Comparative study on the influence of hydrodynamic conditions in the corrosion behavior of a 1018 carbon steel using a green inhibitor in brine-CO2 solution

被引:2
作者
Henao, J. [1 ]
Torres, A. [2 ]
Sotelo-Mazon, O. [3 ,4 ]
Valdez-Rodriguez, S. [5 ]
Poblano-Salas, C. [6 ]
Cuevas-Arteaga, C. [4 ]
Corona-Castuera, J. [6 ]
Ramos-Hernandez, J. J. [5 ]
Casales-Diaz, M. [5 ]
机构
[1] CONAYT CIATEQ AC, Parque Ind Bernardo Quintana,Av Manantiales 23-A, Queretaro 76246, Mexico
[2] Tecnol Monterrey, Av Carlos Lazo 100, Mexico City 01389, Mexico
[3] UAEM, Fac Ciencias Quim & Ingn, Av Univ 1001, Cuernavaca 62209, Mor, Mexico
[4] UAEM, Ctr Invest Ingn & Ciencias Aplicadas, Av Univ 1001, Cuernavaca 62209, Mor, Mexico
[5] UNAM, Inst Ciencias Fis, Av Univ 1001, Cuernavaca 62210, Mor, Mexico
[6] CIAEQ AC, Parque Ind Bernardo Quintana,Av Manantiales 23-A, Cuernavaca 76246, Qro, Mexico
来源
INTERNATIONAL JOURNAL OF CORROSION AND SCALE INHIBITION | 2023年 / 12卷 / 01期
关键词
green corrosion inhibitor; imidazoline; electrochemical techniques; hydrodynamic conditions; CO2; corrosion; ELECTROCHEMICAL IMPEDANCE SPECTROSCOPY; ROTATING CYLINDER ELECTRODE; CO2-CORROSION; MILD-STEEL; TURBULENT-FLOW; AVOCADO OIL; IMIDAZOLINE; ACID; PERFORMANCE; TEMPERATURE;
D O I
10.17675/2305-6894-2023-12-1-1
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The corrosion behavior of a 1018 carbon steel was studied by electrochemical techniques under hydrodynamic conditions employing N-hydroxyethylimidazoline derivatives of avocado oil as a green corrosion inhibitor. The corrosion behavior of the steel surface under hydrodynamic flow conditions before and after the addition of the green corrosion inhibitor was evaluated by means of the rotating cylinder method using rotation speeds of 0, 10, 100, 500, 1000, and 2000 RPM. The inhibitor concentration was set at 25 ppm (7.29x10(-5) mol/L) in all conditions studied. The results display a high corrosion resistance of the carbon steel surface at a rotation speed of 1000 RPM in the absence of inhibitor, which is attributed to the formation of a protective FeCO3 layer. When the inhibitor is added to the electrolyte, the highest corrosion resistance is observed for the samples evaluated under static conditions and the lowest rotational speeds. In the presence of the inhibitor, the carbon steel surface shows a decrease in the corrosion resistance as the rotation speed increases above 500 RPM. Interestingly, the addition of the inhibitor promotes a uniform corrosion process on the steel surface under zero rotation and low rotational speeds, and a localized corrosion process for high rotational speeds, respectively. The results suggest that dynamic conditions are associated to a change in the inhibitor concentration at the metal surface, which influences in a negative way the protective effect of the inhibitor.
引用
收藏
页码:1 / 31
页数:31
相关论文
共 58 条
[11]   An electrochemical investigation on the effect of the chloride content on CO2 corrosion of API-X100 steel [J].
Eliyan, Faysal Fayez ;
Mohammadi, Farzad ;
Alfantazi, Akram .
CORROSION SCIENCE, 2012, 64 :37-43
[12]   Palm oil as green corrosion inhibitors for different metal surfaces and corrosive media: A review [J].
Faraj, M. W. ;
Alamiery, A. .
INTERNATIONAL JOURNAL OF CORROSION AND SCALE INHIBITION, 2022, 11 (02) :465-477
[13]   Corrosion study of the X52 steel immersed in seawater with a corrosion inhibitor using a rotating cylinder electrode [J].
Galvan-Martinez, R. ;
Orozco-Cruz, R. ;
Torres-Sanchez, R. ;
Martinez, E. A. .
MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2010, 61 (10) :872-876
[14]   The effect of electrolyte flow on the performance of 12-aminododecanoic acid as a carbon steel corrosion inhibitor in CO2-saturated hydrochloric acid [J].
Ghareba, Saad ;
Omanovic, Sasha .
CORROSION SCIENCE, 2011, 53 (11) :3805-3812
[15]  
Gonzalez-Rodriguez JG, 2021, Journal of Bio- and Tribo-Corrosion, V7, DOI [10.1007/s40735-021-00523-6, 10.1007/s40735-021-00523-6, DOI 10.1007/S40735-021-00523-6]
[16]  
Gulbrandsen E., 1998, NACE CORROSION, V13
[17]   Chemistry and Structure of the Passive Film on Mild Steel in CO2 Corrosion Environments [J].
Han, Jiabin ;
Young, David ;
Colijn, Hendrik ;
Tripathi, Akhilesh ;
Nesic, Srdjan .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2009, 48 (13) :6296-6302
[18]   Inhibition of mild steel corrosion in hydrochloric acid solution by triazole derivatives Part II: Time and temperature effects and thermodynamic treatments [J].
Hassan, Hamdy H. .
ELECTROCHIMICA ACTA, 2007, 53 (04) :1722-1730
[19]   The formation of FeCO3 and Fe3O4 on carbon steel and their protective capabilities against CO2 corrosion at elevated temperature and pressure [J].
Hua, Yong ;
Xu, Shusheng ;
Wang, Yun ;
Taleb, Wassim ;
Sun, Jianbo ;
Zhang, Lei ;
Barker, Richard ;
Neville, Anne .
CORROSION SCIENCE, 2019, 157 :392-405
[20]   Comparison of corrosion behaviour for X-65 carbon steel in supercritical CO2-saturated water and water-saturated/unsaturated supercritical CO2 [J].
Hua, Yong ;
Barker, Richard ;
Neville, Anne .
JOURNAL OF SUPERCRITICAL FLUIDS, 2015, 97 :224-237