Effect of microstructural evolution during melt pool formation on nano-mechanical properties in LPBF based SS316L parts

被引:19
|
作者
Jeyaprakash, N. [1 ]
Kumar, M. Saravana [2 ]
Yang, Che-Hua [2 ]
Cheng, Yanhai [1 ]
Radhika, N. [3 ]
Sivasankaran, S. [4 ]
机构
[1] China Univ Min & Technol, Sch Mech & Elect Engn, Xuzhou 221116, Peoples R China
[2] Natl Taipei Univ Technol, Grad Inst Mfg Technol, Taipei 10608, Taiwan
[3] Amrita Vishwa Vidyapeetham, Amrita Sch Engn, Dept Mech Engn, Coimbatore, India
[4] Qassim Univ, Coll Engn, Dept Mech Engn, Buraydah 51452, Saudi Arabia
关键词
Additive manufacturing; Steel; Melt pool; Nano-wear; TEM; 316L STAINLESS-STEEL; PROCESS PARAMETERS; LASER; BEHAVIOR; HARDNESS;
D O I
10.1016/j.jallcom.2023.172745
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Laser Powder Bed Fusion (LPBF) based SS316L parts have a wide range of industrial applications, mainly due to their high strength and good structural integrity. However, there is a lack of nano-mechanical studies related to microstructural evolution. The SS316L cubes were examined for grain orientation and phase transformation with the help of OM and FESEM with EDX analysis. Cellular and columnar grains were substantiated by FESEM with EDX. Further, the delta ferrite and gamma austenite phases occurrence was evident in XRD analysis. The orientation of grains was further examined through EBSD analysis. The microstructural transformation was substantiated by mapping based on modulus. Cellular grains showed a maximum hardness of 6 Gpa, whereas the transverse columnar grains displayed a minimum elastic modulus of 105.8 GPa. Nano-wear and scratch analysis predicted the functions caused by the occurrence of cellular dendritic microstructure, and the topographic wear and scratch tracks confirmed the soft nature of transverse columnar grains by forming more pile-up of materials. Strain Rate Sensitivity (SRS) of the SS316L specimens was analysed based on three different strain rates (4.1 x10-5 s-1, 2.08 x10-4 s-1 and 3.3 x10-4 s-1). It was concluded that the LPBFed SS316L parts possessed a negative strain rate. In contrast, the simultaneous attainment of maximum Ultimate Tensile Strength (UTS) and ductility was possible in the quasi-static strain rate.
引用
收藏
页数:13
相关论文
共 23 条
  • [21] Comparing the effect of continuous and pulsed current in the GTAW process of AISI 316L stainless steel welded joint: microstructural evolution, phase equilibrium, mechanical properties and fracture mode
    Tabrizi, Taraneh Reza
    Sabzi, M.
    Anijdan, S. H. Mousavi
    Eivani, A. R.
    Park, N.
    Jafarian, H. R.
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2021, 15 : 199 - 212
  • [22] The effect of pulse current changes in PCGTAW on microstructural evolution, drastic improvement in mechanical properties, and fracture mode of dissimilar welded joint of AISI 316L-AISI 310S stainless steels
    Sabzi, M.
    Anijdan, S. H. Mousavi
    Eivani, A. R.
    Park, N.
    Jafarian, H. R.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 823
  • [23] Effect of Ta on microstructural evolution and mechanical properties of a solid-solution strengthening cast Ni-based alloy during long-term thermal exposure at 700 °C
    Gao, Shuang
    Hou, Jieshan
    Yang, Fei
    Guo, Yongan
    Zhou, Lanzhang
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 729 : 903 - 913