Fluorine-free Plasma Enhanced Atomic Layer Deposited Ultrathin Tungsten Nitride Thin Films for Dual Diffusion Barrier Performance

被引:3
作者
Seo, Kang-Min [1 ]
Mohapatra, Debananda [2 ]
Bae, Gun-Woo [1 ]
Ansari, Mohd Zahid [1 ]
Son, Yeseul [2 ]
Jang, Yujin [3 ]
Bae, Jong-Seong [3 ]
Hong, Tae Eun [3 ]
Kim, Soo-Hyun [2 ,4 ]
机构
[1] Yeungnam Univ, Sch Mat Sci & Engn, Gyongsan 38541, Gyeongbuk, South Korea
[2] Ulsan Natl Inst Sci & Technol UNIST, Grad Sch Semicond Mat & Devices Engn, Ulsan 44919, South Korea
[3] Korea Basic Sci Inst, Busan Ctr, Busan 46742, South Korea
[4] Ulsan Natl Inst Sci & Technol UNIST, Dept Mat Sci & Engn, Ulsan 44919, South Korea
关键词
atomic layer deposition; phase-tuned tungsten nitride; fluorine-free W precursor; N-2 + H-2 mixture plasma; diffusion barrier; Cu and Ru metallization; CHEMICAL-VAPOR-DEPOSITION; CONTROLLED GROWTH; WNX; PRECURSOR; SURFACE; NH3; CVD;
D O I
10.1021/acsanm.3c03956
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A vacuum deposition technique in a highly narrow device is a critical issue for fabricating barrier layers in semiconductor devices. Though tungsten nitride (WNx) thin films' uniform and conformal thickness control can be achieved via atomic layer deposition (ALD), most ALD-WNx processes use fluorine-based precursors, resulting in high resistivity with low growth rate and corrosive and toxic F-containing impurities. This study underscores the importance of the plasma-enhanced ALD (PEALD) process for WNx films via a fluorine-free inorganic WCl5 precursor and critically optimizes the counter reactant ratio (N-2 + H-2 ratio of 1:1 to 1:10), temperature ranges (200 similar to 325 degrees C), plasma mixture, plasma power, and postannealing condition process parameters. The as-grown WNx film properties and the impact of the plasma ratio on the WN phase, crystallinity, and stoichiometry were confirmed comprehensively by advanced transmission electron microscopy, spectroscopy, and diffraction techniques. Notably, secondary ion mass and photoelectron spectroscopies ensure uniformity and fewer impurity contents of O/Cl throughout the thickness of the WNx film. Significantly, the parent nanocrystalline hexagonal WN phase at a N-2 + H-2 ratio of 1:3 at 250 degrees C transformed to a crystalline cubic W2N phase with decreasing resistivity as the H-2 ratio of total N-2 + H-2 mixture plasma gas increased. The postannealed (500 degrees C) deposited WNx film demonstrated the formation of a stable cubic phase, lowering the sheet resistance with increasing deposition temperature (film thickness) and plasma ratio. The as-deposited film's diffusion barrier performance against Cu and Ru (similar to 4 nm) was evaluated to withstand up to 850 degrees C, revealing a promising dual diffusion barrier capability as interconnects in challenging shrinking semiconductor device structures.
引用
收藏
页码:21741 / 21751
页数:11
相关论文
共 35 条
  • [1] Dependence of Nitrogen/Argon Reaction Gas Amount on Structural, Mechanical and Optical Properties of Thin WNx Films
    Asgary, Somayeh
    Ramezani, Amir Hoshang
    [J]. CHINESE PHYSICS LETTERS, 2017, 34 (12)
  • [2] Highly conformal thin films of tungsten nitride prepared by atomic layer deposition from a novel precursor
    Becker, JS
    Suh, S
    Wang, SL
    Gordon, RG
    [J]. CHEMISTRY OF MATERIALS, 2003, 15 (15) : 2969 - 2976
  • [3] Diffusion barrier properties of tungsten nitride films grown by atomic layer deposition from bis(tert-butylimido)bis(dimethylamido)tungsten and ammonia
    Becker, JS
    Gordon, RG
    [J]. APPLIED PHYSICS LETTERS, 2003, 82 (14) : 2239 - 2241
  • [4] Potential of Ruthenium and Cobalt as Next-generation Semiconductor Interconnects
    Choi, Dooho
    [J]. KOREAN JOURNAL OF METALS AND MATERIALS, 2018, 56 (08): : 605 - 610
  • [5] Interface studies of tungsten nitride and titanium nitride composite metal gate electrodes with thin dielectric layers
    Claflin, B
    Binger, M
    Lucovsky, G
    [J]. JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A, 1998, 16 (03): : 1757 - 1761
  • [6] A low valent metalorganic precursor for the growth of tungsten nitride thin films by atomic layer deposition
    Dezelah, Charles L.
    El-Kadri, Oussama M.
    Kukli, Kaupo
    Arstila, Kai
    Baird, Ronald J.
    Lu, Jun
    Niinisto, Lauri
    Winter, Charles H.
    [J]. JOURNAL OF MATERIALS CHEMISTRY, 2007, 17 (11) : 1109 - 1116
  • [7] Highly Scaled Ruthenium Interconnects
    Dutta, Shibesh
    Kundu, Shreya
    Gupta, Anshul
    Jamieson, Geraldine
    Granados, Juan Fernando Gomez
    Bommels, Jurgen
    Wilson, Christopher J.
    Tokei, Zsolt
    Adelmann, Christoph
    [J]. IEEE ELECTRON DEVICE LETTERS, 2017, 38 (07) : 949 - 951
  • [8] THIN-FILM REACTION AND INTERFACE STRUCTURE OF CU ON SI
    ECHIGOYA, J
    ENOKI, H
    SATOH, T
    WAKI, T
    OHMI, T
    OTSUKI, M
    SHIBATA, T
    [J]. APPLIED SURFACE SCIENCE, 1992, 56-8 : 463 - 468
  • [9] Atomic layer deposition of WxN/TiN and WNxCy/TiN nanolaminates
    Elers, KE
    Saanila, V
    Li, WM
    Soininen, PJ
    Kostamo, JT
    Haukka, S
    Juhanoja, J
    Besling, WFA
    [J]. THIN SOLID FILMS, 2003, 434 (1-2) : 94 - 99
  • [10] Elers KE, 2002, CHEM VAPOR DEPOS, V8, P149, DOI 10.1002/1521-3862(20020704)8:4<149::AID-CVDE149>3.0.CO