Base free HMF oxidation over Ru-MnO2 catalysts revisited: Evidence of Mn leaching to Mn-FDCA complexation and its implications on catalyst performance

被引:7
|
作者
Mani, Mariappan [1 ,3 ]
Mariyaselvakumar, Mariyamuthu [1 ]
Tothadi, Srinu [2 ]
Panda, Asit Baran [3 ,4 ]
Srinivasan, Kannan [1 ,3 ]
Konwar, Lakhya Jyoti [1 ,3 ]
机构
[1] Cent Salt & Marine Chem Res Inst CSIR CSMCRI, Council Sci & Ind Res CSIR, Inorgan Mat & Catalysis Div, G B Marg, Bhavnagar 364002, Gujarat, India
[2] Council Sci & Ind Res CSIR, CSIR Cent Salt & Marine Chem Res Inst, Analyt & Environm Sci Div & Centralized Instrument, Bhavnagar 364002, India
[3] Acad Sci & Innovat Res AcSIR, Ghaziabad 201002, India
[4] CSIR Natl Met Lab, Jamshedpur 831007, India
来源
MOLECULAR CATALYSIS | 2024年 / 554卷
关键词
HMF oxidation; MnO2 based oxidation catalysts; catalyst stability; acid promoted Mn-leaching; Mn-FDCA complex; 2,5-FURANDICARBOXYLIC ACID; AEROBIC OXIDATION; SELECTIVE OXIDATION; AQUEOUS-PHASE; CHEMICALS; BIOMASS; DERIVATIVES; CONVERSION; EFFICIENT; CARBON;
D O I
10.1016/j.mcat.2023.113811
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
2,5-furandicarboxylic acid (FDCA) is a high value bio-based chemical useful for the production of next generation renewable polymers, epoxy -resins and surfactants. Herein, we show that the performance and stability of MnO2 based oxidation catalysts used in FDCA production are considerably influence by process conditions (especially initial HMF conc. and presence of base additives). Although, base free aerobic oxidation of HMF to FDCA is known to be highly effective over Ru modified MnO2 catalysts, our experiments showed considerable leaching of MnO2 phase under reaction conditions with the formation of insoluble Mn-FDCA complexes. The formation of Mn-FDCA complex and Mn leaching was also supported by control experiments between FDCA and various Mn oxides under hydrothermal conditions and its structure confirmed by single crystal XRD. Formation of Mn-FDCA and Mn leaching was also identified as the underlying reason for carbon balance deficit, catalyst mass loss and deactivation observed upon reuse.
引用
收藏
页数:12
相关论文
共 3 条
  • [1] Electro-catalytic oxidation of HMF to FDCA over RuO2/MnO2/CNT catalysts in base-free solution
    Wang, Tianci
    Song, Yu
    Zhao, Wanna
    Zhou, Chunmei
    Jin, Yuguang
    Wan, Xiaoyue
    Dai, Yihu
    Yang, Yanhui
    NEW JOURNAL OF CHEMISTRY, 2021, 45 (45) : 21285 - 21292
  • [2] Co3O4 NPs decorated Mn-Co-O solid solution as highly selective catalyst for aerobic base-free oxidation of 5-HMF to 2,5-FDCA in water
    Gao, Tianyu
    Yin, Yongxuan
    Zhu, Guanghui
    Cao, Qiue
    Fang, Wenhao
    CATALYSIS TODAY, 2020, 355 : 252 - 262
  • [3] Enhancement of toluene oxidation performance over Pt/MnO2@Mn3O4 catalyst with unique interfacial structure
    Duan, Xiaoxiao
    Qu, Zhenping
    Dong, Cui
    Qin, Yuan
    APPLIED SURFACE SCIENCE, 2020, 503