Deformation and Fracture Characterization of an Mg-Sn-Ca Alloy Using 3D Processing Maps

被引:4
作者
Zhi, Chenchen [1 ,2 ]
Wu, Zhenyu [1 ]
Lei, Junyi [1 ]
Huang, Zhiquan [1 ,2 ]
Xv, Haijie [3 ]
Zhu, Yanchun [1 ,2 ]
Jia, Weitao [1 ,2 ]
Liu, Pengtao [1 ,2 ]
Ma, Lifeng [1 ,2 ]
机构
[1] Taiyuan Univ Sci & Technol, Coll Mech Engn, Taiyuan 030024, Peoples R China
[2] Taiyuan Univ Sci & Technol, Heavy Machinery Engn Res Ctr, Minist Educ, Taiyuan 030024, Peoples R China
[3] Ningbo Univ, Part Rolling Key Lab Zhejiang Prov, Ningbo 315211, Peoples R China
基金
中国国家自然科学基金;
关键词
processing map; Mg-Sn-Ca; hot deformation; dynamic recrystallization; HOT DEFORMATION; MAGNESIUM ALLOYS; BEHAVIOR; MICROSTRUCTURE; TEMPERATURE;
D O I
10.3390/met13040645
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The deformation and fracture characterization of an Mg-2Sn-1Ca alloy were studied through uniaxial isothermal compression tests. The flow stress curves, the efficiency of power dissipation, the instability parameter and the fracture behavior of an Mg-2Sn-1Ca alloy under the condition of various hot working parameters were investigated according to the experimental data. Processing maps were established by superimposing the instability map over the power dissipation map. It was found that flow stress reduces with increases in the deformation temperature and decreases in the strain rate. The processing of Mg-2Sn-1Ca alloys should avoid the instability region in which the conditions are high strain under high temperature and low strain under low temperature. At 473 K or a high strain rate, unidirectional cracks and fish scale cracks can be produced, and cracks can be avoided under the optimum processing area of 623-723 K/0.001-0.1 s(-1).
引用
收藏
页数:12
相关论文
共 25 条
[11]   The flow behavior and constitutive equation in isothermal compression of FGH4096-GH4133B dual alloy [J].
Liu, Yanhui ;
Yao, Zekun ;
Ning, Yongquan ;
Nan, Yang ;
Guo, Hongzhen ;
Qin, Chun ;
Shi, Zhifeng .
MATERIALS & DESIGN, 2014, 63 :829-837
[12]   The microstructure, creep resistance, and high-temperature mechanical properties of Mg-5Sn alloy with Ca and Sb additions, and aging treatment [J].
Nayyeri, G. ;
Mahmudi, R. ;
Salehi, F. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (21-22) :5353-5359
[13]   Activations of stacking faults in the calcium-containing magnesium alloys under compression [J].
Pan, Hucheng ;
Huang, Qiuyan ;
Qin, Gaowu ;
Fu, He ;
Xu, Ming ;
Ren, Yuping ;
She, Jia ;
Song, Bo ;
Li, Bin .
JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 692 :898-902
[14]   Achieving high strength in indirectly-extruded binary Mg-Ca alloy containing Guinier-Preston zones [J].
Pan, Hucheng ;
Qin, Gaowu ;
Ren, Yuping ;
Wang, Liqing ;
Sun, Shineng ;
Meng, Xiangying .
JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 630 :272-276
[15]   MODELING OF DYNAMIC MATERIAL BEHAVIOR IN HOT DEFORMATION - FORGING OF TI-6242 [J].
PRASAD, YVRK ;
GEGEL, HL ;
DORAIVELU, SM ;
MALAS, JC ;
MORGAN, JT ;
LARK, KA ;
BARKER, DR .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1984, 15 (10) :1883-1892
[16]  
PRASAD YVRK, 1990, INDIAN J TECHNOL, V28, P435
[17]  
Saxena K.K., 2014, Procedia Mater. Sci, V6, P278, DOI [10.1016/j.mspro.2014.07.035, DOI 10.1016/J.MSPRO.2014.07.035]
[18]   3D processing map and hot deformation behavior of 6A02 aluminum alloy [J].
Sun, Yu ;
Cao, Zhuohan ;
Wan, Zhipeng ;
Hu, Lianxi ;
Ye, Wenhong ;
Li, Niankui ;
Fan, Changlong .
JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 742 :356-368
[19]   Hot deformation behavior of Mg-8Li-3Al-2Zn-0.2Zr alloy based on constitutive analysis, dynamic recrystallization kinetics, and processing map [J].
Sun, Yuehua ;
Wang, Richu ;
Ren, Jian ;
Peng, Chaoqun ;
Feng, Yan .
MECHANICS OF MATERIALS, 2019, 131 :158-168
[20]   EFFECT OF INITIAL TEMPERATURE ON THE MICROSTRUCTURE AND PROPERTIES OF CRYOGENIC ROLLED AZ31 MAGNESIUM ALLOY [J].
Wu, Zhenyu ;
Zhi, Chenchen ;
Ma, Lifeng ;
Zheng, Zebang ;
Zhu, Yanchun ;
Jia, Weitao .
MATERIALI IN TEHNOLOGIJE, 2022, 56 (05) :571-577