Role of extrusion rate on the microstructure and tensile properties evolution of ultrahigh-strength low-alloy Mg-1.0Al-1.0Ca-0.4Mn (wt.%) alloy

被引:47
作者
Liu, X. Q. [1 ]
Qiao, X. G. [1 ]
Pei, R. S. [2 ]
Chi, Y. Q. [1 ]
Yuan, L. [1 ]
Zheng, M. Y. [1 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
[2] Rhein Westfal TH Aachen, Inst Met Kunde & Met Phys, D-52056 Aachen, Germany
关键词
Mg-Al-Ca-Mn alloy; Ultrafine grain; Extrusion rate; Grain boundary segregation; Microstructure; Ultrahigh strength; MECHANICAL-PROPERTIES; TEXTURE; STRAIN; RECRYSTALLIZATION; SEGREGATION; DUCTILITY; CALCIUM; SPEED;
D O I
10.1016/j.jma.2021.05.010
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Mg-1.0Al-1.0Ca-0.4Mn (AXM1104, wt.%) low alloy was extruded at 200 degrees C with an extrusion ratio of 25 and different ram speeds from 1.0 to 7.0 mm/s. The influence of extrusion rate on microstructure and mechanical properties of the AXM1104 alloy was systematically studied. With the increasing of extrusion rate, the mean dynamically recrystallized (DRXed) grain size of the low alloy and average particles diameter of precipitate second phases were increased, while the degree of grain boundary segregation and the intensity of the basal fiber texture were decreased. With the rising of extrusion rate from 1.0 to 7.0 mm/s, the tensile yield strength (TYS) of the as-extruded AXM1104 alloy was decreased from 445 MPa to 249 MPa, while the elongation to failure (EL) was increased from 5.0% to 17.6%. The TYS, ultimate tensile strength (UTS) and EL of the AXM1104 alloy extruded at the ram speed of 1.5 mm/s was 412 MPa, 419 MPa and 12.0%, respectively, exhibiting comprehensive tensile mechanical properties with ultra-high strength and excellent plasticity. The ultra-high TYS of 412 MPa was mainly due to the strengthening from ultra-fine DRXed grains with segregation of solute atoms at grain boundaries. The strain hardening rate is increase slightly with increasing extrusion speed, which may be ascribed to the increasing mean DRXed grain size with rising extrusion speed. The higher strain hardening rate contributes to the higher EL of these AXM1104 samples extruded at higher ram speed. (c) 2021 Chongqing University. Publishing services provided by Elsevier B.V. on behalf of KeAi Communications Co. Ltd. This is an open access article under the CC BY-NC-ND license ( http://creativecommons.org/licenses/by-nc-nd/4.0/ ) Peer review under responsibility of Chongqing University
引用
收藏
页码:553 / 561
页数:9
相关论文
共 50 条
[31]   Ca Addition Effects on the Microstructure, Tensile and Corrosion Properties of Mg Matrix Alloy Containing 8 wt.% Mg2Si [J].
Lotfpour, M. ;
Emamy, M. ;
Dehghanian, C. ;
Pourbahari, B. .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2018, 27 (02) :411-422
[32]   Microstructure and Properties of Novel Mg-Al-Zn-Mn-Ca-Ni Dissoluble Alloy Fabricated by Industrial Two-Step Extrusion Method [J].
Wang, Jian ;
Li, Hongxiang ;
Wang, Jinhui ;
Liu, Yaohong ;
Zhang, Jishan .
METALS, 2022, 12 (04)
[33]   Effects of extrusion temperature on the microstructure and mechanical properties of low-alloyed Mg-Bi-Ca-Mn alloy [J].
Huang, Weiying ;
Su, Yongheng ;
Gan, Kefu ;
Chen, Jian ;
Qiu, Wei ;
Zhou, Xiaojie ;
Yu, Qiang ;
Liang, Liang ;
Chen, Wei ;
Zhou, Libo .
INTERMETALLICS, 2024, 175
[34]   Effect of cooling rate on microstructure and mechanical properties of an Al-5.0Mg-3.0Zn-1.0Cu cast alloy [J].
Tang, Hua-Ping ;
Wang, Qu-Dong ;
Lei, Chuan ;
Ye, Bing ;
Wang, Kui ;
Jiang, Hai-Yan ;
Ding, Wen Jiang ;
Zhang, Xiang-Feng ;
Lin, Zhen ;
Zhang, Ji-Bin .
JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 801 :596-608
[35]   Study on the microstructure and properties of Mg-Zn-Mn-Ca alloy subjected to low-temperature extrusion-rolling composite deformation [J].
Sha, Sha ;
Wang, Feng ;
Li, Rongguang ;
Song, Xue ;
Zhang, Hang ;
Liu, Boshu ;
Li, Shanshan ;
Tang, Yan .
MATERIALS TODAY COMMUNICATIONS, 2025, 42
[36]   Effect of 1.0 wt. % Zn addition on the microstructure, mechanical properties, and bio-corrosion behaviour of micro alloyed Mg-0.24Sn-0.04Mn alloy as biodegradable material [J].
El-Mahallawy, Nahed ;
Palkowski, Heinz ;
Klingner, Anke ;
Diaa, Alia ;
Shoeib, Madiha .
MATERIALS TODAY COMMUNICATIONS, 2020, 24
[37]   Room temperature tensile creep behavior of Mg-6Zn-0.4Mn-0.3Al-0.2Ca (wt%) alloy containing icosahedral quasicrystals [J].
Ying, Yu-Lei ;
Guan, Zhi-Ping ;
Wang, Xuan ;
Wang, Gang ;
Yan, Wei .
MATERIALS TODAY COMMUNICATIONS, 2024, 39
[38]   Improving tensile properties of a room-temperature formable and heat-treatable Mg-6Zn-0.2Ca (wt.%) alloy sheet via micro-alloying of Al and Mn [J].
Nakata, T. ;
Xu, C. ;
Kamado, S. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 772
[39]   Role of Mn Addition in Tuning the Microstructure and Mechanical Properties of Mg-Al-Ca Dilute Alloy [J].
Ge, Chuncheng ;
Sun, Xinyu ;
Li, Jingren ;
Xie, Dongsheng ;
Yang, Chubin ;
Pan, Hucheng ;
Qin, Gaowu .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (11) :5109-5115
[40]   Tensile creep behavior of a die-cast Mg-6Al-0.2Mn-2Ca-0.3Si (wt.%) alloy [J].
Sakai, Takahiro ;
Nakata, Taiki ;
Miyamoto, Takeaki ;
Kamado, Shigeharu ;
Liao, Jinsun .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 774