Strengthening mechanisms in Monel K500 alloyed with Al and Ti

被引:8
|
作者
Kostryzhev, A. G. [1 ]
Marenych, O. O. [1 ]
Pan, Z. [2 ]
Li, H. [2 ]
van Duin, S. [3 ]
机构
[1] Univ Queensland, Ctr Microscopy & Microanal, St Lucia, Qld 4072, Australia
[2] Univ Wollongong, Sch Mech Mat Mechatron & Biomed Engn, Northfields Ave, Wollongong, NSW 2522, Australia
[3] DMTC Ltd, Level 1,620 High St, Kew, Vic 3101, Australia
基金
澳大利亚研究理事会;
关键词
316; STAINLESS-STEEL; CORROSION BEHAVIOR; SOLID-SOLUTION; HIGH-TEMPERATURE; PRECIPITATION; NICKEL; EVOLUTION; GRAIN; MICROSTRUCTURE; RESISTANCE;
D O I
10.1007/s10853-023-08248-2
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Monel alloys containing 63Ni-30Cu (wt%) are often used in applications requiring simultaneously high strength and corrosion resistance. Additions of Ti, Al and C to Monel K500 lead to formation of TiC, Ni3Al and Ni3Ti particles, which provide precipitation strengthening effect following heat treatment. The traditional heat treatment schedule includes solution annealing above 1000 degrees C and aging in the 400-600 degrees C temperature range. However, no correlation exists between the alloy composition and the heat treatment schedule (holding temperature and time) required to obtain the optimum microstructure and mechanical properties. This may result in excessive alloying, energy loses during heat treatment, and higher product costs. In this work, we investigate the effect of solution annealing part of heat treatment schedule on microstructure (particularly, particle precipitation and grain growth), hardness and strength. For hot rolled samples, solution annealing followed by aging was shown to result in lower strength compared to aging without annealing. The analysis of strengthening mechanisms carried out utilising our theory for calculation of solute atom concentrations has explained the strength variation with heat treatment and has shown (i) a lower strength after annealing and aging being related to dissolution of fine (< 20 nm) TiC particles, (ii) Ti- and Al-rich precipitates to provide a larger strengthening than Ti and Al solute atoms, (iii) Al to be a more effective strengthening agent than Ti, and (iv) the majority of Al to remain in solution for both processing schedules, this indicates potential for mechanical properties improvement via optimisation of the heat treatment schedule aiming to generate more Al-rich precipitates.
引用
收藏
页码:4150 / 4164
页数:15
相关论文
共 50 条
  • [1] Effect of Ti on stress corrosion cracking behavior and mechanism of Monel K500 alloy in flowing seawater
    Xi, Yuchen
    Wang, Qinying
    Luo, Xiaofang
    Zhang, Xingshou
    Liu, Tingyao
    Zheng, Huaibei
    Dong, Lijin
    Wang, Jie
    Zhang, Jin
    ANTI-CORROSION METHODS AND MATERIALS, 2023, 70 (06) : 428 - 437
  • [2] Stress corrosion cracking behavior and mechanism of aging treated Monel K500 alloy in flowing seawater
    Wang, Qinying
    Luo, Xiaofang
    Zhang, Xingshou
    Liu, Tingyao
    Zheng, Huaibei
    Dong, Lijin
    Xi, Yuchen
    Bai, Shulin
    JOURNAL OF MATERIALS SCIENCE, 2023, 58 (15) : 6784 - 6802
  • [3] A Comparative Analysis of a Microstructure and Properties for Monel K500 Hot-Rolled to a Round Bar and Wire Deposited on a Round Surface
    Kostryzhev, Andrii
    Marenych, Olexandra
    Pan, Zengxi
    Li, Huijun
    van Duin, Stephen
    METALS, 2024, 14 (07)
  • [4] Effect of TiC precipitation on the corrosion behavior of Monel K500 alloy in 3.5 wt.% NaCl solution
    He, Zebang
    Chen, Beiyang
    Zhou, Baowei
    Liu, Feng
    Hu, Qing
    Qin, Zhenbo
    Gao, Zhiming
    Hu, Wenbin
    Wu, Zhong
    CORROSION SCIENCE, 2023, 211
  • [5] Effect of applied potential on the tribocorrosion behaviors of Monel K500 alloy in artificial seawater
    Chen, Jun
    Wang, Jianzhang
    Yan, Fengyuan
    Zhang, Qing
    Li, Quan-an
    TRIBOLOGY INTERNATIONAL, 2015, 81 : 1 - 8
  • [6] Synergistic effect between cavitation erosion and corrosion of Monel K500 alloy in 3.5 wt% NaCl solution
    He, Zebang
    Qin, Zhenbo
    Gao, Zhiming
    Wu, Zhong
    Hu, Wenbin
    MATERIALS CHARACTERIZATION, 2023, 205
  • [7] Ceramic Tools with Ordinary and Wiper Inserts in Near Dry Machining with High Speed on Super Alloy Monel K500
    Amini, S.
    Paktinat, H.
    MATERIALS AND MANUFACTURING PROCESSES, 2014, 29 (05) : 579 - 584
  • [8] The effect of Ni201 transition layer on the corrosion, wear and synergetic cavitation erosion-corrosion behavior of CMT-Monel K500 coating
    Zhao, T.
    Zhang, S.
    Zhang, C. H.
    Sun, X. Y.
    Bai, X. L.
    Wu, C. L.
    SURFACE & COATINGS TECHNOLOGY, 2023, 463
  • [9] THE EFFECT OF THE MICROSTRUCTURE ON THE TRIBOLOGICAL PROPERTIES OF THE MONEL K-500 ALLOY
    Krawczyk, Janusz
    Frocisz, Lukasz
    Matusiewicz, Piotr
    Madej, Marcin
    METAL 2015: 24TH INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS, 2015, : 1326 - 1334
  • [10] Characterization and Slurry Erosion Mechanisms of Nickel-Based Cermet Coatings on Monel K-500
    Singh, Navneet K.
    Kumar, Avneesh
    Ang, Andrew S. M.
    Mahajan, Dhiraj K.
    Singh, Harpreet
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2021, 30 (08) : 2138 - 2154