Hydration superposition effect and mechanism of steel slag powder and granulated blast furnace slag powder

被引:80
作者
Zhao, Jihui [1 ,2 ,3 ]
Li, Zhangheng [1 ,2 ]
Wang, Dongmin [4 ]
Yan, Peiyu [5 ]
Luo, Lu [1 ,2 ]
Zhang, Hewu [6 ]
Zhang, Haiming [6 ]
Gu, Xiaobo [6 ]
机构
[1] Sun Yat sen Univ, Sch Civil Engn, Zhuhai 519082, Peoples R China
[2] Southern Marine Sci & Engn Guangdong Lab Zhuhai, Zhuhai 519082, Peoples R China
[3] Guangdong Prov Key Lab Marine Civil Engn, Guangzhou 510275, Peoples R China
[4] China Univ Min & Technol, Sch Chem & Environm Engn, Beijing 100083, Peoples R China
[5] Tsinghua Univ, Dept Civil Engn, Beijing 100084, Peoples R China
[6] Ansteel Green Resources Technol Co Ltd, Anshan 114001, Peoples R China
基金
中国国家自然科学基金;
关键词
Steel slag; Granulated blast furnace slag; Hydration superposition effect; Microstructure; Hydration mechanism; CEMENTITIOUS PROPERTIES; CONCRETE; PERFORMANCE; COMPOSITE; PROPERTY; KINETICS; CHINA; IRON;
D O I
10.1016/j.conbuildmat.2022.130101
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Steel slag has great potential as a supplementary cementitious material, and often shows good effects when used in combination with granulated blast furnace slag (GBFS). In order to reveal the interaction law of steel slag and GBFS, the hydration superposition effect and mechanism were studied in this paper in terms of ion dissolution, hydration heat, hydration products, hydration degree, microstructure and mechanical properties. The results show that steel slag and GBFS have a significant hydration superposition effect, and the strength of the paste when the two are used in combination is much higher. The mechanical properties at the early and later ages are the best (16.5 MPa at 7 days and 31 MPa at 28 days) when the steel slag-to-GBFS ratio is 1:1 and 2:3, respec-tively. Steel slag-slag composite powder (SSCP) has three exothermic peaks, which are the dissolution peak, hydration peak of steel slag and pozzolanic ash reaction peak of GBFS (after 85 h), respectively. The fibrous and amorphous C-S-H gels and plate Ca(OH)2 appear in the SSCP pastes at 3 days. Furthermore, the microstructure of hydration products consists of a number of fiber-like and particle-like C-S-H gels with widths ranging from 15 nm to 20 nm and lengths ranging from 50 nm to hundreds of nanometers. The C-S-H gels wrap the unhydrated mineral phase (UMP) to form a nucleus(UMP) -membrane (C-S-H) structure. The early hydration of steel slag would increase the pH and conductivity of the pore solution, promoting the dissolution of aluminosilicate glass in GBFS and pozzolanic ash reaction, at the same time, the consumption of Ca(OH)2 by the pozzolanic ash reaction would promote the further hydration of steel slag. The synergistic hydration effect of SSCP would promote hydration and generate more hydration products to fill the pore structure, resulting in good hardening properties.
引用
收藏
页数:13
相关论文
共 49 条
[31]   The review of early hydration of cement-based materials by electrical methods [J].
Tang, S. W. ;
Cai, X. H. ;
He, Z. ;
Zhou, W. ;
Shao, H. Y. ;
Li, Z. J. ;
Wu, T. ;
Chen, E. .
CONSTRUCTION AND BUILDING MATERIALS, 2017, 146 :15-29
[32]   Characterization of early-age hydration process of cement pastes based on impedance measurement [J].
Tang, S. W. ;
Li, Z. J. ;
Shao, H. Y. ;
Chen, E. .
CONSTRUCTION AND BUILDING MATERIALS, 2014, 68 :491-500
[33]   Evaluation of steel furnace slags as cement additives [J].
Tufekci, M ;
Demirbas, A ;
Genc, H .
CEMENT AND CONCRETE RESEARCH, 1997, 27 (11) :1713-1717
[34]   Evaluation of the engineering properties and durability of mortar produced using ground granulated blast-furnace slag and stainless steel reduced slag [J].
Wang, Her-Yung ;
Wang, Wei-Chien ;
Wang, Jen Chun ;
Chen, Yu-Wen .
CONSTRUCTION AND BUILDING MATERIALS, 2021, 280
[35]   Cementitious properties of super-fine steel slag [J].
Wang, Qiang ;
Yang, Jianwei ;
Yan, Peiyu .
POWDER TECHNOLOGY, 2013, 245 :35-39
[36]   A discussion on improving hydration activity of steel slag by altering its mineral compositions [J].
Wang, Qiang ;
Yan, Peiyu ;
Feng, Jianwen .
JOURNAL OF HAZARDOUS MATERIALS, 2011, 186 (2-3) :1070-1075
[37]   Environmental risks for application of iron and steel slags in soils in China: A review [J].
Wang, Xiaobin ;
Li, Xiuying ;
Yan, Xiang ;
Tu, Cheng ;
Yu, Zhaoguo .
PEDOSPHERE, 2021, 31 (01) :28-42
[38]   Early hydration process of Portland cement paste by electrical measurement [J].
Wei, XS ;
Li, ZJ .
JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2006, 18 (01) :99-105
[39]   Hydration mechanism and orthogonal optimisation of mix proportion for steel slag-slag-based clinker-free prefabricated concrete [J].
Xu, Chengwen ;
Ni, Wen ;
Li, Keqing ;
Zhang, Siqi ;
Li, Ying ;
Xu, Dong .
CONSTRUCTION AND BUILDING MATERIALS, 2019, 228
[40]  
[许远辉 Xu Yuanhui], 2004, [上海大学学报. 自然科学版, Journal of Shanghai University (Natural Science)], V10, P91