Surface treatment by crystalline Co-P coating with ultra-thin CoTe2 layer for improved electrical and mechanical properties of the n-type Bi2Te3/Sn TEG electrode

被引:2
作者
Liu, Shuang
Ma, Limin [1 ]
Zhen, Cheng
Li, Dan
Wang, Yishu
Jia, Qiang
Guo, Fu [1 ]
机构
[1] Beijing Univ Technol, Fac Mat & Mfg, Beijing 100124, Peoples R China
基金
中国国家自然科学基金;
关键词
Thermoelectric generator; Bismuth telluride; Co-P coating; Solder; Interfacial diffusion; Intermetallic compound; BI0.5SB1.5TE3; THERMOELECTRIC-MATERIAL; INTERMETALLIC COMPOUNDS; INTERFACIAL REACTION; DIFFUSION BARRIER; MICROSTRUCTURE EVOLUTION; SOLDER JOINTS; SN;
D O I
10.1016/j.apsusc.2023.158856
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Bismuth telluride-based thermoelectric generators (TEG) were widely used in the clean recovery of waste heat, but frequent failure problems at the hot-end electrode interface limited the reliable service of TEGs. Diffusion at the electrode interface between n-type Bi2Te3 and Sn-based solder seriously damaged the performance of the TEGs. In this work, the crystalline Co-4 at.% P coating was deposited to protect the n-type thermoelectric material Bi2Te3. The microstructural characterization proved that the Co-P coating effectively resisted the diffusion of Sn, Bi, Te and Cu atoms, and prevented the generation of brittle intermetallic compounds (IMC) and cracks at the interface. Ultra-thin CoTe2 layer was formed between Co-P and Bi2Te3, much thinner than the brittle Ni-Te layer reported in the literatures. It not only showed that a good metallurgical bond was formed between Co-P and Bi2Te3, but also implied the Co-P only consumed little thermoelectric elements. After the 150-hour aging test at 423 K, the shear strength of the electrode joints did not decrease, and the power generation sustainability of thermoelectric pillars was significantly improved compared with uncoated pillars. Overall, the crystalline Co-P coating would be an excellent candidate to protect the n-type Bi2Te3 pillars of the TEGs.
引用
收藏
页数:13
相关论文
共 40 条
[1]   Ni-W-P layer-induced strength improvement of solder joint in Bi2Te3 thermoelectric module [J].
Bae, Sung Hwa ;
Nguyen, Yen Ngoc ;
Son, Injoon .
SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2023, 28 (05) :399-406
[2]   Interfacial reactions in Sn/Bi2Te3, Sn/Bi2Se3 and Sn/Bi2(Te1-xSex)3 couples [J].
Chen, Sinn-wen ;
Wu, Chih-yu ;
Wu, Hsin-jay ;
Chiu, Wan-ting .
JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 611 :313-318
[3]   Influence of Ni and Cu electrodeposits on the interfacial reaction between SAC305 solder and the Bi2(Te,Se)3 thermoelectric material [J].
Cheng, Jinxuan ;
Hu, Xiaowu ;
Li, Qinglin .
JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2019, 30 (15) :14791-14804
[4]   Improvement of Sn-3Ag-0.5Cu Soldered Joints Between Bi0.5Sb1.5Te3 Thermoelectric Material and a Cu Electrode [J].
Chuang, Tung-Han ;
Hsu, Shih-Wen ;
Lin, Yan-Cheng ;
Yeh, Wei-Ting ;
Chen, Chun-Hao ;
Lee, Pei-Ing ;
Wu, Po-Ching ;
Cheng, Hao-Peng .
JOURNAL OF ELECTRONIC MATERIALS, 2020, 49 (05) :3391-3399
[5]   Recent development and application of thermoelectric generator and cooler [J].
He, Wei ;
Zhang, Gan ;
Zhang, Xingxing ;
Ji, Jie ;
Li, Guiqiang ;
Zhao, Xudong .
APPLIED ENERGY, 2015, 143 :1-25
[6]   Microstructural variation and high-speed impact responses of Sn-3.0Ag-0.5Cu/ENEPIG solder joints with ultra-thin Ni-P deposit [J].
Ho, Cheng-Ying ;
Duh, Jenq-Gong ;
Lin, Chih-Wei ;
Lin, Chun-Jen ;
Wu, Yu-Hui ;
Hong, Huei-Cheng ;
Wang, Te-Hui .
JOURNAL OF MATERIALS SCIENCE, 2013, 48 (06) :2724-2732
[7]   Electroless Co-P diffusion barrier for n-PbTe thermoelectric material [J].
Hsieh, Hsien-Chien ;
Wang, Chun-Hsien ;
Lin, Wen-Chih ;
Chakroborty, Subhendu ;
Lee, Tse-Hsiao ;
Chu, Hsu-Shen ;
Wu, Albert T. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 728 :1023-1029
[8]   Microstructure evolution and shear fracture behavior of aged Sn3Ag0. 5Cu/Cu solder joints [J].
Hu, Xiaowu ;
Xu, Tao ;
Keer, Leon M. ;
Li, Yulong ;
Jiang, Xiongxin .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 673 :167-177
[9]   Interfacial reaction and IMC growth between Bi-containing Sn0.7Cu solders and Cu substrate during soldering and aging [J].
Hu, Xiaowu ;
Li, Yulong ;
Min, Zhixian .
JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 582 :341-347
[10]   The nanoindentation characteristics of Cu6Sn5, Cu3Sn, and Ni3Sn4 intermetallic compounds in the solder bump [J].
Jang, GY ;
Lee, JW ;
Duh, JG .
JOURNAL OF ELECTRONIC MATERIALS, 2004, 33 (10) :1103-1110