Effect of in situ formation of Ti(C,N) on the properties of Al2O3-ZrO2-C slide plate material

被引:7
|
作者
Jiang, Qingzhu [1 ]
Han, Bingqiang [1 ]
Wei, Jiawei [1 ]
Chen, Junfeng [1 ]
Nan Li [1 ]
Li Youqi [2 ]
Jian He [2 ]
Wang, Huijun [3 ]
机构
[1] Wuhan Univ Sci & Technol, State Key Lab Refractories & Met, 947 Heping Rd, Wuhan 430081, Hubei, Peoples R China
[2] JiangSu Jingxin High Temp Mat Co Ltd, Yangzhou, Jiangsu, Peoples R China
[3] St Gobain Res Shanghai Co Ltd, Shanghai, Peoples R China
基金
中国国家自然科学基金;
关键词
Al2O3-ZrO2-C slide plate; dynamic slag corrosion resistance; Ti(C; N); viscosity; MGO-C REFRACTORIES; CARBON AL2O3-C REFRACTORIES; MECHANICAL-PROPERTIES; OXIDATION RESISTANCE; CORROSION-RESISTANCE; FRACTURE-BEHAVIOR; TI-C; MICROSTRUCTURE; SLAG; PERFORMANCE;
D O I
10.1111/ijac.14250
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Al2O3-ZrO2-C slide plate was ordinarily used in sliding nozzle system because of its excellent mechanical properties and slag corrosion resistance. This study improved the slag corrosion resistance of the slide plate by the carbothermic reduction of TiO2 and aluminothermic reduction of TiO2 under high temperature in coke bed to generate Ti(C,N) phase in situ. The result revealed that TiC of the high melting point phase could enter into anorthite (CaAl2Si2O8) of the low melting point phase, forming eutectic phase CaAl2Si2O8-TiC, and improve the viscosity of the slag. Furthermore, TiC and CaAl2Si2O8 captured FeO and MnO from the slag, resulting in the increase of the slag viscosity, inhibiting the penetration corrosion of the slag, and improving the slag corrosion resistance of the materials. In general, compared with the material without TiO2 powder, the slag corrosion resistance of the material introduced 2 wt.% TiO2 powder was increased by 24%. Meanwhile, the cold crushing strength of fired specimen at room temperature was increased by 35.6%.
引用
收藏
页码:1260 / 1268
页数:9
相关论文
共 50 条
  • [1] Preparation, microstructure and properties of Al2O3-ZrO2-C slide plate material in presence of nanoscale oxides
    Wang, Zihao
    Su, Kai
    Gao, Jinxing
    Jia, Quanli
    Zhang, Zongtao
    Liu, Xinhong
    CERAMICS INTERNATIONAL, 2022, 48 (07) : 10126 - 10135
  • [2] Effect of nano-oxides on corrosion resistance of Al2O3-ZrO2-C material
    Zhao, Zhenyi
    Wang, Zihao
    Tian, Xuekun
    Liang, Xinxing
    Su, Kai
    Liu, Xusheng
    Zhao, Fei
    Liu, Xinhong
    CERAMICS INTERNATIONAL, 2024, 50 (10) : 16890 - 16900
  • [3] Strengthening mechanism of Al2O3-ZrO2-C sliding plate material by existence modes of in-situ generated β-SiC whiskers
    Jiang, Qingzhu
    Peng, Yuefang
    Han, Bingqiang
    Zhang, Meijie
    Wei, Jiawei
    Li, Nan
    Li, Youqi
    He, Jian
    Wang, Huijun
    Chen, Junfeng
    CERAMICS INTERNATIONAL, 2023, 49 (24) : 39815 - 39824
  • [4] Reaction mechanisms between slag and Ti(C,N)-MgAl2O3-Al2O3 refractories at 1600 °C
    Sun, Yang
    Li, Yong
    Zhang, Lixin
    Li, Ling
    Sun, Jialin
    CERAMICS INTERNATIONAL, 2020, 46 (17) : 27774 - 27782
  • [5] Role of nano-ZrO2 powder in in-situ formation of ceramic whiskers in Al2O3-C slide plate materials
    Tian, Xuekun
    Liu, Zhifang
    Ouyang, Deze
    Su, Kai
    Wang, Hongsen
    Jia, Quanli
    Zhao, Fei
    Liu, Xinhong
    CERAMICS INTERNATIONAL, 2022, 48 (21) : 31579 - 31586
  • [6] Microstructure and Mechanical Properties of In situ Al2O3-Ti(C,N) Composites
    Feng, Xiumei
    Lian, Xiaoqing
    Jiang, Mingxue
    He, Yiner
    ADVANCED MATERIALS, PTS 1-4, 2011, 239-242 : 1243 - 1247
  • [7] Preparation and application of ZrB2-SiCw composite powder for corrosion resistance improvement in Al2O3-ZrO2-C slide plate materials
    Ban, Jinjin
    Zhou, Chaojie
    Feng, Long
    Jia, Quanli
    Liu, Xinhong
    Hu, Junhua
    CERAMICS INTERNATIONAL, 2020, 46 (07) : 9817 - 9825
  • [8] Effect of Ni and Ti on Mechanical Properties of Al2O3-Ti(C, N) Composites
    Li Qian
    Sun Xu-Dong
    Xiu Zhi-Meng
    JOURNAL OF INORGANIC MATERIALS, 2011, 26 (09) : 955 - 960
  • [9] Effect of Cr2O3/Cr3C2 additions on mechanical and tribological properties of Ti(C,N)-based cermets
    Liu, Mei-ling
    Cao, Ya-jing
    Hai, Wan-xiu
    Chen, Yu-hong
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2025, 35 (02) : 525 - 537
  • [10] Fabrication of in-situ Ti(C,N) phase toughened Al2O3 based ceramics from natural bauxite
    Li, Ziyan
    Fu, Lvping
    Gu, Huazhi
    Or, Siu Wing
    Huang, Ao
    Lv, Renxiang
    CERAMICS INTERNATIONAL, 2021, 47 (18) : 25497 - 25504