Photodegradation behavior and blocking strategy of waterborne polyurethane under UV and Xenon irradiation

被引:6
|
作者
Gao, Qiang [1 ]
Wang, Li [1 ]
Luo, Haihang [1 ]
Fan, Haojun [1 ]
Xiang, Jun [1 ]
Yan, Jun [1 ]
Li, Chengxiang [2 ]
Chen, Zhijun [2 ]
机构
[1] Sichuan Univ, Key Lab Leather Chem & Engn, Minist Educ, Chengdu 610065, Peoples R China
[2] Dymat Post Polymer Mat Ltd Co, Taizhou 323000, Zhejiang, Peoples R China
来源
MATERIALS TODAY COMMUNICATIONS | 2023年 / 34卷
关键词
Waterborne polyurethane; UV and Xenon photodegradation; Mechanism; Blocking strategy; Composite additives; THERMOPLASTIC POLYURETHANE; DEGRADATION; TEMPERATURE; EXPOSURE;
D O I
10.1016/j.mtcomm.2022.105212
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Waterborne polyurethane (WPU) materials are vulnerable to be destroyed under long-term sunlight exposure, reducing their service life. Therefore, it is necessary to investigate the photodegradation behavior and blocking strategy of WPU. In general, UV and Xenon light sources are often used to accelerate photodegradation process to shorten the experimental time. In this work, the blocked and un-blocked WPU were synthesized and the dif-ference in photodegradation behavior under UV and Xenon irradiation was preliminarily investigated. The re-sults showed that the urethane bonds of WPU were cleaved and ether linkages were oxidized and degraded, generating some primary degradation products after UV and Xenon irradiation, the primary degradation prod-ucts can continue to decompose or re-construct after UV exposure, inducing deeper yellowing and more cracks or holes on the surface of the film. Fortunately, this photodegradation behavior can be blocked by addition of composite additives according to the photodegradation mechanism. The morphology, structure and properties of the blocked WPU changed slightly after UV irradiation and kept almost unchanged after Xenon exposure. In comparison with control sample, the tensile strength retention ratio increased from 9.3% to 77.5% for UV exposure 72 h and from 12.4% to 88.4% for Xenon irradiation 72 h, which confirmed that the proposed blocking strategy was successful and effective.
引用
收藏
页数:12
相关论文
共 50 条
  • [41] Photodegradation of methylene blue under UV and visible light irradiation by Er2O3-coated silicon nanowires as photocatalyst
    Brik, Afaf
    Naama, Sabrina
    Hadjersi, Toufik
    Benamar, Mohamed El Amine
    Bouanik, Sihem
    Manseri, Amar
    REACTION KINETICS MECHANISMS AND CATALYSIS, 2020, 131 (01) : 525 - 536
  • [42] Achievement of Both Mechanical Properties and Intrinsic Self-Healing under Body Temperature in Polyurethane Elastomers: A Synthesis Strategy from Waterborne Polymers
    Zhang, Liangdong
    Qiu, Teng
    Sun, Xiting
    Guo, Longhai
    He, Lifan
    Ye, Jun
    Li, Xiaoyu
    POLYMERS, 2020, 12 (04)
  • [43] Unveiling the Photodegradation Mechanism of Monochlorinated Naphthalenes under UV-C Irradiation: Affecting Factors Analysis, the Roles of Hydroxyl Radicals, and DFT Calculation
    Yu, Yingtan
    Liu, Mengdi
    Wang, Shimeng
    Zhang, Chaoxing
    Zhang, Xue
    Liu, Li
    Xue, Shuang
    MOLECULES, 2024, 29 (19):
  • [44] Assessing the efficacy of iron (II, III) oxide nanocomposite for the photodegradation of organic dye pollutants and textile wastewater under UV-visible irradiation
    Gharehlar, Mahnaz Parastar
    Sheshmani, Shabnam
    Nikmaram, Farrokh Roya
    Doroudi, Zohreh
    CHEMICAL PAPERS, 2024, 78 (03) : 2015 - 2032
  • [45] Synthesis and characterization of TiO2-montmorillonites doped with vanadium and/or carbon and their application for the photodegradation of sulphorhodamine B under UV-vis irradiation
    Chen, Ke
    Li, Jingyi
    Li, Jie
    Zhang, Yumin
    Wang, Wenxi
    COLLOIDS AND SURFACES A-PHYSICOCHEMICAL AND ENGINEERING ASPECTS, 2010, 360 (1-3) : 47 - 56
  • [46] Enhanced photodegradation of methyl orange dye under UV irradiation using MoO3 and Ag doped TiO2 photocatalysts
    Kader, Shahina
    Al-Mamun, Md. Rashid
    Suhan, Md. Burhan Kabir
    Shuchi, Sanzeeda Baig
    Islam, Md. Shahinoor
    ENVIRONMENTAL TECHNOLOGY & INNOVATION, 2022, 27
  • [47] Facile synthesis of Y2O3/CuO nanocomposites for photodegradation of dyes/mixed dyes under UV- and visible light irradiation
    El-Sayed, F.
    Ganesh, V
    Hussien, Mai S. A.
    AlAbdulaal, T. H.
    Zahran, H. Y.
    Yahia, I. S.
    Abdel-wahab, Mohamed Sh
    Shakir, Mohd
    Bitla, Yugandhar
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 19 : 4867 - 4880
  • [48] Photodegradation of azo dye Congo Red from aqueous solution by the WO3-TiO2/activated carbon (AC) photocatalyst under the UV irradiation
    Sun, Jian-hui
    Wang, Yong-kui
    Sun, Rui-xia
    Dong, Shu-ying
    MATERIALS CHEMISTRY AND PHYSICS, 2009, 115 (01) : 303 - 308
  • [49] Sol-gel preparation of metal and nonmetal-codoped TiO2-graphene nanophotocatalyst for photodegradation of MO under UV and visible-light irradiation
    Rotami, Mojtaba
    Hamadanian, Masood
    Rahimi-Nasrabadi, Mehdi
    Ganjali, Mohammad Reza
    IONICS, 2019, 25 (04) : 1869 - 1878
  • [50] Highly Active S-Modified ZnFe2O4 Heterogeneous Catalyst and Its Photo-Fenton Behavior under UV-Visible Irradiation
    Liu, Liangjun
    Zhang, Guoliang
    Wang, Ling
    Huang, Tao
    Qin, Lei
    INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2011, 50 (12) : 7219 - 7227