High Voltage Cycling Stability of LiF-Coated NMC811 Electrode

被引:12
|
作者
Llanos, Princess Stephanie [1 ]
Ahaliabadeh, Zahra [1 ]
Miikkulainen, Ville [1 ]
Lahtinen, Jouko [2 ]
Yao, Lide [3 ]
Jiang, Hua [3 ]
Kankaanpaa, Timo [4 ]
Kallio, Tanja M. [1 ]
机构
[1] Aalto Univ, Sch Chem Engn, Dept Chem & Mat Sci, Espoo 02150, Finland
[2] Aalto Univ, Sch Sci, Dept Appl Phys, Espoo 02150, Finland
[3] Aalto Univ, OtaNano Nanomicroscopy Ctr, Espoo 02150, Finland
[4] Umicore Finland Oy, Kokkola 67101, Finland
关键词
NMC811; high voltage cycling; electrode coating; LiF; atomic layer deposition; cathode electrolyteinterface; ATOMIC LAYER DEPOSITION; LITHIUM-ION BATTERIES; ELECTROCHEMICAL PERFORMANCE; CATHODE MATERIAL; NI-RICH; POSITIVE ELECTRODE; RATE CAPABILITY; THIN-FILMS; LINI0.8CO0.1MN0.1O2; MECHANISMS;
D O I
10.1021/acsami.3c14394
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The development of LiNi0.8Mn0.1Co0.1O2 (NMC811) as a cathode material for high-energy-density lithium-ion batteries (LIBs) intends to address the driving limitations of electric vehicles. However, the commercialization of this technology has been hindered by poor cycling stability at high cutoff voltages. The potential instability and drastic capacity fade stem from irreversible parasitic side reactions at the electrode-electrolyte interface. To address these issues, a stable nanoscale lithium fluoride (LiF) coating is deposited on the NMC811 electrode via atomic layer deposition. The nanoscale LiF coating diminishes the direct contact between NMC811 and the electrolyte, suppressing the detrimental parasitic reactions. LiF-NMC811 delivers cycling stability superior to uncoated NMC811 with high cutoff voltage for half-cell (3.0-4.6 V vs Li/Li+) and full-cell (2.8-4.5 V vs graphite) configurations. The structural, morphological, and chemical analyses of the electrodes after cycling show that capacity decline fundamentally arises from the electrode-electrolyte interface growth, irreversible phase transformation, transition metal dissolution and crossover, and particle cracking. Overall, this work demonstrates that LiF is an effective electrode coating for high-voltage cycling without compromising rate performance, even at high discharge rates. The findings of this work highlight the need to stabilize the electrode-electrolyte interface to fully utilize the high-capacity performance of NMC811.
引用
收藏
页码:2216 / 2230
页数:15
相关论文
共 50 条
  • [21] Unlocking Stable Multi-Electron Cycling in NMC811 Thin-Films between 1.5-4.7 V
    Aribia, Abdessalem
    Sastre, Jordi
    Chen, Xubin
    Futscher, Moritz H.
    Rumpel, Matthias
    Priebe, Agnieszka
    Doebeli, Max
    Osenciat, Nicolas
    Tiwari, Ayodhya N.
    Romanyuk, Yaroslav E.
    ADVANCED ENERGY MATERIALS, 2022, 12 (40)
  • [22] Effect of Annealing on the Structure, Composition, and Electrochemistry of NMC811 Coated with Al2O3 Using an Alkoxide Precursor
    Riesgo-Gonzalez, Victor
    Hall, David S.
    Marker, Katharina
    Slaughter, Jonathan
    Wright, Dominic S.
    Grey, Clare P.
    CHEMISTRY OF MATERIALS, 2022, 34 (21) : 9722 - 9735
  • [23] Effect of Ambient Storage on the Degradation of Ni-Rich Positive Electrode Materials (NMC811) for Li-Ion Batteries
    Jung, Roland
    Morasch, Robert
    Karayaylali, Pinar
    Phillips, Katherine
    Maglia, Filippo
    Stinner, Christoph
    Shao-Horn, Yang
    Gasteiger, Hubert A.
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2018, 165 (02) : A132 - A141
  • [24] Effect of charging protocols on electrochemical performance and failure mechanism of commercial level Ni-rich NMC811 thick electrode
    Phattharasupakun, Nutthaphon
    Bunyanidhi, Panyawee
    Chiochan, Poramane
    Chanlek, Narong
    Sawangphruk, Montree
    ELECTROCHEMISTRY COMMUNICATIONS, 2022, 139
  • [25] Synthesis of Tantalum Doped NMC811 and Its Impact on Crystal Structure and Electrochemical Performance at Higher Upper Cut-off Voltage
    Dalkilic, Mert
    Schmidt, Alexander
    Schladt, Thomas D.
    Axmann, Peter
    Wohlfahrt-Mehrens, Margret
    Linden, Mika
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2022, 169 (09)
  • [26] Physical vapor deposited coatings on high Ni content NMC811 Li-ion battery cathode powder
    Kurinjimala, R.
    Boehm, D.
    Pessenhofer, W.
    Eisenmenger-Sittner, C.
    SURFACE & COATINGS TECHNOLOGY, 2023, 462
  • [27] Ti-Modification of Grain Boundaries for Enhanced High Voltage Cycling Stability of NCM811
    Huang, Kai
    Mu, Xulin
    Ding, Yang
    Li, Jinhui
    Sui, Manling
    Yan, Pengfei
    ACS APPLIED ENERGY MATERIALS, 2024, 7 (11): : 4856 - 4865
  • [28] Evolution of Structure and Lithium Dynamics in LiNi0.8Mn0.1Co0.1O2 (NMC811) Cathodes during Electrochemical Cycling
    Marker, Katharina
    Reeves, Philip J.
    Xu, Chao
    Griffith, Kent J.
    Grey, Clare P.
    CHEMISTRY OF MATERIALS, 2019, 31 (07) : 2545 - 2554
  • [29] Mechanistic Understanding of Additive Reductive Degradation and SEI Formation in High-Voltage NMC811||SiOx-Containing Cells via Operando ATR-FTIR Spectroscopy
    Weiling, Matthias
    Lechtenfeld, Christian
    Pfeiffer, Felix
    Frankenstein, Lars
    Diddens, Diddo
    Wang, Jian-Fen
    Nowak, Sascha
    Baghernejad, Masoud
    ADVANCED ENERGY MATERIALS, 2024, 14 (05)
  • [30] A Timescale characterization of (NMC811)/SiOx-graphite 1Ah pouch cell: Improving cycling stability with carbonate-based electrolytes and triallyl phosphate (TAP) co-additive
    Mehranjani, Alireza Soleimany
    Golmohammad, Mohammad
    Bozorgmehri, Shahriar
    Abdoli, Hamid
    JOURNAL OF POWER SOURCES, 2024, 602