Effect of Al Concentration on Basal Texture Formation Behavior of AZ-Series Magnesium Alloys during High-Temperature Deformation

被引:2
作者
Kim, Kibeom [1 ]
Ji, Yebin [1 ]
Kim, Kwonhoo [1 ,2 ]
Park, Minsoo [3 ]
机构
[1] Pukyong Natl Univ, Dept Marine Design Convergence Engn, 45 Yongso Ro, Pusan 48513, South Korea
[2] Pukyong Natl Univ, Dept Met Engn, 45 Yongso Ro, Pusan 48513, South Korea
[3] Tohoku Univ, Inst Multidisciplinary Res Adv Mat IMRAM, Katahira 2-1-1, Sendai 9808577, Japan
关键词
magnesium alloy; aluminum content; crystallographic texture; uniaxial compression; AZ-series magnesium alloy; stacking fault energy (SFE); UNIAXIAL COMPRESSION DEFORMATION; DYNAMIC RECRYSTALLIZATION; MG ALLOYS; MICROSTRUCTURE;
D O I
10.3390/ma16062380
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Magnesium and its alloys have been restricted in their industrial applications due to problems related to their formability. To overcome this issue, controlling the crystallographic texture is important, and the texture formation mechanism should be investigated in relation to factors including deformation conditions and solute atoms. In particular, the effects of solute atoms on the texture formation behavior should be further analyzed because they can considerably affect the deformation behavior. Thus, in this study, to clarify the effect of aluminum concentration on the texture formation behavior and microstructure, high-temperature uniaxial compression tests were conducted on three types of AZ-series magnesium alloys (AZ31, AZ61, and AZ91). Compression was conducted at 673 K and 723 K, with strain rates of 0.05 s(-1) and 0.005 s(-1), up to a true strain of -1.0. Cylindrical specimens were prepared from a rolled plate that had a (0001) basal texture and was compressed parallel to the c-axis of the grains. Consequently, work softening and fiber texture formation were observed in all the specimens. During the deformation, the development of grain boundaries, which is a typical characteristic of continuous dynamic recrystallization (CDRX), was observed, and the (0001) texture was highly developed with increasing Al content. Although each alloy was associated with the same deformation conditions and mechanisms, the AZ31 alloy exhibited a non-basal texture component. The stacking fault energy contributed to the generation of slip systems and gliding, and it was seen as the main reason for texture variation.
引用
收藏
页数:13
相关论文
共 50 条
  • [31] High-temperature mechanical properties of AZ61 and AZ61-0.7Si magnesium alloys
    Geranmayeh, R.
    Mahmudi, R.
    Movahedi-Rad, A.
    Malekoshoaraei, M. H.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2012, 50 (06): : 393 - 397
  • [32] Mechanism of Texture and Microstructure Evolution during High Temperature Plane Strain Compression in AZ31B and AZ80 Magnesium Alloys with Various Initial Textures
    Fukutomi, Hiroshi
    Park, Hyung-Gyun
    Kim, Kwon-Hoo
    Okayasu, Kazuto
    Hasegawa, Makoto
    Umezawa, Osamu
    JOURNAL OF THE JAPAN INSTITUTE OF METALS AND MATERIALS, 2019, 83 (08) : 264 - 272
  • [33] The significant effect of adding trace amounts of Ti on the high-temperature deformation behavior of fine-grained Mg-6Al-1Zn magnesium alloys
    Lee, T. J.
    Kim, W. I.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 617 : 352 - 358
  • [34] High temperature deformation behavior of extruded AZ31B magnesium alloy
    Wong, Tsz Wun
    Hadadzadeh, Amir
    Wells, Mary A.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2018, 251 : 360 - 368
  • [35] Effect of deformation temperature on microstructure and texture of AZ31 magnesium alloy processed by new plastic deformation method
    Fan, Yu-tian
    Lu, Li-wei
    Liu, Jian-bo
    Ma, Min
    Huang, Wei-ying
    Wu, Rui-zhi
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2024, 34 (07) : 2138 - 2152
  • [36] Texture evolution in AZ80 magnesium alloy by the plane strain compression deformation at high temperature
    Kim, Jinuk
    Okayasu, Kazuto
    Fukutomi, Hiroshi
    Keikinzoku/Journal of Japan Institute of Light Metals, 2012, 62 (02): : 54 - 59
  • [37] High-temperature tensile behavior of AZ61 magnesium plate prepared by multi-pass friction stir processing
    Luo, X. C.
    Zhang, D. T.
    Cao, G. H.
    Qiu, C.
    Chen, D. L.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 759 : 234 - 240
  • [38] Grain boundary sliding mechanism during high temperature deformation of AZ31 Magnesium alloy
    Roodposhti, Peiman Shahbeigi
    Sarkar, Apu
    Murty, Korukonda Linga
    Brody, Harold
    Scattergood, Ronald
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 669 : 171 - 177
  • [39] Texture formation during high temperature compression deformation in Al-3mass%Mg alloy
    Okayasu, Kazuto
    Fukutomi, Hiroshi
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2006, 70 (07) : 562 - 567
  • [40] Texture formation during high temperature deformation of Al-3amass%Mg solid solution
    Okayasu, K
    Fukutomi, H
    ICOTOM 14: TEXTURES OF MATERIALS, PTS 1AND 2, 2005, 495-497 : 579 - 584