Adhesive Performance of Resin Cement to Glass-Ceramic and Polymer-Based Ceramic CAD/CAM Materials after Applying Self-Etching Ceramic Primer or Different Surface Treatments

被引:4
|
作者
Turunc Oguzman, Rana [1 ]
Sismanoglu, Soner [2 ]
机构
[1] Altınbaş Univ, Fac Dent, Dept Prosthodont, TR-34147 Istanbul, Turkiye
[2] Istanbul Univ Cerrahpasa, Fac Dent, Dept Restorat Dent, TR-34098 Istanbul, Turkiye
关键词
CAD/CAM materials; surface treatments; self-etching ceramic primer; 10-MDP; bond strength; BOND STRENGTH; ROUGHNESS; COMPOSITE;
D O I
10.3390/ma17010002
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Ensuring optimum bond strength during cementation is vital for restoration success, with the practicality of the process being crucial in clinical practice. This study analyzed the effect of a single-step self-etching ceramic primer (MEP) and various surface treatments on the microshear bond strength (mu SBS) between resin cement and glass-ceramic or polymer-based ceramic CAD/CAM materials. Specimens were fabricated from leucite-based glass-ceramic (LEU), lithium disilicate glass-ceramic (LDC), resin nanoceramic (RNC), and polymer infiltrated ceramic network (PICN) (n = 160). They were then classified based on the surface treatments (n = 10): control (no treatment); sandblasting with Al2O3 (AL); etching with hydrofluoric acid (HF); and MEP application. Scanning electron microscopy was used to evaluate the surface topography. mu SBS was measured after cementation and thermocycling procedures. Failure modes were examined with a stereomicroscope. Statistical analysis involved two-way analysis of variance and Tukey HSD tests with a significance level of 0.05. mu SBS was significantly influenced by both surface treatment and CAD/CAM material type. The most enhanced mu SBS values for each material, regarding the surface treatment, were: LEU and LDC, HF; RNC, AL; PICN, AL or HF. MEP significantly increased the mu SBS values of CAD/CAM materials except RNC, yet it did not yield the highest mu SBS values for any of them.
引用
收藏
页数:13
相关论文
共 33 条
  • [31] Impact of various clinical factors on the final color of ceramic/glass-polymer based CAD-CAM materials
    Yilmaz, Sebnem
    Egilmez, Ferhan
    AMERICAN JOURNAL OF DENTISTRY, 2023, 36 (01) : 8 - 14
  • [32] Effect of Thickness and Shade of Resin and Ceramic-Based Hybrid Materials on Color Masking Abilities and Optical Performance of CAD/CAM Materials
    Husain, Nadin Al-Haj
    Walther, Lorenz
    Ozcan, Mutlu
    Bragger, Urs
    Joda, Tim
    EUROPEAN JOURNAL OF PROSTHODONTICS AND RESTORATIVE DENTISTRY, 2021, 29 (01) : P14 - P21
  • [33] CAD-CAM milled versus pressed lithium-disilicate monolithic crowns adhesively cemented after distinct surface treatments: Fatigue performance and ceramic surface characteristics
    Schestatsky, Ricardo
    Zucuni, Camila Pauleski
    Venturini, Andressa Borin
    de Lima Burgo, Thiago Augusto
    Bacchi, Atais
    Valandro, Luiz Felipe
    Rocha Pereira, Gabriel Kalil
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2019, 94 : 144 - 154