First-Principles Study on the Electronic and Mechanical Properties of the Cr(001)/Al(001) Structure

被引:0
作者
Park, Soon-Dong [1 ]
Kim, Sung Youb [1 ,2 ]
机构
[1] Ulsan Natl Inst Sci & Technol, Grad Sch Carbon Neutral, Ulsan 44919, South Korea
[2] Ulsan Natl Inst Sci & Technol, Dept Mech Engn, Ulsan 44919, South Korea
基金
新加坡国家研究基金会;
关键词
TOTAL-ENERGY CALCULATIONS; SPIN-DENSITY-WAVE; ELASTIC-CONSTANTS; METALS; STABILITY; CR; ELECTRODEPOSITION; EFFICIENCY; INTERFACE; CRYSTALS;
D O I
10.1021/acsomega.3c05827
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
We utilized spin-polarized density functional theory to analyze the properties of the Cr(001)/Al(001) structure. The interface was classified into three forms-bcc, bridge, and top-based on the bonding coordinates between Cr and Al atoms. The total density of states (DOS) of the structures is mainly influenced by the Cr (d) orbitals. The local DOS of the Cr atoms at the interface exhibits slight variations based on their coordination with neighboring Al atoms. The mechanical properties of a specific layer were analyzed by using the rigid grain shift (RGS) method, and the properties of all layers were analyzed by using the homogeneous lattice extension method. Our results confirmed that the bonding strength, as determined by the RGS method, follows a decreasing order from the strongest to the weakest: bcc, bridge, and top. We applied uniform deformation to the entire system in the thickness direction and allowed it to relax: we observed that deformation occurs mainly in the Al region and ultimately leads to failure regardless of the type of interface. Consequently, similar strain-stress curves were observed in all Cr(001)/Al(001) structures. The failure in the Al region is attributed to the lower stiffness of the Al-Al layers compared to the top interface despite the lower work of separation for the top interface.
引用
收藏
页码:42840 / 42848
页数:9
相关论文
共 55 条
[51]   Localised SKP studies of Cathodic Disbondment on Chromium/Chromium Oxide Coated Steel; The Influence of Coating Oxide [J].
Warren, D. J. ;
McMurray, H. N. ;
de Vooys, A. C. A. .
HIGH RESOLUTION CHARACTERIZATION OF CORROSION PROCESSES 3, 2013, 50 (47) :67-78
[52]   Electrodeposition of mixed chromium metal-carbide-oxide coatings from a trivalent chromium-formate electrolyte without a buffering agent [J].
Wijenberg, J. H. O. J. ;
Steegh, M. ;
Aarnts, M. P. ;
Lammers, K. R. ;
Mol, J. M. C. .
ELECTROCHIMICA ACTA, 2015, 173 :819-826
[53]   First-Principles Study on the Grain Boundary Embrittlement of Metals by Solute Segregation: Part I. Iron (Fe)-Solute (B, C, P, and S) Systems [J].
Yamaguchi, Masatake .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2011, 42A (02) :319-329
[54]   Cl-induced passivity breakdown in α-Fe2O3 (0001), α-Cr2O3 (0001), and their interface: A DFT study [J].
Yin, Xiaoran ;
Wang, Haitao ;
Han, En-Hou .
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2022, 129 :70-78
[55]   Effects of B on the Segregation Behavior of Mo at the Fe-Cr(111)/Cr2O3(0001) Interface: A First-Principles Study [J].
Zhang, Yanlu ;
Zhang, Caili ;
Zhang, Zhuxia ;
Dong, Nan ;
Wang, Jian ;
Liu, Ying ;
Lei, Zhibo ;
Han, Peide .
METALS, 2020, 10 (05)