The Effects of Oscillating Frequency on Microstructure and Hardness of W-Ni-Fe Refractory Alloy Sintered by Hot Oscillating Pressure

被引:1
作者
Gao, Ka [1 ]
Hu, Yanghu [2 ]
Zhang, Zixiang [1 ]
Ren, Chunyang [1 ]
Zhao, Wei [3 ]
Sun, Dejian [4 ]
Gao, Yang [4 ]
An, Linan [5 ]
Kong, Qingquan [6 ]
机构
[1] Univ Shanghai Sci & Technol, Sch Mech Engn, Shanghai 200093, Peoples R China
[2] China Natl Heavy Machinery Res Inst Co Ltd, State Key Lab Met Extrus & Forging Equipment Techn, Xian 710000, Peoples R China
[3] Changhai Hosp, Dept Gen Med, Shanghai 200000, Peoples R China
[4] Zhengzhou Univ Aeronaut, Sch Mat Sci & Engn, Zhengzhou 450015, Peoples R China
[5] Dongguan Univ Technol, Sch Mech Engn, Dongguan 523808, Peoples R China
[6] Chengdu Univ, Sichuan Prov Engn Technol Res Ctr Powder Met, Chengdu 610106, Peoples R China
基金
中国国家自然科学基金;
关键词
hardness; hot oscillating pressure; microstructure; oscillating frequency; W-Ni-Fe alloy; MECHANICAL-PROPERTIES; HEAVY ALLOYS; TUNGSTEN; DENSIFICATION; TEMPERATURE;
D O I
10.1002/adem.202301326
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
90 W-7Ni-3Fe refractory alloys are first sintered by hot oscillating pressure (HOP) under different oscillating frequencies (0, 1, and 10 Hz) in this work. The effects of oscillating frequencies on the microstructure and Vickers hardness are investigated. With the oscillating frequency increasing, the relative density and hardness of refractory alloys are obviously improved. Especially, the alloy sintered at the oscillating frequency of 10 Hz had the highest relative density of approximately 98.9% and the smallest average grain size of 3.26 mu m. Moreover, the narrowest average thickness of the bonding phase is about 0.18 mu m, and the lowest tungsten contiguity is about 61.1%. Then its excellent hardness (456.8 HV30) is obtained, which is nearly 16.1% higher than that of the 0 Hz frequency alloy. The refractory alloy with high densification, small grain size, and good hardness could be obtained by HOP with a high oscillating frequency. W-Ni-Fe refractory alloy is prepared by hot oscillating pressure at different oscillating frequencies (0, 1, and 10 Hz). The higher relative density (98.9%) and excellent hardness (456.8 HV30) of sintered alloys with the narrowest average thickness bonding phase (0.18 mu m), lowest tungsten contiguity (61.1%), and smallest grain size (3.26 mu m) are significantly improved through higher oscillating frequency applied.image (c) 2024 WILEY-VCH GmbH
引用
收藏
页数:6
相关论文
共 37 条
[31]   Microstructure and mechanical properties of spark plasma-sintered La2O3 dispersion-strengthened W–Ni–Fe alloy [J].
Muthuchamy AyyappaRaj ;
Digvijay Yadav ;
Dinesh K. Agrawal ;
Raja Annamalai Arunjunai Rajan .
Rare Metals, 2021, 40 :2230-2236
[32]   Densification, Microstructure Evolution, and Mechanical Properties of Low-Temperature-Sintered 90W-4.9Ni-2.1Fe-3Cu Alloy [J].
Zhu, Wentan ;
Liu, Wensheng ;
Ma, Yunzhu ;
Cai, Qingshan ;
Wang, Jianning ;
Duan, Youteng .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2021, 30 (04) :2761-2771
[33]   Effect of heat treatment on microstructure and mechanical properties of hot-hydrostatically extruded 93W-4.9Ni-2.1Fe alloy [J].
Yu, Yang ;
Zhang, Wencong ;
Wang, Erde .
JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 622 :880-884
[34]   PRODUCTION OF Fe-Co-Cr-Ni-Al HEAS VIA ECAS AND EFFECTS OF HEAT TREATMENT ON SINTERED ALLOY MICROSTRUCTURE [J].
Ipek, Mediha ;
Yener, Tuba ;
Zeytin, Sakin .
METAL 2017: 26TH INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS, 2017, :1625-1629
[35]   On the effect of high-temperature annealing on the microstructure and mechanical properties of a hot-rolled 90W7Ni3Fe tungsten heavy alloy [J].
Alam, M. E. ;
Haag, J. V. ;
Setyawan, W. ;
Henager Jr, C. H. ;
Odette, G. R. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 896
[36]   Microstructure and mechanical characterizations of liquid phase sintered W-Ni-Cu heavy alloy modified with La2O3 and Fe addition [J].
Shakunt, Navindra Shekhar ;
Gouthama ;
Upadhyaya, Anish .
INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2025, 127
[37]   Effects of hot-forging and subsequent annealing on microstructure and mechanical behaviors of Fe35Ni35Cr20Mn10 high-entropy alloy [J].
Zhou, Jun ;
Liao, Hengcheng ;
Chen, Hao ;
Huang, Aijing .
MATERIALS CHARACTERIZATION, 2021, 178