Behaviour of nickel coatings made by brush plating technology in conditions of cavitation erosion and corrosion

被引:15
|
作者
Krella, Alicja K. [1 ]
Grzes, Jaroslaw [2 ]
Erbe, Andreas [3 ]
Folstad, Marthe [3 ]
机构
[1] Polish Acad Sci, Inst Fluid Flow Machinery, Gdansk, Poland
[2] Warsaw Univ Technol, Inst Mfg Technol, Warsaw, Poland
[3] Norwegian Univ Sci & Technol, Dept Mat Sci & Engn, Trondheim, Norway
关键词
Brush plating; Cavitation erosion; Nickel coating; Coating structure; Electrochemical properties; STAINLESS-STEEL; TIN COATINGS; RESISTANCE; MICROSTRUCTURE; PERFORMANCE; ALLOYS; WEAR;
D O I
10.1016/j.wear.2023.204998
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The basic hypothesis of the research was that the structure of the coating, i.e. the type of defects, affects the mechanical and electrochemical properties, as well as the resistance to cavitation erosion and corrosion. For this purpose, nickel coatings produced by brush-plating technology using two different electrolytes and deposited on X20Cr13 steel were tested. The electrolytes affected the structure and properties of the coatings: one coating had a network of cracks, and the second one had a "cauliflower-like" structure. The hardness and Young's modulus of both coatings were investigated under multi-cycle loading modes. Cavitation erosion resistance was tested in a cavitation tunnel equipped with a barricade system at an inlet pressure of 600 kPa and outlet pressure of 120 kPa. Both nickel coatings protected the substrate against cavitation erosion. The lowest rate of cavitation erosion had a coating with a network of cracks and high hardness. Microscopic examinations showed no influence of the net of cracks on the degradation process. Electrochemical tests confirmed the better corrosion resistance of the compact coating. The compact coating had about an order of magnitude lower corrosion potential and about 100 mV higher corrosion current density than that of the agglomerate coating. The agglomerate coating had electrochemical parameters comparable to the substrate.
引用
收藏
页数:15
相关论文
共 50 条
  • [21] Effects of Bacillus sp. adhesion on cavitation erosion behaviour of nickel aluminium bronze in artificial seawater
    Tian, Ye
    Zhao, Hang
    Yang, Rui
    Liu, Xiaomei
    Li, Hua
    Chen, Xiuyong
    WEAR, 2022, 498
  • [22] A study on slurry erosion and corrosion behaviour of HVOF sprayed titania coatings
    Ramesh, C. S.
    Sekhar, N.
    Keshavamurthy, R.
    Pramod, S.
    INTERNATIONAL JOURNAL OF SURFACE SCIENCE AND ENGINEERING, 2015, 9 (01) : 55 - 68
  • [23] Cavitation erosion and corrosion resistance of hydrophobic sol-gel coatings on aluminium alloy
    Hegde, Manasa
    Mohan, Joseph
    Warraich, Muhammad Qasim Mushtaq
    Kavanagh, Yvonne
    Duffy, Brendan
    Tobin, Edmond F.
    WEAR, 2023, 524
  • [24] Different methods of measuring synergy between cavitation erosion and corrosion for nickel aluminium bronze in 3.5% NaCl solution
    Basumatary, J.
    Wood, R. J. K.
    TRIBOLOGY INTERNATIONAL, 2020, 147
  • [25] Preparation and characterization of graphite-nickel composite coatings by automatic brush plating
    Wu, Bin
    Yu, Xu-Hua
    Zhang, Bin
    Xu, Bin-Shi
    SURFACE & COATINGS TECHNOLOGY, 2008, 202 (10) : 1975 - 1979
  • [26] Understanding Liquid Impingement erosion behaviour of nickel-alumina based thermal spray coatings
    Grewal, H. S.
    Singh, H.
    Agrawal, Anupam
    WEAR, 2013, 301 (1-2) : 424 - 433
  • [27] Correlation of microstructure with cavitation erosion behaviour of a nickel-aluminum bronze in simulated seawater
    Zhang, L. M.
    Ma, A. L.
    Yu, H.
    Umoh, A. J.
    Zheng, Y. G.
    TRIBOLOGY INTERNATIONAL, 2019, 136 : 250 - 258
  • [28] Cavitation erosion and corrosion behavior of Ni-Al intermetallic coatings
    Chang, JT
    Yeh, CH
    He, JL
    Chen, KC
    WEAR, 2003, 255 : 162 - 169
  • [29] Iso-material manufacturing of 304 stainless steel: Microstructure, corrosion-cavitation erosion synergistic behaviour
    Cao, Bosheng
    Wu, Chenliang
    Wang, Li
    Zhang, Song
    Zhang, Chunhua
    Sun, Xueying
    MATERIALS SCIENCE AND TECHNOLOGY, 2024, 40 (04) : 310 - 326
  • [30] The role of microstructural characteristics in the cavitation erosion behaviour of laser melted and laser processed Nickel-Aluminium Bronze
    Cottam, R.
    Luzin, V.
    Moody, H.
    Edwards, D.
    Majumdar, A.
    Wong, Y. C.
    Wang, J.
    Brandt, M.
    WEAR, 2014, 317 (1-2) : 56 - 63