Oxidation and internal nitridation behaviors of a Ni-based superalloy Rene 65 during high-temperature homogenization

被引:8
作者
Zhang, Xian-guang [1 ,2 ]
Chen, Jia-jun [1 ,2 ]
Zhou, Yang [3 ,4 ,5 ]
Shui, Lang [3 ,4 ,5 ]
Xiao, Dong-ping [3 ,4 ,5 ]
Fu, Jian-hui [3 ,4 ,5 ]
Yang, Wen-chao [1 ,2 ]
Liu, Huan [1 ,2 ]
Ren, Ying-jie [1 ,2 ]
Shi, Peng [1 ,2 ]
Zhang, Jian [3 ,4 ,5 ]
机构
[1] Univ Sci & Technol Beijing USTB, State Key Lab Adv Met, Beijing 100083, Peoples R China
[2] Univ Sci & Technol Beijing USTB, Sch Met & Ecol Engn, Beijing 100083, Peoples R China
[3] Chengdu Adv Met Mat Ind Technol Inst Co Ltd, Chengdu 610300, Sichuan, Peoples R China
[4] Iron & State Key Lab Met Mat Marine Equipment & Ap, Anshan 114009, Liaoning, Peoples R China
[5] Pangang Grp Res Inst Co Ltd, Panzhihua 617000, Sichuan, Peoples R China
基金
中国国家自然科学基金;
关键词
Nickel-based superalloy; Homogenization; Oxidation; Kinetics; Internal nitridation; Thermodynamics; SINGLE-CRYSTAL SUPERALLOY; DEGREES-C; MECHANISM; ALLOY; AIR; 1000-DEGREES-C; 900-DEGREES-C; INTERFACE; TITANIUM;
D O I
10.1007/s42243-023-01007-2
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Homogenization heat treatment is a key process to remove the micro-segregation and re-dissolve the undesired phases for wrought superalloy. The oxidation behavior of the wrought superalloy during the high-temperature homogenization process, however, was rarely studied. The oxidation film evolution and growth kinetics of an as-cast superalloy Rene 65 during the homogenization were systematically studied. The oxide film consists of Cr2O3 external oxidation layer and dendritic TiO2 and Al2O3 internal oxidation layer. And the growth kinetics of the oxide film followed a parabolic law. Internal nitridation occurs during the oxidation process, and TiN is apparently formed at the tip of internal oxidation layer. The originally formed TiN can be transformed into TiO2 or retained with the progress of oxidation. Meanwhile, the TiN is newly formed in the deeper matrix at the new oxidation-layer tip. Thermodynamic analyses revealed that there is a competition between the oxidation and nitridation. Nitridation can occur when the partial pressure of nitrogen exceeds the threshold of nitridation and the critical partial pressure ratio of nitrogen and oxygen.
引用
收藏
页码:1622 / 1632
页数:11
相关论文
共 42 条
[1]   THE ROLE OF ALUMINUM AND TITANIUM ON THE OXIDATION PROCESS OF A NICKEL-BASE SUPERALLOY IN STEAM AT 800-DEGREES-C [J].
ABE, F ;
ARAKI, H ;
YOSHIDA, H ;
OKADA, M .
OXIDATION OF METALS, 1987, 27 (1-2) :21-36
[2]   High Temperature Oxidation Behavior of Conventional and Nb-Modified MAR-M246 Ni-Based Superalloy [J].
Alkmin, L. B. ;
Chaia, N. ;
Utada, S. ;
Cormier, J. ;
Baldan, R. ;
Coelho, G. ;
Nunes, C. A. .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2021, 52 (06) :2589-2600
[3]  
Athreya C., 2019, J ALLOY COMPD, V617, P139310567
[4]   High temperature oxidation behavior of Ni-based superalloy GH202 [J].
Cao, Jiangdong ;
Zhang, Junsong ;
Chen, Ruifang ;
Ye, Yunxia ;
Hua, Yinqun .
MATERIALS CHARACTERIZATION, 2016, 118 :122-128
[5]  
Chen JY., 2018, BASIS OPTIMIZED CONT
[6]  
Chen YJ., 2014, SYNTHESIS NANOTITANI
[7]   OXIDATION OF NI-CR-AL ALLOYS BETWEEN 1000 DEGREES AND 1200 DEGREES C [J].
GIGGINS, CS ;
PETTIT, FS .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1971, 118 (11) :1782-&
[8]  
Hao WH, 2015, RARE METAL MAT ENG, V44, P419
[9]  
Heaney JA, 2014, 8TH INTERNATIONAL SYMPOSIUM ON SUPERALLOY 718 AND DERIVATIVES, P67
[10]  
Hu Y.B., 2019, Analysis on the relationship between oxidation kinetics and oxide film structure evolution of the nickel-based superalloy