Effects of different glass formers on Li2S-P2S5-MS2 (M = Si, Ge, Sn) chalcogenide solid-state electrolytes

被引:9
|
作者
Zhang, Jiahui [1 ,2 ]
Gao, Chengwei [1 ,2 ]
He, Chengmiao [1 ,2 ]
Tan, Linling [1 ,2 ]
Kang, Shiliang [1 ,2 ]
Jiao, Qing [1 ,2 ]
Xu, Tiefeng [3 ]
Lin, Changgui [1 ,2 ]
机构
[1] Ningbo Univ, Res Inst Adv Lbchnol, Lab Infrared Mat & Devices, Ningbo 315211, Peoples R China
[2] Key Lab Photoelect Detect Mat & Devices Zhejiang, Ningbo 315211, Peoples R China
[3] Ningbo Inst Oceanog, Ningbo, Peoples R China
基金
中国国家自然科学基金;
关键词
air stability; chalcogenide solid-state electrolyte; cycling stability; electrochemical stability; glass network former; interface formation; IONIC-CONDUCTIVITY; ELECTROCHEMICAL PROPERTIES; INTERFACE STABILITY; LITHIUM; MECHANISM; TEMPERATURE; DEPOSITION; BATTERIES; ORIGIN; CELL;
D O I
10.1111/jace.18719
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Chalcogenide solid-state electrolytes (SSEs) have been receiving growing attentions due to their high ionic conductivity and suitable mechanic properties, especially the Li2S-P2S5 systems incorporated with a second glass network formers (Si, Ge, Sn, and so on) besides P. Although the ionic conductivities are generally enhanced with the second glass network formers, the comprehensive effects of different glass formers on other properties, including electrochemical, cycling, and air stability, remain elusive. To acquire deeper understanding, herein, three common but representative glass network formers (SiS2, GeS2, and SnS2) were introduced into Li2S-P2S5, and their individual effects were investigated systematically. The results of multiscale characterizations before and after lithium stripping/plating cycling confirmed that the introduction of metal cations (Ge, Sn) generally leads to worse electrochemical stability and shorter cycle life of these SSEs toward lithium metal compared with SSEs with nonmetal cation (Si) modification. However, the air stability is related to the binding energy of M-S (M = Si, Ge, Sn), which is consistent with the hard base soft acid theory. This work provides valuable understanding for designing pragmatic Li2S-P2S5-MS2-based SSEs with high electrochemistry, cycling, and air stability.
引用
收藏
页码:354 / 364
页数:11
相关论文
共 50 条
  • [21] Microelectrode Studies on Kinetics of Charge Transfer at an Interface of Li Metal and Li2S-P2S5 Solid Electrolytes
    Chiku, Masanobu
    Tsujiwaki, Wataru
    Higuchi, Eiji
    Inoue, Hiroshi
    ELECTROCHEMISTRY, 2012, 80 (10) : 740 - 742
  • [22] Preparation of sulfide solid electrolytes in the Li2S-P2S5 system by a liquid phase process
    Calpa, Marcela
    Rosero-Navarro, Nataly Carolina
    Miura, Akira
    Tadanaga, Kiyoharu
    INORGANIC CHEMISTRY FRONTIERS, 2018, 5 (02): : 501 - 508
  • [23] Analysis of the structure and degree of crystallisation of 70Li2S-30P2S5 glass ceramic
    Seino, Yoshikatsu
    Nakagawa, Masaru
    Senga, Minoru
    Higuchi, Hiroyuki
    Takada, Kazunori
    Sasaki, Takayoshi
    JOURNAL OF MATERIALS CHEMISTRY A, 2015, 3 (06) : 2756 - 2761
  • [24] Enhancing the Interfacial Stability of the Li2S-SiS2-P2S5 Solid Electrolyte toward Metallic Lithium Anode by LiI Incorporation
    Gao, Chengwei
    Zhang, Jiahui
    He, Chengmiao
    Kang, Shiliang
    Tan, Linling
    Jiao, Qing
    Xu, Tiefeng
    Dai, Shixun
    Lin, Changgui
    ACS APPLIED MATERIALS & INTERFACES, 2023, 15 (01) : 1392 - 1400
  • [25] Nanostructured all-solid-state supercapacitor based on Li2S-P2S5 glass-ceramic electrolyte
    Francisco, Brian E.
    Jones, Christina M.
    Lee, Se-Hee
    Stoldt, Conrad R.
    APPLIED PHYSICS LETTERS, 2012, 100 (10)
  • [26] Structure, ionic conductivity and electrochemical stability of Li2S-P2S5-LiI glass and glass-ceramic electrolytes
    Ujiie, Satoshi
    Hayashi, Akitoshi
    Tatsumisago, Masahiro
    SOLID STATE IONICS, 2012, 211 : 42 - 45
  • [27] All Solid-State Lithium-Sulfur Battery Using a Glass-Type P2S5-Li2S Electrolyte: Benefits on Anode Kinetics
    Yamada, Takanobu
    Ito, Seitaro
    Omoda, Ryo
    Watanabe, Taku
    Aihara, Yuichi
    Agostini, Marco
    Ulissi, Ulderico
    Hassoun, Jusef
    Scrosati, Bruno
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2015, 162 (04) : A646 - A651
  • [28] Suppressing Li Dendrite Formation in Li2S-P2S5 Solid Electrolyte by LiI Incorporation
    Han, Fudong
    Yue, Jie
    Zhu, Xiangyang
    Wang, Chunsheng
    ADVANCED ENERGY MATERIALS, 2018, 8 (18)
  • [29] Modification of 70Li2S-30P2S5 glass-ceramic electrolytes by Ce2S3 doping
    Zhang N.
    Zhong X.-Q.
    Ding F.
    Zhao X.-S.
    Liu X.-J.
    Xu Q.
    Gao Xiao Hua Xue Gong Cheng Xue Bao/Journal of Chemical Engineering of Chinese Universities, 2020, 34 (01): : 200 - 207
  • [30] Improved chemical stability and cyclability in Li2S-P2S5-P2O5-ZnO composite electrolytes for all-solid-state rechargeable lithium batteries
    Hayashi, Akitoshi
    Muramatsu, Hiromasa
    Ohtomo, Takamasa
    Hama, Sigenori
    Tatsumisago, Masahiro
    JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 591 : 247 - 250