Microstructural Characterization of Improved Formability of Ti-6Al-4V Sheet by Pulsating Hydraulic Bulging at Room Temperature

被引:4
|
作者
Yapan, Yusuf Furkan [1 ]
Ozturk, Osman [2 ]
Turkoz, Mevlut [2 ]
Dilmec, Murat [3 ]
Livatyali, Haydar [4 ]
Halkaci, Huseyin Selcuk [2 ]
Kotan, Hasan [5 ]
机构
[1] Yildiz Tech Univ, Dept Mech Engn, TR-34349 Istanbul, Turkey
[2] Konya Tech Univ, Dept Mech Engn, TR-42250 Konya, Turkey
[3] Necmettin Erbakan Univ, Dept Mech Engn, TR-42090 Konya, Turkey
[4] Yildiz Tech Univ, Dept Mechatron Engn, TR-34349 Istanbul, Turkey
[5] Necmettin Erbakan Univ, Dept Met & Mat Engn, TR-42090 Konya, Turkey
关键词
formability; microstructural characterization; pulsating hydroforming; stress relaxation; sheet metal forming; Ti-6Al-4V; STRESS-RELAXATION; MECHANICAL-PROPERTIES; TI-6A1-4V ALLOY; TITANIUM; BEHAVIOR; STRAIN; 304-STAINLESS-STEEL; OPTIMIZATION; DUCTILITY;
D O I
10.1007/s11665-022-07550-5
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This study aims to increase the limited formability of the Ti-6Al-4V sheet at room temperature using the pulsating hydraulic bulging and to investigate the microstructural reasons for the increased formability. Accordingly, monotonic and pulsating hydraulic bulge tests (HBTs) were applied to Ti-6Al-4V sheets with 0.55 mm thickness at room temperature, and the underlying microstructural reasons for the improved formability were investigated by conducting detailed microstructural characterizations. The experimental results showed that the pulsating HBT samples reached 15.4% higher bulge dome height than the monotonic HBT samples, and a more homogeneous thickness distribution was achieved by pulsating bulging. The thickness and microhardness distributions, dislocation density estimations, and fracture surface analysis were utilized to correlate the increased formability with the microstructure. It was determined that stress relaxation occurred during the pulsating HBT, resulting in the achieved improved formability. The decrease in the dislocation density in the early stage of forming prevented the locking of the dislocations and delayed the occurrence of the damage, i.e., leading to the increased bulge dome height. The higher plastic deformation resulting from the increased formability also increased the hardness along the cross-section. The increased formability of the Ti-6Al-4V sheet during the pulsating HBT and the underlying microstructural phenomena elaborated in this study are expected to make significant contributions to the current literature on the sheet metals with limited formability at room temperature.
引用
收藏
页码:6258 / 6269
页数:12
相关论文
共 50 条
  • [31] Superplastic Deformation and Microstructural Evolution of Ti-6Al-4V Alloy
    Zhu Tangkui
    Li Miaoquan
    RARE METAL MATERIALS AND ENGINEERING, 2012, 41 (11) : 1970 - 1974
  • [32] Formability and deformation mechanism of Ti-6Al-4V sheet under electropulsing assisted incremental forming
    Ao, Dongwei
    Gao, Jun
    Chu, Xingrong
    Lin, Shuxia
    Lin, Jun
    INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 2020, 202 (357-367) : 357 - 367
  • [33] Microstructural Strengthening and Plastic Degradation of Ti-6Al-4V Induced by Laser Ablation
    Zhang, Yu
    Shi, Xianzhe
    Du, Zhiqin
    Yang, Yahui
    Liu, Xiaochuan
    Li, Yulong
    Shen, Jianghua
    METALS AND MATERIALS INTERNATIONAL, 2023, 30 (4) : 895 - 908
  • [34] Investigation on high-temperature stress relaxation behavior of Ti-6Al-4V sheet
    Luo, Jingfeng
    Xiong, Wei
    Li, Xifeng
    Chen, Jun
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 743 : 755 - 763
  • [35] Microstructural Characterization of Ti-6Al-4V Metal Chips by Focused Ion Beam and Transmission Electron Microscopy
    Schneider, Judy
    Dong, Lei
    Howe, Jane Y.
    Meyer, Harry M., III
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2011, 42A (11): : 3527 - 3533
  • [36] STRUCTURE AND PITTING CORROSION OF Ti-6Al-4V ALLOY AND Ti-6Al-4V WELDS
    Ferdinandov, Nikolay Vasilev
    Gospodinov, Danail Dimitrov
    Ilieva, Mariana Dimitrova
    Radev, Rossen Hristov
    PROCEEDINGS OF THE 7TH INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND SYSTEMS, 2018, : 325 - 330
  • [37] Mechanical and Microstructural Characterization of Cold-Sprayed Ti-6Al-4V After Heat Treatment
    Vo, P.
    Irissou, E.
    Legoux, J. -G.
    Yue, S.
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2013, 22 (06) : 954 - 964
  • [38] Characterization of Ti-6Al-4V Tribopairs: Effect of Thermal Oxidation Treatment
    Durante, Massimo
    Boccarusso, Luca
    Velotti, Carla
    Astarita, Antonello
    Squillace, Antonino
    Carrino, Luigi
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (02) : 571 - 583
  • [39] Microstructural evolution in laser melted boron alloyed Ti-6Al-4V
    Hizli, Huseyin
    Zou, Zhiyi
    Murray, James
    Clare, Adam
    Simonelli, Marco
    JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 981
  • [40] Importance of shielding and mechanical characterization of GTAW on Ti-6AL-4V alloy sheet
    Anbalagan, Karpagaraj
    Ramasubramanian, Sarala
    David, Charles
    Manivannan, S.
    Kannan, A. Rajesh
    Mohan, Dhanesh G.
    WELDING INTERNATIONAL, 2023, 37 (06) : 324 - 333