Effect of nanoheterogeneities on the fracture toughness and tensile ductility of CuTa metallic glass thin films

被引:3
作者
Behboud, Ali B. [1 ]
Fadaie, Amir [2 ]
Motallebzadeh, Amir [3 ]
Sehirli, Servet [1 ]
Ozerinc, Sezer [1 ,2 ]
机构
[1] Middle East Tech Univ, Dept Mech Engn, TR-06800 Ankara, Turkiye
[2] Middle East Tech Univ, Dept Micro & Nanotechnol, TR-06800 Ankara, Turkiye
[3] Koc Univ Surface Sci, Technol Ctr KUYTAM, Sarıyer 34450, Rumelifeneri, Istanbul, Turkiye
关键词
Metallic glasses; Thin films; Heterogeneity; Ductility; Fracture toughness; SIZE-INDEPENDENT STRENGTH; MECHANICAL-PROPERTIES; NANOCRYSTALLINE COPPER; BEHAVIOR; DEFORMATION; NANOINDENTATION; STABILIZATION; PLASTICITY; STABILITY; HARDNESS;
D O I
10.1016/j.jallcom.2023.173331
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Nanoheterogenenous metallic glasses (MG) can offer improved ductility through a nanoscale modulation in their mechanical properties. However, the relationship between the modulation parameters and the mechanical behavior is not well understood. Physical vapor deposition can directly control the compositional and morphological parameters of nanoheterogeneous MGs and enables the systematic investigation of this problem. This work explores the microstructure and mechanical properties of a range of CuTa-based nanolayered amorphous/amorphous (A/A) and amorphous/semi-crystalline (A/SC) nanoheterogeneous MGs and MG composites. The first step was the identification of three microstructural regimes in CuTa, namely, a fully amorphous form (23-65 at.% Ta), a Ta-rich amorphous-crystalline composite (65-75 at.% Ta), and a Cu-rich amorphous-crystalline composite (16-23 at.% Ta). The hardness of the films increased from 6 GPa to 17 GPa with increasing Ta content. Next, a range of CuxTa1_ x/CuyTa1_y nanolayers composed of A/A and A/SC nanolayers were investigated. The hardness of all nanolayers follows the rule of mixture. A/A structures do not provide a significant increase in fracture toughness and only a minor increase in tensile ductility despite the high amplitude modulation of hardness between layers. A/SC nanolayers' hardness and toughness was higher than A/A nanolayers as well as monolithic amorphous films, but still remained below the monolithic Cu25Ta75 SC film. The results show that the design of nanoheterogeneities in MGs requires careful optimization to achieve a useful improvement in mechanical properties.
引用
收藏
页数:10
相关论文
共 50 条
  • [1] Nanoheterogeneous ZrTa metallic glass thin films with high strength and toughness
    Behboud, Ali B.
    Motallebzadeh, Amir
    Ozerinc, Sezer
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 901
  • [2] Extrinsic mechanical size effects in thin ZrNi metallic glass films
    Ghidelli, M.
    Gravier, S.
    Blandin, J. -J.
    Djemia, P.
    Mompiou, F.
    Abadias, G.
    Raskin, J. -P.
    Pardoen, T.
    ACTA MATERIALIA, 2015, 90 : 232 - 241
  • [3] Simultaneous enhancement of tensile properties and fracture toughness of bulk metallic glass composites
    Yan, Tingyi
    Zhang, Long
    Yuan, Xudong
    Li, Biao
    Bai, Jianhua
    Fu, Huameng
    Zhang, Hongwei
    Zhang, Haifeng
    ACTA MATERIALIA, 2025, 291
  • [4] A Microbridge Method in Tensile Testing of Substrate for Fracture Toughness of Thin Films
    Zhang, Xiaomin
    Zhang, Sam
    NANOSCIENCE AND NANOTECHNOLOGY LETTERS, 2011, 3 (06) : 735 - 743
  • [5] Scaling of the fracture toughness of freestanding metallic thin films with the yield strength
    Preiss, Eva I.
    Gannott, Florentina
    Goeken, Mathias
    Merle, Benoit
    MATERIALS RESEARCH LETTERS, 2018, 6 (10): : 607 - 612
  • [6] Grain boundary mediated plasticity: A blessing for the ductility of metallic thin films?
    Liebig, Jan P.
    Mackovic, Mirza
    Spiecker, Erdmann
    Goeken, Mathias
    Merle, Benoit
    ACTA MATERIALIA, 2021, 215
  • [7] A maximum in ductility and fracture toughness in nanostructured Cu/Cr multilayer films
    Zhang, J. Y.
    Liu, G.
    Zhang, X.
    Zhang, G. J.
    Sun, J.
    Ma, E.
    SCRIPTA MATERIALIA, 2010, 62 (06) : 333 - 336
  • [8] Effect of environment on tensile ductility and fracture toughness of iron aluminides
    Ko, SH
    Gnanamoorthy, R
    Hanada, S
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1997, 222 (02): : 133 - 139
  • [9] Gradient Confinement Induced Uniform Tensile Ductility in Metallic Glass
    Lu, X. L.
    Lu, Q. H.
    Li, Y.
    Lu, L.
    SCIENTIFIC REPORTS, 2013, 3 : 1 - 5
  • [10] Cold rolling improves the fracture toughness of a Zr-based bulk metallic glass
    Xie, Shenghui
    Kruzic, Jamie J.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 694 : 1109 - 1120