Axial compression performance of steel tube columns filled with slurry-wrapping recycled concrete after exposure to high temperatures

被引:3
作者
Wang, Jinhao [1 ]
Li, Zhudan [1 ,2 ]
Jin, Baohong [1 ]
机构
[1] Ningxia Univ, Coll Civil & Hydraul Engn, Yinchuan 750021, Peoples R China
[2] Zhongwei Emergency Management Bur, Zhongwei 755000, Peoples R China
基金
中国国家自然科学基金;
关键词
Concrete-filled steel tube column; High temperature; Axial compression; Slurry-wrapping treatment; Recycled coarse aggregate; Calculation formula; STUB COLUMNS; MECHANICAL-PROPERTIES; AGGREGATE; BEHAVIOR; STRENGTH; OPTIMIZATION; RESISTANCE; FIBER; CO2;
D O I
10.1016/j.pce.2023.103505
中图分类号
P [天文学、地球科学];
学科分类号
07 ;
摘要
Due to frequent fire accidents and stone scarcity, fire protection design and recycled aggregates are issues that needed to be solved in the construction industry. Steel tubes and slurry-wrapping reinforcement treatment can effectively improve the load-bearing capacity of recycled concrete. This paper reports on the mechanical behavior of slurry-wrapping recycled aggregate concrete-filled steel tube (CFST) columns after exposure to high temperatures. Three series of 30 CFST columns were designed with the coarse aggregate type and exposure temperature as variation parameters: natural aggregate concrete-filled steel tube (NACFST) column, recycled aggregate concrete-filled steel tube (RACFST) column, and slurry-wrapping recycled aggregate concrete-filled steel tube (SRACFST) column. The results show that the failure pattern of the specimen is less affected by the exposure temperature and the coarse aggregate type. The compressive strength of the RACFST columns is significantly increased after the slurry-wrapping treatment. With the temperature increasing, the ultimate strength tends to increase initially and then drop. Since the recycled concrete has more pores, the compressive strength loss rate of the RACFST columns is lower than that of the NACFST and SRACFST columns at 800 degrees C. The lateral deformation factor is maintained until the exposure temperature reaches 400 degrees C and then begins to decrease as the temperature increase. It is not accurate to predict the strength of CFST columns after high temperatures by ultrasonic pulse velocity. The predicted strength of CFST column after high temperatures was compared with design codes, and an equation considering the material strength variation was proposed.
引用
收藏
页数:14
相关论文
共 59 条
[11]  
CEN (European Committee for Standardization), 2004, Eurocode 2: Design of concrete structuresPart 1-1: General rules and rules for buildings, DOI DOI 10.2514/2.2772
[12]   Axial compressive behavior of recycled concrete filled steel tubular stub columns with the inclusion of crushed brick [J].
Chen, Jie ;
Zhang, Sumei ;
Wang, Yuyin ;
Geng, Yue .
STRUCTURES, 2020, 26 :271-283
[13]   Bond behavior of recycled aggregate concrete-filled steel tube after elevated temperatures [J].
Chen, Zongping ;
Jia, Hengrui ;
Li, Shengxin .
CONSTRUCTION AND BUILDING MATERIALS, 2022, 325
[14]  
[陈宗平 Chen Zongping], 2015, [建筑结构学报, Journal of Building Structures], V36, P117
[15]   Experimental investigation on recycled aggregate concrete filled steel tubular stub columns under axial compression [J].
de Azevedo, Vanessa da S. ;
de Lima, Luciano R. O. ;
Vellasco, Pedro C. G. da S. ;
Tavares, Maria E. da N. ;
Chan, Tak-Ming .
JOURNAL OF CONSTRUCTIONAL STEEL RESEARCH, 2021, 187
[16]   Post-fire resistance of internally ring stiffened high performance concrete filled steel tube columns [J].
Ekmekyapar, Talha ;
Alhatmey, Ihssan A. H. .
ENGINEERING STRUCTURES, 2019, 183 :375-388
[17]   Experimental behaviour of circular concrete filled steel tube columns and design specifications [J].
Ekmekyapar, Talha ;
Al-Eliwi, Baraa J. M. .
THIN-WALLED STRUCTURES, 2016, 105 :220-230
[18]  
Eurocode4, 2004, DES COMP STEEL CON 1
[19]   Compressive behavior of circular concrete-filled steel tubular columns under freeze-thaw cycles [J].
Gao, Shan ;
Peng, Zhen ;
Guo, Lanhui ;
Fu, Feng ;
Wang, Yonggang .
JOURNAL OF CONSTRUCTIONAL STEEL RESEARCH, 2020, 166
[20]   Residual Mechanical Properties of High-Strength Concretes after Exposure to Elevated Temperatures [J].
Ghandehari, Masoud ;
Behnood, Ali ;
Khanzadi, Mostafa .
JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2010, 22 (01) :59-64