WC-Co-TiNbZr composite with simultaneously high hardness and fracture toughness

被引:6
|
作者
Zhou, Bin [1 ]
Wang, Haibin [1 ]
Lu, Hao [1 ]
Liu, Xuemei [1 ]
Liu, Chao [2 ]
Wen, Xiao [2 ]
Fan, Chaoying [2 ]
Song, Xiaoyan [1 ]
机构
[1] Beijing Univ Technol, Fac Mat & Mfg, Key Lab Adv Funct Mat, Minist Educ China, Beijing 100124, Peoples R China
[2] Xiamen Tungsten Co Ltd, Xiamen 361009, Peoples R China
基金
中国国家自然科学基金;
关键词
WC-based composite; Shape memory alloy; Intermediate phase; Toughening mechanism; MECHANICAL-PROPERTIES; CEMENTED CARBIDES; SHAPE-MEMORY; NBC; MICROSTRUCTURE; VC; FABRICATION; STRENGTH; SPS;
D O I
10.1016/j.ijrmhm.2023.106332
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, the shape memory alloy of TiNb24Zr6 was firstly prepared and then introduced into WC-Co and a new type of WC-Co-TiNbZr composite was fabricated. The phase constitution, element distribution, microstructure, and mechanical properties were systematically characterized. It was found that the added TiNb24Zr6 reacted with the WC matrix and an intermediate (Ti,Nb)C phase formed during the sintering process. As a result, the shape memory effect of TiNb24Zr6 did not play a part in the plastic deformation of the composite. On the other side, the produced (Ti,Nb)C phase played a significant role in the mechanical behavior of the composite. Due to the difference in the elastic modulus between (Ti,Nb)C and WC, cracks deflection and bridging occurred in the vicinity of (Ti,Nb)C under mechanical loading. Moreover, the produced (Ti,Nb)C had a specific coherent interfacial relationship with the WC matrix, which enhanced the interfacial bonding strength and resistance against intergranular fracture of the composite. The hardness and fracture toughness of the present composite achieved 1943.5 & PLUSMN; 12.8 kgf/mm2 and 17.3 & PLUSMN; 0.5 MPa & BULL;m1/2 respectively, which are superior compared with those of the counterparts reported in the literature. The strengthening and toughening mechanisms disclosed in this study will be applicable to a wide range of WC-based composites to achieve excellent comprehensive mechanical properties.
引用
收藏
页数:10
相关论文
共 50 条
  • [1] Nanocrystalline WC-Co composite with ultrahigh hardness and toughness
    Peng, Yong
    Wang, Haibin
    Zhao, Chong
    Hu, Huaxin
    Liu, Xuemei
    Song, Xiaoyan
    COMPOSITES PART B-ENGINEERING, 2020, 197
  • [2] Influence of Ru on the hardness and fracture toughness of WC-VC-Co alloys
    Chipise, L.
    Jain, P. K.
    Cornish, L. A.
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2018, 77 : 54 - 60
  • [3] Achieving combination of high hardness and toughness for WC-8Co hardmetals by creating dual scale structured plate-like WC
    Wang, Wei
    Lu, Zhongchen
    Zeng, Meiqin
    Zhu, Min
    CERAMICS INTERNATIONAL, 2018, 44 (03) : 2668 - 2675
  • [4] Enhancing hardness and toughness of WC simultaneously by dispersed ZrO2
    Liang, Zhantao
    Liu, Xuemei
    Zhao, Zhi
    Lu, Hao
    Wang, Haibin
    Liu, Chao
    Wang, Mingsheng
    Song, Xiaoyan
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 870
  • [5] High Hardness and High Toughness WC-Fe-Ni-Cemented Carbides Prepared by Hot Oscillating Pressing
    Gao, Yang
    Deng, Sheng-Qiang
    Yang, Fang
    Sun, De-Jian
    Gao, Ka
    An, Li-Nan
    ADVANCED ENGINEERING MATERIALS, 2023, 25 (10)
  • [6] Simultaneously enhanced toughness and hardness of nanocrystalline SiC sintered under high pressure
    Sun, Rongxin
    Zhang, Xiang
    Hao, Xiaokuan
    Hu, Wentao
    Wei, Xudong
    Song, Xiaoxu
    Zhang, Zhenbang
    Ying, Pan
    Zhao, Song
    Wang, Yuefeng
    Gao, Yufei
    Yu, Dongli
    Xu, Bo
    Gao, Guoying
    Tian, Yongjun
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2025, 45 (01)
  • [7] Fracture toughness and hardness investigation in ZrB2-SiC-ZrC composite
    Rezapour, Arsalan
    Balak, Zohre
    MATERIALS CHEMISTRY AND PHYSICS, 2020, 241
  • [8] Effect of WC content on hardness and fracture toughness of WC-Ni60A wear-resistant coatings
    Wei, Min
    Li, Jing
    Xie, Kun
    Xiao, Yang-yi
    Wan, Qiang
    Yang, Zhen-ting
    Huang, Yong-jun
    Refai, Mohamed
    SURFACE & COATINGS TECHNOLOGY, 2024, 491
  • [9] High hardness-high toughness WC-20Co nanocomposites: Effect of VC variation and sintering temperature
    Kumar, Devender
    Singh, K.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 663 : 21 - 28
  • [10] Relationship between hardness and fracture toughness in WC-FeAl composites fabricated by pulse current sintering technique
    Furushima, R.
    Katou, K.
    Nakao, S.
    Sun, Z. M.
    Shimojima, K.
    Hosokawa, H.
    Matsumoto, A.
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2014, 42 : 42 - 46