Effect of large pre-deformation on microstructure and mechanical properties of 7B52 laminated aluminum alloy

被引:8
作者
Ding, Xuefeng [1 ]
Liu, Wenhui [1 ,2 ]
Jiang, Bo [3 ]
Qiang, Hu [1 ]
Huang, Hao [4 ]
Xiao, Mingyue [4 ]
Chen, Yuqiang [1 ]
Song, Yufeng [1 ]
机构
[1] Hunan Univ Sci & Technol, Coll Mech & Elect Engn, Xiangtan 411201, Peoples R China
[2] Jimei Univ, Sch Marine Equipment & Mech Engn, Xiamen 361021, Peoples R China
[3] Changzhou Univ, Sch Mat Sci & Engn, Changzhou 213164, Jiangsu, Peoples R China
[4] Jianglu Machinery Elect Grp Co Ltd, Xiangtan 411201, Peoples R China
基金
中国国家自然科学基金;
关键词
Large pre -deformation; Microstructure; Strengthening mechanism; Fracture behavior; MG-CU ALLOY; SC-ZR ALLOY; STRENGTHENING MECHANISMS; TENSILE PROPERTIES; PRECIPITATION; COMPOSITES; COALESCENCE;
D O I
10.1016/j.jallcom.2023.171749
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
With the continuous upgrade of weapons, improving the mechanical properties of 7xxx laminated aluminum alloys for tank armor is a very important task. In this study, the 7B52 laminated aluminum alloy was strengthened through the successive solution treatment, large pre-deformation of 50%, and aging process. The yield strength, ultimate tensile strength, and interlaminar shear bonding strength of this alloy remarkably increased to 558 MPa, 593 MPa, and 93.8 MPa, respectively, which exceeded the values obtained after the traditional solution and aging processes. The effect of the large pre-deformation on the microstructural evolution and mechanical behavior of the 7B52 alloy was examined as well. The mechanical properties depended on the presence of dislocations, low-angle grain boundaries, and tiny precipitates in the alloy structure. The introduction of numerous dislocations and low-angle grain boundaries via large pre-deformation were beneficial for the full precipitation of tiny precipitates during the aging process. According to theoretical calculations, precipitation and dislocation strengthening were the dominant strengthening mechanisms. Moreover, because of its finer grain size, higher dislocation density, and larger number density of precipitates, the 7A62 alloy exhibited higher strength increments than those of the 7A52 alloy after pre-deformation. Therefore, a large predeformation may serve as an effective method for improving the mechanical properties of 7xxx laminated aluminum alloys for their application in the military industry.
引用
收藏
页数:13
相关论文
共 50 条
[31]   Effect of gradient microstructure on the mechanical properties of aluminum alloy [J].
Hassanpour, Hossein ;
Jamaati, Roohollah ;
Hosseinipour, Seyed Jamal .
MATERIALS CHARACTERIZATION, 2021, 174
[32]   Effect of Rolling Deformation on Microstructure and Properties of 7085 Aluminum Alloy [J].
Leng, Jinfeng ;
Dong, Yunfan ;
Ren, Binghui ;
Xu, Xianglei ;
Zhu, Bao ;
Tian, Shuo .
PHYSICS OF METALS AND METALLOGRAPHY, 2021, 122 (14) :1543-1550
[33]   Influence of pre-deformation and subsequent ageing on the hardening behavior and microstructure of 2219 aluminum alloy forgings [J].
Wang, Huimin ;
Yi, Youping ;
Huang, Shiquan .
JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 685 :941-948
[34]   Interface analysis of 7B52 Al alloy laminated composite fabricated by hot-roll bonding [J].
Zhou, Gu-xin ;
Lang, Yu-jing ;
Hao, Jie ;
Liu, Wen ;
Wang, Sheng ;
Qiao, Li ;
Chen, Min .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2016, 26 (05) :1269-1275
[35]   Effect of pre-recovery heat treatment on microstructure and mechanical properties of cold extruded 2219-0.89Ti aluminum alloy [J].
Jin, Xiaopeng ;
Xu, Xiaojing ;
Liu, Zheng ;
Zhang, Bin ;
Zhang, Rikai ;
Zhuang, Yuan ;
Zhang, Peng ;
Wei, Hongbo .
MATERIALS RESEARCH EXPRESS, 2019, 6 (12)
[36]   Effect of pulsed laser frequency on microstructure and mechanical properties of 2219 aluminum alloy welded joints [J].
Zhang, Chao ;
Zhao, Yuhui ;
Liu, Dehua ;
Niu, Fangyong ;
Ma, Guangyi ;
Wu, Dongjiang .
OPTICS AND LASER TECHNOLOGY, 2023, 158
[37]   Effect of pre-deformation on agehardening and microstructure in Al-Mg-Si-Cu alloy [J].
Gu, Yuan ;
Chen, Jianghua ;
Liu, Chunhui ;
Zhu, Donghui ;
Liu, Limei ;
Tao, Guanhui .
Jinshu Xuebao/Acta Metallurgica Sinica, 2015, 51 (11) :1400-1406
[38]   Effect of a Novel Thermomechanical Treatment on Microstructure and Mechanical Properties of 7034 Aluminum Alloy [J].
Xue, Kemin ;
Tian, Zhehuan ;
Wang, Kecheng ;
Li, Yunhui ;
Shi, Wenchao ;
Li, Ping .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2025, 34 (07) :5586-5596
[39]   The Effect of Pre-Deformation on the Microstructure and Hardness of Al-Zn-Mg-Cu Alloy [J].
Zhai, Hongchao ;
Zhang, Lei ;
Xing, Shuohao ;
Hou, Huiying ;
Wang, Zhijie ;
Liu, Sha .
COATINGS, 2025, 15 (03)
[40]   Effect of Pre-Deformation on the Microstructure and Precipitation Behavior of Spray-Formed 7xxx Series Aluminum Alloys [J].
Hou, Huiying ;
Zhang, Lei ;
Xing, Shuohao ;
Zhai, Hongchao ;
Xia, Shule ;
Zhai, Long ;
Wang, Zhijie ;
Liu, Sha .
METALS, 2025, 15 (04)