Surface Tensile Strength and Hertzian Fracture Resistance of Patterned Acid-Etched Glass

被引:1
作者
Datsiou, Kyriaki Corinna [1 ]
Overend, Mauro [2 ]
机构
[1] Univ Hertfordshire, Ctr Engn Res, Sch Phys Engn & Comp Sci, Hatfield AL10 9AB, England
[2] Delft Univ Technol, Dept Architectural Engn & Technol, NL-2628 BL Delft, Netherlands
关键词
Frosted glass; Acid-etched glass; Patterned glass; Strength; Ageing; Hertzian fracture; Foot traffic; Hard-body contact strength; Glass fracture interpretation;
D O I
10.1061/JAEIED.AEENG-1464
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Patterned acid-etched glasses are frequently used in horizontal glass surfaces that may be walked on, such as floors and staircase treads. These glasses provide useful antislip properties, but the foot traffic cause contact stresses and ageing mechanisms that are poorly understood and can affect the strength of the acid-etched glass. This study explores these strength-reducing effects by undertaking nondestructive and destructive evaluations of two acid-etched glasses with geometrically different surface patterns and comparing their mechanical performance to unetched float glass. In particular, residual surface stress, Hertzian fracture resistance, and fractographic characteristics are determined for each glass type. The surface tensile strength of the glasses is also evaluated by means of destructive flexural tests before and after artificial ageing. The flexural tests reveal that the ridge areas of the acid-etched surface patterns are more susceptible to the formation of digs and deeper surface flaws and are therefore weaker than both the valley areas of the acid-etched pattern and the surface of the unetched float glass. Correspondingly, the acid-etched glass with the highest proportion of ridges was more susceptible to ageing-induced flaws and had the lowest surface tensile strength. The contact (Hertzian) fracture resistance was also significantly affected by the presence of a surface pattern in the acid-etched glass; specifically, the lowest contact strengths were recorded for hard body contact on the ridges of the pattern. The fracture phenomena and new data presented in this paper provide useful insights on the long-term performance of etched patterned glass. The findings can provide the bases for real-world design decisions and for glass forensics.
引用
收藏
页数:14
相关论文
共 26 条
[21]   A computer algorithm for determining the tensile strength of float glass [J].
Overend, M. ;
Zammit, K. .
ENGINEERING STRUCTURES, 2012, 45 :68-77
[22]   Influence of glass composition on the kinetics of glass etching and frosting in concentrated HF solutions [J].
Piret, Nicolas ;
Santoro, Ronny ;
Dogot, Loick ;
Barthelemy, Bastien ;
Peyroux, Eugenie ;
Proost, Joris .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 2018, 499 :208-216
[23]  
Quinn GD., 2007, Fractography of ceramics and glasses, NIST Special Publication, V960-16, p8
[24]   WET CHEMICAL ETCHING OF SILICATE-GLASSES IN HYDROFLUORIC-ACID BASED SOLUTIONS [J].
SPIERINGS, GACM .
JOURNAL OF MATERIALS SCIENCE, 1993, 28 (23) :6261-6273
[25]   Effect of normal scratch load and HF etching on the mechanical behavior of annealed and chemically strengthened aluminosilicate glass [J].
Wang, Zhen ;
Guan, Tianhao ;
Ren, Tengfei ;
Wang, Haokang ;
Suo, Tao ;
Li, Yulong ;
Iwamoto, Takeshi ;
Wang, Xiang ;
Wang, Yinmao ;
Gao, Guozhong .
CERAMICS INTERNATIONAL, 2020, 46 (04) :4813-4823
[26]   HERTZIAN FRACTURE TEST [J].
WILSHAW, TR .
JOURNAL OF PHYSICS D-APPLIED PHYSICS, 1971, 4 (10) :1567-&