Evolution of microstructure, mechanical and corrosion properties of Fe-13Cr-4Al-1.5Nb alloy aged at 450 °C

被引:3
作者
An, Xuguang [1 ,2 ]
Zhang, Yiyong [3 ]
Luo, Yuanqi [1 ]
Liu, Jia [1 ]
Zhang, Jing [1 ,2 ]
Kong, Qingquan [1 ,2 ]
Wang, Hui [2 ,4 ]
Wang, Yuan [5 ]
机构
[1] Chengdu Univ, Sch Mech Engn, Chengdu 610106, Peoples R China
[2] Chengdu Univ, Inst Adv Study, Interdisciplinary Mat Res Ctr, Chengdu 610106, Peoples R China
[3] Sichuan Univ, Sch Aeronaut & Astronaut, Chengdu 610065, Peoples R China
[4] Nucl Power Inst China, Sci & Technol Reactor Fuel & Mat Lab, Chengdu, Peoples R China
[5] Sun Yat Sen Univ, Sch Phys & Astron, Zhuhai 519082, Guangdong, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2023年 / 24卷
基金
中国国家自然科学基金;
关键词
Fe-13Cr-4Al-1; 5Nb alloy; Aging treatment; Microstructure; Mechanical properties; Corrosion resistance; CR-AL ALLOYS; FECRAL ALLOYS; OXIDATION; NB; EMBRITTLEMENT; PARTICLES; BEHAVIOR; STEELS; MO;
D O I
10.1016/j.jmrt.2023.05.016
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In the present work, the microstructure evolution, mechanical and corrosion properties of Fe-13Cr-4Al-1.5Nb alloys were systematically studied after the long-term thermal aging treatment. After aging, the Fe-13Cr-4Al-1.5Nb alloys are still mainly composed of a-Fe phase and a small amount of Fe2Nb-type laves phase, but the preferred orientation almost disappeared. With the increase of aging time, the average grain size of Fe-13Cr-4Al-1.5Nb alloy increased obviously and the amount of Fe2Nb-type laves phase also increased significantly. After aging at 450 & DEG;C for 2000 h, some coarse grains were observed in the Fe-13Cr-4Al-1.5Nb alloy and it exhibited much coarser grains with an average grain size of 19.7 mm than unaged Fe-13Cr-4Al-1.5Nb alloy due to the incomplete recrystallization. With the increase of aging time, the tensile strength was almost unchanged while the ductility decreased significantly. Due to the incomplete recrystallization, the Fe-13Cr-4Al1.5Nb alloy exhibited the highest tensile strength of 670.5 MPa but the worst elongation of 3.9% after aging at 450 & DEG;C for 2000 h. In addition, the electrochemical corrosion test results showed that the unaged Fe-13Cr-4Al-1.5Nb alloy has better comprehensive corrosion resistance than the aged Fe-13Cr-4Al-1.5Nb alloy in 3.5wt.%NaCl solution. & COPY; 2023 The Author(s). Published by Elsevier B.V. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).
引用
收藏
页码:7313 / 7325
页数:13
相关论文
共 44 条
[1]   Fabrication of in-situ TiC-TiB2 reinforced Al foam with enhanced properties [J].
An, Xuguang ;
Liu, Ying ;
Ye, Jinwen ;
Li, Xun .
JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 825
[2]   Recovery, recrystallization and precipitation behavior in an ATF FeCrAl alloy during annealing treatment [J].
Chen, Li ;
Wang, Hui ;
An, Xuguang ;
Huang, Xuefei .
MATERIALS CHARACTERIZATION, 2022, 190
[3]   Precipitation behavior and age hardening effect of the precipitates in a Fe-13Cr-4Al-2Mo-1.2Nb alloy [J].
Chen, Li ;
Huang, Xuefei ;
He, Kun ;
Wang, Hui .
MATERIALS CHARACTERIZATION, 2021, 173
[4]   Effects of ZrC addition on the microstructure and mechanical properties of Fe-Cr-Al alloys fabricated by spark plasma sintering [J].
Ding, Rongfa ;
Wang, Hui ;
Jiang, Yan ;
Liu, Rui ;
Jing, Ke ;
Sun, Meng ;
Zhang, Ruiqian ;
Qiu, Shaoyu ;
Xie, Zhuoming ;
Deng, Haowei ;
Wang, Xianping ;
Kong, Mingguang ;
Jiang, Weibin ;
Fang, Qianfeng ;
Liu, Changsong .
JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 805 :1025-1033
[5]   Development of low-Cr ODS FeCrAl alloys for accident-tolerant fuel cladding [J].
Dryepondt, Sebastien ;
Unocic, Kinga A. ;
Hoelzer, David T. ;
Massey, Caleb P. ;
Pint, Bruce A. .
JOURNAL OF NUCLEAR MATERIALS, 2018, 501 :59-71
[6]   Dual heterogeneous structures lead to ultrahigh strength and uniform ductility in a Co-Cr-Ni medium-entropy alloy [J].
Du, X. H. ;
Li, W. P. ;
Chang, H. T. ;
Yang, T. ;
Duan, G. S. ;
Wu, B. L. ;
Huang, J. C. ;
Chen, F. R. ;
Liu, C. T. ;
Chuang, W. S. ;
Lu, Y. ;
Sui, M. L. ;
Huang, E. W. .
NATURE COMMUNICATIONS, 2020, 11 (01)
[7]   Microstructural stability of Fe-Cr-Al alloys at 450-550 °C [J].
Ejenstam, Jesper ;
Thuvander, Mattias ;
Olsson, Par ;
Rave, Fernando ;
Szakalos, Peter .
JOURNAL OF NUCLEAR MATERIALS, 2015, 457 :291-297
[8]   Oxidation studies of Fe10CrAl-RE alloys exposed to Pb at 550 °C for 10,000 h [J].
Ejenstam, Jesper ;
Halvarsson, Mats ;
Weidow, Jonathan ;
Jonsson, Bo ;
Szakalos, Peter .
JOURNAL OF NUCLEAR MATERIALS, 2013, 443 (1-3) :161-170
[9]   An investigation of FeCrAl cladding behavior under normal operating and loss of coolant conditions [J].
Gamble, K. A. ;
Barani, T. ;
Pizzocri, D. ;
Hales, J. D. ;
Terrani, K. A. ;
Pastore, G. .
JOURNAL OF NUCLEAR MATERIALS, 2017, 491 :55-66
[10]   The influence of nanocrystalline structure and processing route on corrosion of stainless steel: A review [J].
Gupta, R. K. ;
Birbilis, N. .
CORROSION SCIENCE, 2015, 92 :1-15