New protective coatings against liquid zinc corrosion

被引:2
作者
Cieplak, Aleksandra [1 ]
Gdoura, Asma [2 ]
Gay, Bruno [3 ]
Portebois, Leo [4 ]
Ramenatte, Nicolas [4 ]
Proriol Serre, Ingrid [1 ]
Balloy, David [1 ]
机构
[1] Univ Lille, UMR 8207, CNRS, INRAE,UMET Unite Mat & Transformat,Cent Lille, F-59000 Lille, France
[2] Carthage Univ, Natl Inst Appl Sci & Technol INSAT, BP 676, Tunis 1080, Tunisia
[3] BCircle, 2 Clos 3 Couleurs, B-1150 Brussels, Belgium
[4] Univ Lorraine, EEIGM, 6 Rue Bastien Lepage, F-54010 Nancy, France
来源
SN APPLIED SCIENCES | 2023年 / 5卷 / 05期
关键词
Batch galvanizing; Molten zinc corrosion; Slurry process; WT.PERCENT B STEEL; INTERFACIAL MORPHOLOGY; STAINLESS-STEEL; AL SYSTEM; BEHAVIOR; RESISTANCE; ZN;
D O I
10.1007/s42452-023-05319-6
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
Hot dip galvanizing is a surface treatment used to form a corrosion-resistant layer on the surface of steel by dipping it in a liquid zinc bath. However, a lot of structures used for hanging or containing the parts during the process are made of steel and suffer from liquid zinc corrosion. Furthermore, Fe-Zn intermetallics formed on the surface induce an additional pickling and zinc consummation, therefore generating supplementary economic and environmental costs. In this article, two Fe-Cr-Ni-Si coatings synthetized by the slurry process on carbon steel (C22) were characterized by XRD, EDX, EPMA and EBSD analyses. Their corrosion protective properties were studied in the process imitating cyclic batch galvanizing and compared to those of uncoated carbon steel (C22) and stainless steel (316 L). The coatings were verified to be more efficient than the 316 L steel usually used for this application. After 9 cycles of no weight loss, molten zinc corrosion was linear and the same for Fe-Cr-Ni-Si coatings as for the stainless steel.
引用
收藏
页数:9
相关论文
共 29 条
  • [1] PACK CEMENTATION ALUMINIDE COATINGS ON SUPERALLOYS - CODEPOSITION OF CR AND REACTIVE ELEMENTS
    BIANCO, R
    RAPP, RA
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1993, 140 (04) : 1181 - 1190
  • [2] A high-strength silicide phase in a stainless steel alloy designed for wear-resistant applications
    Bowden, D.
    Krysiak, Y.
    Palatinus, L.
    Tsivoulas, D.
    Plana-Ruiz, S.
    Sarakinou, E.
    Kolb, U.
    Stewart, D.
    Preuss, M.
    [J]. NATURE COMMUNICATIONS, 2018, 9
  • [3] Improving the corrosion resistance of Fe-21Cr-9Mn alloy in liquid zinc by heat treatment
    Fang, Xuanwei
    Wang, Yan
    Zhang, Ying
    Feng, Shuaijie
    Du, Jingyuan
    Liu, Dawei
    Ouyang, Taoyuan
    Suo, Jinping
    Cai, Shuizhou
    [J]. CORROSION SCIENCE, 2016, 111 : 362 - 369
  • [4] Latest Developments in Suspension and Liquid Precursor Thermal Spraying
    Fauchais, Pierre
    Montavon, Ghislain
    [J]. JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2010, 19 (1-2) : 226 - 239
  • [5] Hardy Y, 2007, 7 INT C ZINC ZINC AL
  • [6] Kergar Neghab A, 2015, 10 INT C ZINC ZINC A
  • [7] Experimental Investigation of Hydrogen Embrittlement during Coating Process and Effect on Mechanical Properties of High Strength Steel used for Fasteners
    Khare, Amit
    Dwivedi, Sandeep Kumar
    Vishwakarma, Manish
    Ahmed, Siraj
    [J]. MATERIALS TODAY-PROCEEDINGS, 2018, 5 (09) : 18707 - 18715
  • [8] Development of suicide coatings to ensure the protection of Nb and suicide composites against high temperature oxidation
    Knittel, S.
    Mathieu, S.
    Portebois, L.
    Drawin, S.
    Vilasi, M.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2013, 235 : 401 - 406
  • [9] Interaction of liquid zinc with non-metallic coatings on steel
    Liberski, P
    Podolski, P
    Gierek, A
    Formanek, B
    [J]. HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 4, PTS 1 AND 2, 1997, 251-2 : 693 - 699
  • [10] Interfacial morphology and corrosion resistance of Fe-B cast steel containing chromium and nickel in liquid zinc
    Ma, Shengqiang
    Xing, Jiandong
    Fu, Hanguang
    Yi, Dawei
    Zhang, Jianjun
    Li, Yefei
    Zhang, Zhiyun
    Zhu, Baojian
    Ma, Shengchao
    [J]. CORROSION SCIENCE, 2011, 53 (09) : 2826 - 2834