Hydrogen embrittlement behavior in the nugget zone of friction stir welded X100 pipeline steel

被引:21
作者
Duan, R. H. [1 ]
Wang, Y. Q. [1 ]
Luo, Z. A. [1 ]
Wang, G. D. [1 ]
Xie, G. M. [1 ]
机构
[1] Northeastern Univ, State Key Lab Rolling & Automat, 3 Wenhua Rd, Shenyang 110819, Peoples R China
关键词
Friction stir welding; Pipeline steel; Microstructure; Hydrogen diffusion; Hydrogen embrittlement; INDUCED CRACKING; MICROSTRUCTURAL CONSTITUENTS; BAINITIC STEEL; STRENGTH; PERMEATION; PLASTICITY; TOUGHNESS; DEFORMATION; MECHANISMS; MN;
D O I
10.1016/j.ijhydene.2022.11.262
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Hydrogen-induced damage is an inevitable challenge in pipeline safety applications, especially, the fusion welded joints owing to microstructure heterogeneity caused by welding process. In this work, X100 pipeline steel was subjected to friction stir welding (FSW) at rotation rates of 300-600 rpm under water cooling, and the relationship among the microstructure, hydrogen diffusivity, and hydrogen embrittlement (HE) behavior of the nugget zone (NZ) were studied. The NZ at 600 rpm had the highest effective hydrogen diffusion coefficient (Deff) of 2.1 x 10-10 m2/s because of the highest dislocation density and lowest ratio of effective grain boundary. The Deff decreased with decreasing rotation rate due to the decrease of dislocation density and the increase of ratio of effective grain boundary, and the lowest Deff of 1.32 x 10-10 m2/s was obtained at 300 rpm. After hydrogen charging, the tensile strength of all specimens decreased slightly, while the elongation decreased significantly. As the rotation rate decreased, the elongation loss was obviously inhibited, and ultimately a lowest elongation loss of 31.8% was obtained at 300 rpm. The abovementioned excellent mechanical properties were attributed to the fine ferrite/ martensite structure, low Deff, and strong {111}//ND texture dramatically inhibiting hydrogen-induced cracking initiation and propagation.(c) 2022 Hydrogen Energy Publications LLC. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:8296 / 8309
页数:14
相关论文
共 55 条
[51]   Effects of hydrogen on the fracture toughness of X80 steel base metal and girth weld under strong cathodic current with in-situ hydrogen charging [J].
Xing, Yunying ;
Yang, Zhile ;
Yao, Xingcheng ;
Wang, Xiuyun ;
Lu, Minxu ;
Zhang, Lei ;
Qiao, Lijie .
ENGINEERING FAILURE ANALYSIS, 2022, 135
[52]  
Xue P, 2013, PROCEEDINGS OF THE 1ST INTERNATIONAL JOINT SYMPOSIUM ON JOINING AND WELDING, P445
[53]   Enhanced mechanical properties in friction stir welded low alloy steel joints via structure refining [J].
Xue, P. ;
Komizo, Y. ;
Ueji, R. ;
Fujii, H. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 606 :322-329
[54]   HYDROGEN ASSISTED CRACKING IN C-MN AND LOW-ALLOY STEEL WELDMENTS [J].
YURIOKA, N ;
SUZUKI, H .
INTERNATIONAL MATERIALS REVIEWS, 1990, 35 (04) :217-249
[55]   Hydrogen permeation and embrittlement susceptibility of X80 welded joint under high-pressure coal gas environment [J].
Zhao, Weimin ;
Zhang, Timing ;
Zhao, Yujiao ;
Sun, Jianbo ;
Wang, Yong .
CORROSION SCIENCE, 2016, 111 :84-97