Effect of post-weld heat treatments on the microstructure and mechanical properties of underwater friction stir welded joints of 7003-T4/6060-T4 aluminium alloys

被引:22
作者
Dong, Jialiang [1 ]
Zhang, Datong [2 ]
Zhang, Weiwen [2 ]
Cao, Genghua [3 ]
Qiu, Cheng [2 ]
机构
[1] Guizhou Minzu Univ, Sch Mat Sci & Engn, Guiyang 550025, Peoples R China
[2] South China Univ Technol, Natl Engn Res Ctr Near Net Shape Forming Met Mat, Guangdong Key Lab Proc & Forming Adv Met Mat, Guangzhou 510640, Guangdong, Peoples R China
[3] Guangdong Haomei New Mat Co Ltd, Guangzhou 510640, Qingyuan, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2023年 / 862卷
关键词
Post-weld heat treatment; Underwater friction stir weld; Microstructure; Mechanical properties; GRAIN-GROWTH; CELLULAR MICROSTRUCTURES; TENSILE PROPERTIES; UNIFIED THEORY; STABILITY; BEHAVIOR; RECRYSTALLIZATION; RECOVERY; 2024-T4;
D O I
10.1016/j.msea.2022.144423
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
To further improve the mechanical properties of underwater friction stir welded joints of 7003/6060 aluminium alloys, post-weld heat treatment (PWHT) was carried out. The results show that the combination of water-cooling and PWHT is an efficient method to greatly improve the strength of the dissimilar joints. Through solution heat treatment followed by artificial aging (STA), the largest ultimate tensile strength (UTS) of the dissimilar joint can reach 254.0 MPa, which is equal to the UTS of 6060-T6, and the elongation of the joint is 12.7%. The improvement in strength is attributed to reprecipitation of the high density of the beta" phase. For direct artificial aging (AA) after welding, the largest UTS (218.9 MPa) is obtained when aged at 175 degrees C for 8 h. Although the pre-existing beta ' phase grows coarse to some extent, GP zones and the beta" phase are reprecipitated during AA, which leads to a great increase in joint strength compared with the as-welded samples. However, the elongation severely deteriorates to 4.4% due to strain localization caused by the decreasing width of the soft region. Abnormal grain growth (AGG) takes place in the stir zone (SZ) of all joints subjected to STA, while equiaxed grains with limited growth are retained in joints subjected to AA. Compared with the distribution of precipitation phases, the grain size plays a minor role in the mechanical properties of the dissimilar joints.
引用
收藏
页数:12
相关论文
共 48 条
[1]   Effects of natural aging after pre-aging on clustering and bake-hardening behavior in an Al-Mg-Si alloy [J].
Aruga, Yasuhiro ;
Kozuka, Masaya ;
Takaki, Yasuo ;
Sato, Tatsuo .
SCRIPTA MATERIALIA, 2016, 116 :82-86
[2]   The effect of post-weld heat treatment on the mechanical properties of 2024-T4 friction stir-welded joints [J].
Aydin, Hakan ;
Bayram, Ali ;
Durgun, Ismail .
MATERIALS & DESIGN, 2010, 31 (05) :2568-2577
[3]   Effect of post-weld heat treatment on the mechanical behavior and dislocation density of friction stir welded Al6061 [J].
Baghdadi, Amir Hossein ;
Rajabi, Armin ;
Selamat, Nor Fazilah Mohamad ;
Sajuri, Zainuddin ;
Omar, Mohd Zaidi .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 754 :728-734
[4]   Influence of heat treatment on the coefficient of thermal expansion of Al (6061) based hybrid composites [J].
Benal, Mahagundappa M. ;
Shivanand, H. K. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 435 :745-749
[5]   GP-zones in Al-Zn-Mg alloys and their role in artificial aging [J].
Berg, LK ;
Gjonnes, J ;
Hansen, V ;
Li, XZ ;
Knutson-Wedel, M ;
Waterloo, G ;
Schryvers, D ;
Wallenberg, LR .
ACTA MATERIALIA, 2001, 49 (17) :3443-3451
[6]   Abnormal grain growth in friction stir processed alloys [J].
Charit, I. ;
Mishra, R. S. .
SCRIPTA MATERIALIA, 2008, 58 (05) :367-371
[7]   Atomic pillar-based nanoprecipitates strengthen AlMgSi alloys [J].
Chen, JH ;
Costan, E ;
van Huis, MA ;
Xu, Q ;
Zandbergen, HW .
SCIENCE, 2006, 312 (5772) :416-419
[8]   Transmission electron microscopy investigation of separated nucleation and in-situ nucleation in AA7050 aluminium alloy [J].
Chung, Tsai-Fu ;
Yang, Yo-Lun ;
Huang, Bo-Ming ;
Shi, Zhusheng ;
Lin, Jianguo ;
Ohmura, Takahito ;
Yang, Jer-Ren .
ACTA MATERIALIA, 2018, 149 :377-387
[9]   Evolution of interface and tensile properties in 5052 aluminum alloy/304 stainless steel rotary friction welded joint after post-weld heat treatment [J].
Dong, Honggang ;
Yang, Jiang ;
Li, Yanguang ;
Xia, Yueqing ;
Hao, Xiaohu ;
Li, Peng ;
Sun, Dongsheng ;
Hu, Jianjun ;
Zhou, Wenlong ;
Lei, Mingkai .
JOURNAL OF MANUFACTURING PROCESSES, 2020, 51 (51) :142-150
[10]   EBSD study of underwater friction stir welded AA7003-T4 and AA6060-T4 dissimilar joint [J].
Dong, Jialiang ;
Zhang, Datong ;
Luo, Xicai ;
Zhang, Weiwen ;
Zhang, Wen ;
Qiu, Cheng .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2020, 9 (03) :4309-4318