5% can be found for MFREC exposed to steel bridge coatings in southern as long as 3 years compared to the northern environment.
引用
收藏
页数:16
相关论文
共 38 条
  • [31] The Effect of Hydrothermal Aging on the Low-Velocity Impact Behavior of Multi-Walled Carbon Nanotubes Reinforced Carbon Fiber/Epoxy Composite Pipes
    Kara, Memduh
    Ak, Safa
    Uyaner, Mesut
    Gunoz, Alper
    Kepir, Yusuf
    APPLIED COMPOSITE MATERIALS, 2021, 28 (05) : 1567 - 1587
  • [32] Effect of multi-walled carbon nano-tube on mechanical behavior of glass laminate aluminum reinforced epoxy composites
    Logesh, K.
    Hariharasakthisudhan, P.
    Rajan, B. Surya
    Moshi, A. Arul Marcel
    Khalkar, V.
    POLYMER COMPOSITES, 2020, 41 (11) : 4849 - 4860
  • [33] Hydrogen permeation behavior and mechanism of multi-layered graphene coatings and mitigation of hydrogen embrittlement of pipe steel
    Shi, Kejun
    Xiao, Shu
    Ruan, Qingdong
    Wu, Hao
    Chen, Guohua
    Zhou, Chilou
    Jiang, Saihua
    Xi, Ke
    He, Mohan
    Chu, Paul K.
    APPLIED SURFACE SCIENCE, 2022, 573
  • [34] Mechanical behavior and failure mechanism of aerogel-reinforced carbon fibre/epoxy composites under quasi-static/impact loading
    Zhou, Zhipeng
    Sun, Weifu
    POLYMER TESTING, 2022, 115
  • [35] Hybrid Treatment and Natural Aging Behavior of Peak-Aged Eutectoid Steel Powder-Reinforced Al 7075 Matrix Composites
    Hegde, Ananda
    Manjunathaiah, Karthik Birur
    Sharma, Sathyashankara
    Chennegowda, Gowrishankar Mandya
    Anne, Gajanan
    Sadanand, Ramakrishna Vikas
    JOURNAL OF COMPOSITES SCIENCE, 2024, 8 (03):
  • [36] Impact behavior and fractographic study of carbon nanotubes grafted carbon fiber-reinforced epoxy matrix multi-scale hybrid composites
    Sharma, S. P.
    Lakkad, S. C.
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2015, 69 : 124 - 131
  • [37] The effect of filler type (tungsten carbide, zinc oxide) and content on the mechanical and wear behavior of jute/flax reinforced epoxy hybrid composites: Experimental and artificial neural network analysis
    Demir, Mehmet Emin
    POLYMER COMPOSITES, 2025,
  • [38] Hygrothermal aging behavior of sandwich-structure Ba0.6Sr0.4TiO3/PVDF composites with high energy storage property and dielectric tunability
    Guo, Yiting
    Liu, Shuhang
    Xu, Xin
    Xu, Jie
    Bulejak, Weronika
    Szafran, Mikolaj
    Gao, Feng
    JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 962