共 145 条
Impact of microporous ?-Al2O3 on the thermal stability of pre-cast cementitious composite containing glass waste
被引:35
作者:
Mohamed, O. A.
[1
]
Hazem, M. M.
[2
]
Mohsen, Alaa
[3
]
Ramadan, M.
[2
]
机构:
[1] Beni Suef Univ, Fac Postgrad Studies Adv Sci, Environm Sci & Ind Dev Dept, Bani Suwayf, Egypt
[2] Ain Shams Univ, Fac Sci, Chem Dept, Cairo, Egypt
[3] Ain Shams Univ, Fac Engn, Cairo, Egypt
关键词:
Glass waste;
Pre-cast binding materials;
Hydrothermal curing;
Fire resistivity;
Micro-porous gamma alumina;
MECHANICAL-PROPERTIES;
FIRE RESISTANCE;
PORTLAND-CEMENT;
NANO-ALUMINA;
ELEVATED-TEMPERATURE;
MULLITE FORMATION;
GAMMA-ALUMINA;
CONCRETE;
PASTES;
STRENGTH;
D O I:
10.1016/j.conbuildmat.2023.131186
中图分类号:
TU [建筑科学];
学科分类号:
0813 ;
摘要:
Upcycling sodium-rich glass waste (SGW) in fabricating pre-cast binding materials is the main motivation of this work. The impact of different curing regimes on the mechanical resistance of OPC-SGW pastes was investigated: normal curing under tap water as well as hydrothermal treatment at different pressures (3, 6, 9 and 12 bars). Replacing OPC with 50 wt% SGW (Blend-G composite) reduced the compressive strength by 30.9% under normal curing after 28 days, but the strength value was completely close to the OPC reading (68 MPa) under hydro -thermal curing at 9 bars for 4 hrs. According to the fire resistance results, the compressive strength value of autoclaved Blend-G paste was reduced by 87 and 97.4% after firing at 500 and 750 degrees C, respectively. Therefore, it was necessary to search for a radical solution to solve this problem, and consequently, 1 wt% micro-porous gamma alumina nanoparticle (MP-NA) was incorporated into Blend-G to produce Blend-M composite. The MP-NA was prepared by the sol-gel method from low-cost commercial materials. Inclusion of 1 wt% MP-NA (Blend-M) enhanced the strength by 140, 48.4 and 31.9% after 1, 7 and 28 days, respectively and by 22.9% at 9 bars/4hrs than Blend-G. This may be attributed to the super-fine/nucleation effect, pore structure rear-rangement, and high pozzolancity of MP-NA that increased the amount of binding hydrates (CSHs, CASHs, and CAHs), which was detected via XRD, TGA/DSC, and SEM. Moreover, high thermal stability up to 750 degrees C was observed for Blend-M due to the generation of new ceramic phases such as nepheline and Mullite.