Modification of structural, mechanical, corrosion and biocompatibility properties of Ti40Zr10Cu36Pd14 metallic glass by minor Ga and Sn additions

被引:5
|
作者
Lachova, Andrea [1 ]
Stoica, Mihai [2 ]
Michalik, Stefan [3 ]
Gostin, Petre F. [4 ]
Fujioka-Kobayashi, Masako [5 ,6 ]
Schaller, Benoit [5 ]
Loeffler, Joerg F. [2 ]
Sovak, Pavol [1 ]
机构
[1] Pavol J Safarik Univ Kosice, Fac Sci, Dept Condensed Matter Phys, Pk Angelinum 9, Kosice 04154, Slovakia
[2] ETH, Lab Met Phys & Technol, Dept Mat, CH-8093 Zurich, Switzerland
[3] Diamond Light Source Ltd, Harwell Sci & Innovat Campus, Didcot OX11 0DE, Oxon, England
[4] Tech Univ Denmark, Dept Chem & Biochem Engn, DK-2800 Lyngby, Denmark
[5] Univ Bern, Bern Univ Hosp, Inselspital, Dept Craniomaxillofacial Surg, CH-3010 Bern, Switzerland
[6] Nippon Dent Univ Tokyo, Sch Life Dent Tokyo, Dept Oral & Maxillofacial Surg, Tokyo 1028159, Japan
关键词
Metallic glasses; X-ray diffraction; Mechanical properties; Biocompatibility; Titanium; FORMING ABILITY; BEHAVIOR; ALLOY; PLASTICITY; DYNAMICS; ADHESION; MODULUS; CU;
D O I
10.1016/j.jallcom.2023.168776
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Ti40Zr10Cu32Pd14Ga4 and Ti40Zr10Cu32Pd14Sn4 (in at%) bulk metallic glasses (BMGs) with different geome-tries (wedges, rods, ribbons and discs) were prepared by suction casting, melt spinning and splat quenching, respectively. For comparison, the reference Ti40Zr10Cu36Pd14 BMG was cast as a rod with 2 mm diameter and in wedge-shaped form. High-energy X-ray diffraction measurements yielded a critical casting thickness of 2.4, 2.1 and at least 4 mm for the reference, Ga-containing, and Sn-containing BMGs, respectively. The extension of the supercooled liquid region of about 50 K, measured for the glassy rods and ribbons by differential scanning calorimetry, is larger than that of only 20 K found for the splat-quenched discs. As to the alloys' mechanical properties, the Ti40Zr10Cu36Pd14 glassy rods deform plastically in compression up to a strain of 3.8% and possess a Young's modulus of 78 GPa. The Sn-and Ga-containing BMG rods reach respectively a plastic strain of 6.1% and 4.7%, and a Young's modulus of 72 and 63 GPa. Corrosion tests were performed by electrochemical experiments, and the highest pitting resistance was observed for Ti40Zr10Cu32Pd14Sn4 (pitting overpotential eta pit = 446 mV) compared to Ti40Zr10Cu32Pd14Ga4 (379 mV) and Ti40Zr10Cu36Pd14 (183 mV). The results of live/dead assay and cell viability revealed excellent biocompat-ibility for the Ga-containing BMGs.(c) 2023 Elsevier B.V. All rights reserved.
引用
收藏
页数:11
相关论文
共 50 条
  • [1] Properties of the Ti40Zr10Cu36Pd14 BMG Modified by Sn and Nb Additions
    Sypien, Anna
    Stoica, Mihail
    Czeppe, Tomasz
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2016, 25 (03) : 800 - 808
  • [2] Properties of the Ti40Zr10Cu36Pd14 BMG Modified by Sn and Nb Additions
    Anna Sypien
    Mihail Stoica
    Tomasz Czeppe
    Journal of Materials Engineering and Performance, 2016, 25 : 800 - 808
  • [3] The Influence of Partial Replacement of Cu with Ga on the Corrosion Behavior of Ti40Zr10Cu36Pd14 Metallic Glasses
    Wei, Qi
    Gostin, Petre Flaviu
    Addison, Owen
    Reed, Daniel
    Calin, Mariana
    Bera, Supriya
    Ramasamy, Parthiban
    Davenport, Alison
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2019, 166 (14) : C485 - C491
  • [4] Ti40Zr10Cu36Pd14 bulk metallic glass as oral implant material
    Rezvan, Amir
    Sharifikolouei, Elham
    Soprunyuk, Viktor
    Schranz, Wilfried
    Todt, Juraj
    Lassnig, Alice
    Gammer, Christoph
    Sifferlinger, Nikolaus August
    Asci, Atacan
    Okulov, Ilya
    Schlogl, Sandra
    Keckes, Jozef
    Najmi, Ziba
    Cochis, Andrea
    Scalia, Alessandro Calogero
    Rimondini, Lia
    Sarac, Baran
    Eckert, Juergen
    MATERIALS & DESIGN, 2023, 233
  • [5] The Effects of Cooling Rate on the Microstructure and Mechanical Properties of Ti40Zr10Cu36Pd14 Metallic Glass Matrix Composites
    Park, Seon Yong
    Lim, Ka Ram
    Na, Young Sang
    Kim, Seong Eon
    Choi, Youn Suk
    Korean Journal of Metals and Materials, 2016, 54 (11): : 802 - 807
  • [6] Relaxation of Ni-free Ti40Zr10Cu36Pd14 bulk metallic glass under mechanical stress
    Qiao, J. C.
    Wang, Q.
    Pelletier, J. M.
    Yao, Y.
    INTERMETALLICS, 2018, 102 : 6 - 10
  • [7] Antibacterial activity, cytocompatibility, and thermomechanical stability of Ti40Zr10Cu36Pd14 bulk metallic glass
    Rezvan, Amir
    Sharifikolouei, Elham
    Lassnig, Alice
    Soprunyuk, Viktor
    Gammer, Christoph
    Spieckermann, Florian
    Schranz, Wilfried
    Najmi, Ziba
    Cochis, Andrea
    Scalia, Alessandro Calogero
    Rimondini, Lia
    Manfredi, Marcello
    Eckert, Jurgen
    Sarac, Baran
    MATERIALS TODAY BIO, 2022, 16
  • [8] On the Potential of Bulk Metallic Glasses for Dental Implantology: Case Study on Ti40Zr10Cu36Pd14
    Liens, Alethea
    Etiemble, Aurelien
    Rivory, Pascaline
    Balvay, Sandra
    Pelletier, Jean-Marc
    Cardinal, Sandrine
    Fabregue, Damien
    Kato, Hidemi
    Steyer, Philippe
    Munhoz, Tais
    Adrien, Jerome
    Courtois, Nicolas
    Hartmann, Daniel J.
    Chevalier, Jerome
    MATERIALS, 2018, 11 (02)
  • [9] In vitro corrosion and biocompatibility screening of sputtered Ti40Cu36Pd14Zr10 thin film metallic glasses on steels
    Subramanian, B.
    MATERIALS SCIENCE & ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS, 2015, 47 : 48 - 56
  • [10] Insights into the crystallisation pathways in as-cast Ti40Zr10Cu36Pd14 glassy alloys
    Douest, Yohan
    Cazottes, Sophie
    Costa, Miguel B.
    Ter-Ovanessian, Benoit
    Courtois, Nicolas
    Chevalier, Jerome
    Greer, A. Lindsay
    Fabregue, Damien
    MATERIALS CHARACTERIZATION, 2024, 214