Environment effect on internal fatigue crack propagation studied with in-situ X-ray microtomography

被引:7
|
作者
Hebrard, Louis [1 ]
Buffiere, Jean-Yves [1 ]
Palin-Luc, Thierry [2 ,3 ]
Ranc, Nicolas [4 ]
Majkut, Marta [1 ,5 ]
King, Andrew [6 ]
Weck, Arnaud [7 ,8 ,9 ]
机构
[1] Univ Lyon, INSA Lyon, MATEIS, CNRS,UMR 5510, F-69621 Villeurbanne, France
[2] Univ Bordeaux, CNRS, Bordeaux INP, I2M,UMR 5295, F-33400 Talence, France
[3] Hesam Univ, Arts & Metiers Inst Technol, CNRS, Bordeaux INP,I2M,UMR 5295, F-33400 Talence, France
[4] HESAM Univ, Arts & Metiers Inst Technol, PIMM Lab, CNRS,Cnam, 151 Blvd lHop, F-75013 Paris, France
[5] ESRF European Synchrotron, 71 Ave Martyrs,BP 220, F-38043 Grenoble 9, France
[6] LOrme Merisiers St Aubin, Synchrotron SOLEIL, F-91192 Gif Sur Yvette, France
[7] Univ Ottawa, Dept Mech Engn, 161 Louis Pasteur, Ottawa, ON K1N 6N5, Canada
[8] Univ Ottawa, Ctr Res Photon, 25 Templeton, Ottawa, ON K1N 6N5, Canada
[9] Univ Ottawa, Dept Phys, 150 Louis Pasteur, Ottawa, ON K1N 6N5, Canada
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2023年 / 882卷
关键词
Fatigue; Internal crack; Environment; Synchrotron; Ultrasonic; Short crack; HIGH-CYCLE FATIGUE; TITANIUM-ALLOY; STRESS RATIO; TI-6AL-4V; INITIATION; BEHAVIOR; GROWTH; MECHANISM; FAILURE; THERMOGRAPHY;
D O I
10.1016/j.msea.2023.145462
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In the present study, physically short fatigue cracks initiated from an artificial internal notch under vacuum conditions are observed in smooth specimens made of titanium alloy. The crack initiated from such a notch is not in contact with the surface during the majority of its propagation. Another batch of artificially notched specimens in the same alloy having their internal notch linked with the surface to bring air to the initiated short crack were tested too. All the specimens were ultrasonically cycled with synchrotron micro-computed tomography acquisitions which were regularly acquired from crack initiation detection to final failure without demounting the specimen. The number of cycles to failure, the internal crack growth rate and the crack growth mechanisms of internal cracks are compared for propagation under either air conditions or in the core of the alloy (i.e. under vacuum environment). It is shown that the environment plays a key role in the explanation of the very low crack growth rate of internal short crack loaded at very low stress amplitude leading to the gigacycle regime.
引用
收藏
页数:13
相关论文
共 50 条
  • [1] In situ fretting fatigue crack propagation analysis using synchrotron X-ray radiography
    de Pannemaecker, A.
    Buffiere, J. Y.
    Fouvry, S.
    Graton, O.
    INTERNATIONAL JOURNAL OF FATIGUE, 2017, 97 : 56 - 69
  • [2] Characterisation of short fatigue cracks in titanium alloy IMI 834 using X-ray microtomography
    Chapman, T. P.
    Kareh, K. M.
    Knop, M.
    Connolley, T.
    Lee, P. D.
    Azeem, M. A.
    Rugg, D.
    Lindley, T. C.
    Dye, D.
    ACTA MATERIALIA, 2015, 99 : 49 - 62
  • [3] Study fatigue crack initiation in TiB2/Al-Cu-Mg composite by in-situ SEM and X-ray microtomography
    Geng, Jiwei
    Li, Yugang
    Xiao, Hongyu
    Li, Hongping
    Sun, Huanhuan
    Chen, Dong
    Wang, Mingliang
    Wang, Haowei
    INTERNATIONAL JOURNAL OF FATIGUE, 2021, 142
  • [4] Synchrotron X-ray 3D characterisation of fatigue crack initiation during in-situ torsion cyclic tests
    Le, Viet-Duc
    Morel, Franck
    Saintier, Nicolas
    Osmond, Pierre
    Bellett, Daniel
    Ludwig, Wolfgang
    Majkut, Marta
    Buffiere, Jean-Yves
    INTERNATIONAL JOURNAL OF FATIGUE, 2025, 193
  • [5] In-situ X-ray computed tomography of composites subjected to fatigue loading
    Wagner, Peter
    Schwarzhaupt, Oliver
    May, Michael
    MATERIALS LETTERS, 2019, 236 : 128 - 130
  • [6] In situ synchrotron X-ray imaging of high-cycle fatigue crack propagation in single-crystal nickel-base alloys
    Liu, L.
    Husseini, N. S.
    Torbet, C. J.
    Lee, W. -K.
    Clarke, R.
    Jones, J. W.
    Pollock, T. M.
    ACTA MATERIALIA, 2011, 59 (13) : 5103 - 5115
  • [7] Internal fatigue crack propagation in a Ti-6Al-4V alloy: An in situ study
    Junet, Arnaud
    Messager, Alexandre
    Weck, Arnaud
    Nadot, Yves
    Boulnat, Xavier
    Buffiere, Jean-Yves
    INTERNATIONAL JOURNAL OF FATIGUE, 2023, 168
  • [8] Fatigue damage mechanisms of short fiber reinforced PA66 as observed by in-situ synchrotron X-ray microtomography
    Rolland, H.
    Saintier, N.
    Raphael, I.
    Lenoir, N.
    King, A.
    Robert, G.
    COMPOSITES PART B-ENGINEERING, 2018, 143 : 217 - 229
  • [9] Micro fatigue crack propagation behavior in a duplex stainless steel studied using in-situ SEM/EBSD method
    Chai, Guocai
    Peng, Ru Lin
    Johansson, Sten
    11TH INTERNATIONAL FATIGUE CONGRESS, PTS 1 AND 2, 2014, 891-892 : 313 - +
  • [10] 3D X-ray Microtomography Volume Correlation to Study Fatigue Crack Growth
    Limodin, Nathalie
    Rethore, Julien
    Buffiere, Jean-Yves
    Hild, Francois
    Ludwig, Wolfgang
    Rannou, Johann
    Roux, Stephane
    ADVANCED ENGINEERING MATERIALS, 2011, 13 (03) : 186 - 193