Hydrogen effect on mechanical properties and cracking of creep-resistant 9% Cr P92 steel and P91 weld metal

被引:2
作者
Rhode, Michael [1 ,2 ]
Nietzke, Jonathan [1 ]
Richter, Tim [1 ]
Mente, Tobias [1 ]
Mayr, Peter [3 ]
Nitsche, Alexander [4 ]
机构
[1] Bundesanstalt Mat Forsch & Prufung BAM, Dept Component Safety 9, Unter Eichen 87, Berlin, Germany
[2] Otto Von Guericke Univ, Inst Mat Sci & Joining Technol, Magdeburg, Germany
[3] Tech Univ Munich, Dept Mech Engn, Chair Mat Engn Addit Mfg, Garching, Germany
[4] ZABAG Secur Engn GmbH, Grunhainichen, Germany
关键词
Creep-resisting materials; Diffusion; Hydrogen embrittlement; Weld metal; HEAT-TREATMENT; EMBRITTLEMENT; MICROSTRUCTURE; DIFFUSION;
D O I
10.1007/s40194-022-01410-5
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Martensitic 9% Cr steels like P91 and P92 can show an increased susceptibility to delayed hydrogen-assisted cracking. The focus of this study was the microstructure and heat treatment effect on the mechanical properties of P92 base material and P91 multi-layer weld metal in both as-welded and post weld heat treated (PWHT) condition. Tensile tests with hydrogen-free reference samples and electrochemically hydrogen charged samples were carried out; the mechanical properties were assessed and supported by detailed fractographic analysis. Finally, a hydrogen and microstructure-dependent fracture criterion is established. All investigated microstructures showed a hydrogen-influenced degradation of the mechanical properties compared to the hydrogen-free reference samples. The as-welded martensitic P91 weld metal had the highest degree of degradation in the presence of hydrogen. The P91 PWHT weld metal and the P92 base material had comparable properties. From that point of view, a significantly increased risk for hydrogen-assisted cold cracking during welding fabrication of P91 weld joints must be considered before any heat treatment is conducted.
引用
收藏
页码:183 / 194
页数:12
相关论文
共 42 条
[1]  
Abd El-Rahman Abd El-Salam M., 2013, International Heat Treatment & Surface Engineering, V7, P32, DOI 10.1179/1749514813Z.00000000051
[2]   Protective Coatings for High Temperature Molten Salt Heat Storage Systems in Solar Concentration Power Plants [J].
Aguero, Alina ;
Audigie, Pauline ;
Rodriguez, Sergio ;
Encinas-Sanchez, Victor ;
Teresa de Miguel, Ma ;
Javier Perez, Francisco .
INTERNATIONAL CONFERENCE ON CONCENTRATING SOLAR POWER AND CHEMICAL ENERGY SYSTEMS (SOLARPACES 2017), 2018, 2033
[3]   Influence of alloying on hydrogen-assisted cracking and diffusible hydrogen content in Cr-Mo steel welds [J].
Albert, S.K. ;
Ramasubbu, V. ;
Parvathavarthini, N. ;
Gill, T.P.S. .
Sadhana - Academy Proceedings in Engineering Sciences, 2003, 28 (3-4) :383-393
[4]  
[Anonymous], 2015, MAN SPEC WELD WIR BO
[5]  
[Anonymous], 36902018 EN ISO, DOI [10.31030/3002668, DOI 10.31030/3002668]
[6]  
[Anonymous], 1021622014 EN, DOI [10.31030/3068303, DOI 10.31030/3068303]
[7]  
[Anonymous], 1764212004 ISO, DOI [10.31030/9519379, DOI 10.31030/9519379]
[8]  
[Anonymous], 176342015 EN ISO, DOI [10.31030/2353520, DOI 10.31030/2353520]
[9]   Numerical model for hydrogen-assisted cracking [J].
Boellinghaus, T ;
Hoffmeister, H .
CORROSION, 2000, 56 (06) :611-622
[10]  
Brozda J., 2005, Welding International, V19, P5, DOI 10.1533/wint.2005.3370