Ground waste ceramic brick effect at different times on mortar

被引:8
作者
Paes, Ana Luiza Campinho [1 ]
Botelho, Larissa C. G. [1 ]
Xavier, Gustavo de Castro [1 ]
Vieira, Carlos Mauricio Fontes [1 ]
Azevedo, Afonso R. G. [2 ]
Monteiro, Sergio N. [3 ]
机构
[1] UENF State Univ Northern Rio de Janeiro, LAMAV Adv Mat Lab, Ave Alberto Lamego 2000, BR-28013602 Campos Dos Goytacazes, RJ, Brazil
[2] UENF State Univ Northern Rio de Janeiro, LECIV Civil Engn Lab, Ave Alberto Lamego 2000, BR-28013602 Campos Dos Goytacazes, RJ, Brazil
[3] IME Mil Inst Engn, Mat Sci Program, Praca Gen Tiburcio 80, BR-22290270 Rio De Janeiro, RJ, Brazil
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2023年 / 24卷
关键词
Waste ceramic brick; Mortar; Pozzolanicity; CAMPOS DOS GOYTACAZES; CLAY BRICKS; GLASS WASTE; HYDRATION;
D O I
10.1016/j.jmrt.2023.03.191
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The work aims to observe the effect of waste ceramic brick (WCB), ground in two times, 60 and 120 min for use in mortar. The crystalline phases presented in clays of the north of Rio de Janeiro have already been identified, indicating that after firing at an adequate temperature, it is possible to apply it as a pozzolanic material. In this direction, in Brazil there is a single metakaolin industry in Sao Paulo operating in the domestic market supplying pozzolanic material for all regions of the country. The researched material was burned in the industry at approximately 700 degrees C, and its pozzolanic activity was tested by the Luxan test presenting 2.01 mS/cm (good pozzolanicity). The mortars proportions were 1:6 (cement: sand), with the addition of 0% (reference), 10%, 20% and 30% of WCB, and their crystalline phases were analyzed by XRD and it was not identified a kaolinite peak, a good indication of the transformation to metakaolinite. The tests in both fresh and hardened state were performed. For both grindings, the residue reacted with the paste, a fact confirmed by the nucleation calorimetry of particles <2 mu m (20%-25% clay fraction), reducing the pore size from 0.90 to 50 mm to 0.008 at 5 mu m, forming CeSeH in the XRD and the portlandite peaks disappearing when compared to the reference. The results showed that the best result was 10% incorporation, both for WCB ground for 60 and 120 min, and this is the proportion indicated. (c) 2023 The Author(s). Published by Elsevier B.V. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).
引用
收藏
页码:3513 / 3523
页数:11
相关论文
共 50 条
  • [41] Evaluation of strength of mortar using different saw waste with sand and model development
    Mahzuz, H. M. A.
    Ahmed, M.
    Hossain, M. M.
    Islam, M. M.
    Alam, M. K.
    KSCE JOURNAL OF CIVIL ENGINEERING, 2016, 20 (07) : 2822 - 2831
  • [42] Evaluation of strength of mortar using different saw waste with sand and model development
    H. M. A. Mahzuz
    M. Ahmed
    M. M. Hossain
    M. M. Islam
    M. K. Alam
    KSCE Journal of Civil Engineering, 2016, 20 : 2822 - 2831
  • [43] Effect of waste glass particle size on high temperature properties of mortar
    Ke, G.-J. (kegj320@sina.com), 1600, Tongji University (16): : 335 - 340
  • [44] THE EFFECT OF RECYCLED WASTE MEDICINE MATERIALS ON THE PROPERTIES OF CEMENT MORTAR COATIS
    Hamead, Alaa A. Abdul
    JOURNAL OF ENGINEERING SCIENCE AND TECHNOLOGY, 2020, 15 (06): : 4182 - 4199
  • [45] Combined Effect of Marble Waste as Powder and Aggregate Form on the Proprieties of the Mortar
    Maza, Mekki
    Tebbal, Nadia
    Zitouni, Salim
    Rahmouni, Zine El Abidine
    ANNALES DE CHIMIE-SCIENCE DES MATERIAUX, 2021, 45 (06): : 467 - 476
  • [46] Alternative Use of the Waste from Ground Olive Stones in Doping Mortar Bricks for Sustainable Façades
    San Vicente-Navarro, Alejandro
    Mendivil-Giro, Manuel
    Los Santos-Ortega, Jorge
    Fraile-Garcia, Esteban
    Ferreiro-Cabello, Javier
    BUILDINGS, 2023, 13 (12)
  • [47] Use of industrial ceramic sludge in brick production: Effect on aesthetic quality and physical properties
    Coletti, Chiara
    Maritan, Lara
    Cultrone, Giuseppe
    Mazzoli, Claudio
    CONSTRUCTION AND BUILDING MATERIALS, 2016, 124 : 219 - 227
  • [48] Evaluating the effect of waste glass granules on the fresh, mechanical properties and shear bond strength of sustainable cement mortar
    Ahmad, Soran Abdrahman
    Rafiq, Serwan Khwrshed
    Faraj, Rabar H.
    CLEAN TECHNOLOGIES AND ENVIRONMENTAL POLICY, 2023, 25 (06) : 1989 - 2008
  • [49] Evaluating the effect of waste glass granules on the fresh, mechanical properties and shear bond strength of sustainable cement mortar
    Soran Abdrahman Ahmad
    Serwan Khwrshed Rafiq
    Rabar H. Faraj
    Clean Technologies and Environmental Policy, 2023, 25 : 1989 - 2008
  • [50] Pozzolanic potentials and hydration behavior of ground waste clay brick obtained from clamp-firing technology
    Bediako, Mark
    CASE STUDIES IN CONSTRUCTION MATERIALS, 2018, 8 : 1 - 7