Metal-metal and metal-composite joints with 3D printed aluminium substrates: effect of surface treatment on the mode I fracture toughness

被引:8
作者
Gulino, Michele [1 ]
Moroni, Fabrizio [1 ]
Pirondi, Alessandro [1 ]
机构
[1] Univ Parma, Dept Engn & Architecture, Parco Area Sci 181-A, I-43124 Parma, Italy
关键词
Mode I fracture toughness; co-bonding; selective laser melting (SLM); aluminium; carbon fibre reinforced polymer (CFRP); BONDED JOINTS; DELAMINATION SUPPRESSION; MECHANISMS; STRENGTH; BEHAVIOR;
D O I
10.1080/00218464.2023.2285074
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
Adhesive bonding of composite laminates to metals is an increasingly employed technique to manufacture lightweight structures. However, this type of joints is sensitive to defects and composite delamination near the bonded area. Thus, increasing their damage tolerance is fundamental to design reliable multi-material components. This work is the first step in a project aimed at improving the fracture toughness of Carbon Fibre Reinforced Polymer (CFRP)/metal joints, exploiting Additive Manufacturing (AM) to produce small features on the metal adherend. This first step is devoted to the qualification of the Mode I fracture toughness of the as-built AM surface. Thus, Double Cantilever Beam (DCB) tests are carried out on metal/metal secondary bonded and CFRP/metal co-bonded joints. The metal part is obtained by Selective Laser Melting (SLM) of AlSi10Mg aluminium alloy, without surface pre-treatment to preserve the as-built roughness. The fracture toughness of the AM un-treated joints is also compared to that of joints in which the metal adherend is sandblasted. Optical profilometry is employed to evaluate the surface morphology of both as printed and sandblasted adherends. The results show that the untreated joints have comparable fracture toughness to their treated counterparts, despite manifesting dissimilar failure modes due to the different surface morphologies.
引用
收藏
页码:115 / 143
页数:29
相关论文
共 44 条
[21]   On the fracture behaviour of CFRP bonded joints under mode I loading: Effect of supporting carrier and interface contamination [J].
Heide-Jorgensen, Simon ;
de Freitas, Sofia Teixeira ;
Budzik, Michal K. .
COMPOSITES SCIENCE AND TECHNOLOGY, 2018, 160 :97-110
[22]   Failure behaviour of composite T-joints with novel metallic arrow-pin reinforcement [J].
Heimbs, S. ;
Nogueira, A. C. ;
Hombergsmeier, E. ;
May, M. ;
Wolfrum, J. .
COMPOSITE STRUCTURES, 2014, 110 :16-28
[23]   Adhesively bonded joints in components manufactured via selective laser melting [J].
Koch, C. ;
Richter, J. ;
Vollmer, M. ;
Kahlmeyer, M. ;
Niendorf, T. ;
Boehm, S. .
PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART C-JOURNAL OF MECHANICAL ENGINEERING SCIENCE, 2021, 235 (03) :518-526
[24]   Design of adhesively bonded lap joints with laminated CFRP adherends: Review, challenges and new opportunities for aerospace structures [J].
Kupski, J. ;
de Freitas, S. Teixeira .
COMPOSITE STRUCTURES, 2021, 268
[25]  
Lander J. K., 2008, THESIS CRANFIELD U C
[26]   Uncovering the toughening mechanisms of bonded joints through tailored CFRP layup [J].
Lima, R. A. A. ;
Tao, R. ;
Bernasconi, A. ;
Carboni, M. ;
Carrere, N. ;
Freitas, S. Teixeira de .
COMPOSITES PART B-ENGINEERING, 2023, 263
[27]   A REVIEW OF THE STRENGTH OF JOINTS IN FIBER-REINFORCED PLASTICS .2. ADHESIVELY BONDED JOINTS [J].
MATTHEWS, FL ;
KILTY, PF ;
GODWIN, EW .
COMPOSITES, 1982, 13 (01) :29-37
[28]   A novel strategy to obtain the fracture envelope under mixed-mode I plus II loading of composite bonded joints [J].
Moreira, R. D. F. ;
de Moura, M. F. S. F. ;
Silva, F. G. A. .
ENGINEERING FRACTURE MECHANICS, 2020, 232
[29]   Additive Manufacturing of Titanium with Different Surface Structures for Adhesive Bonding and Thermal Direct Joining with Fiber-Reinforced Polyether-Ether-Ketone (PEEK) for Lightweight Design Applications [J].
Moritz, Juliane ;
Goetze, Philipp ;
Schiefer, Tom ;
Stepien, Lukas ;
Klotzbach, Annett ;
Standfuss, Jens ;
Lopez, Elena ;
Brueckner, Frank ;
Leyens, Christoph .
METALS, 2021, 11 (02) :1-14
[30]   Comparison of Tensile Strength and Fracture Toughness of Co-Bonded and Cold-Bonded Carbon Fiber Laminate-Aluminum Adhesive Joints [J].
Moroni, Fabrizio ;
Pirondi, Alessandro ;
Pernechele, Chiara ;
Vescovi, Luca .
MATERIALS, 2021, 14 (14)