Adhesive wear mechanism of coated tools and its influence on cutting performance during machining of Zr-based bulk metallic glass

被引:12
作者
Ding, Feng [1 ]
Wang, Chengyong [1 ]
Zhang, Tao [1 ]
Deng, Yang [1 ]
Zhu, Xuguang [1 ,2 ]
机构
[1] Guangdong Univ Technol, State Key Lab High Performance Tools, Guangzhou 510006, Peoples R China
[2] Dongguan Yihao Met Technol Co Ltd, Dongguan 523690, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2023年 / 27卷
基金
中国国家自然科学基金;
关键词
Zr-based bulk metallic glass; Machining; Coated tool; Adhesive wear; Cutting performance; TEMPERATURES; BEHAVIOR; ALLOYS;
D O I
10.1016/j.jmrt.2023.11.073
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Adhesive wear is the primary failure form of coated tools in zirconium-based bulk metallic glasses (Zr-based BMGs) machining. This work investigated the adhesion formation and failure of TiN/Al2O3/Ti(C,N), Al2O3/Ti(C, N), and TiAlN-coated tools when machining Zr41.2Ti13.8Cu10Ni12.5Be22.5 BMG. Characterization of tool-chip interfacial material responses revealed the mechanism of adhesive wear. The relationship between the wear resistance and micro-mechanical properties of coatings was established. The cutting performance of coated tools is also discussed. According to the results, the adhesive wear of coated tools results because the temperature at the tool-chip interface is above the glass transition temperature, reducing the viscosity of chips. Low-viscosity chips were welded to the tool surface under high pressure. Subsequently, high interfacial friction tore the ad-hesive interface, causing coatings to peel off layer by layer. The exposed tool substrate also generated secondary adhesion, which triggered the diffusion of tungsten and cobalt atoms towards the chip. This was accompanied by redox reactions that exacerbated tool failure. The wear resistance of coatings depended on the elastic modulus (E) and the ratio of nano hardness to elastic modulus (H/E). The TiAlN coating had a lower E of-410 GPa and higher H/E of 0.064, and it exhibited better wear resistance than the TiN/Al2O3/Ti(C,N) (E -436 GPa, H/E = 0.051) and Al2O3/Ti(C,N) (E -469 GPa, H/E = 0.061) coatings. The lifespan of the TiAlN-coated tool was more than three times longer that of the other two, and the obtained machined surface roughness was less than half that of the others.
引用
收藏
页码:5489 / 5506
页数:18
相关论文
共 49 条
  • [1] Chip formation, cutting forces, and tool wear in turning of Zr-based bulk metallic glass
    Bakkal, M
    Shih, AJ
    Scattergood, RO
    [J]. INTERNATIONAL JOURNAL OF MACHINE TOOLS & MANUFACTURE, 2004, 44 (09) : 915 - 925
  • [2] Light emission, chip morphology, and burr formation in drilling the bulk metallic glass
    Bakkal, M
    Shih, AJ
    McSpadden, SB
    Liu, CT
    Scattergood, RO
    [J]. INTERNATIONAL JOURNAL OF MACHINE TOOLS & MANUFACTURE, 2005, 45 (7-8) : 741 - 752
  • [3] Oxidation and crystallization of Zr-based bulk metallic glass due to machining
    Bakkal, M
    Liu, CT
    Watkins, TR
    Scattergood, RO
    Shih, AJ
    [J]. INTERMETALLICS, 2004, 12 (02) : 195 - 204
  • [4] Machining of a Zr-Ti-Al-Cu-Ni metallic glass
    Bakkal, M
    Shih, AJ
    Scattergood, RO
    Liu, CT
    [J]. SCRIPTA MATERIALIA, 2004, 50 (05) : 583 - 588
  • [5] The influence of the H/E ratio on wear resistance of coating systems - Insights from small-scale testing
    Beake, Ben D.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2022, 442
  • [6] Effect of TiN, TiAlCN, AlCrN, and AlTiN ceramic coatings on corrosion behavior of tungsten carbide tool
    Bilgin, Sumran
    Guler, Onur
    Alver, Umit
    Erdemir, Fatih
    Aslan, Mustafa
    Canakci, Aykut
    [J]. JOURNAL OF THE AUSTRALIAN CERAMIC SOCIETY, 2021, 57 (01) : 263 - 273
  • [7] Properties and performance of commercial TiCN coatings. Part 2: tribological performance
    Bull, SJ
    Bhat, DG
    Staia, MH
    [J]. SURFACE & COATINGS TECHNOLOGY, 2003, 163 : 507 - 514
  • [8] Micro-machinability of bulk metallic glass in ultra-precision cutting
    Chen, Xiao
    Xiao, Junfeng
    Zhu, Yan
    Tian, Ruiji
    Shu, Xuewen
    Xu, Jianfeng
    [J]. MATERIALS & DESIGN, 2017, 136 : 1 - 12
  • [9] A review on microstructures and mechanical properties of protective nano-multilayered films or coatings
    Cheng, Wenjie
    Wang, Jingjing
    Ma, Xun
    Liu, Ping
    Liaw, Peter K.
    Li, Wei
    [J]. JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 27 : 2413 - 2442
  • [10] Synthesis and characterization of particulate reinforced Zr57Nb5Al10Cu15.4Ni12.6 bulk metallic glass composites
    Choi-Yim, H
    Busch, R
    Köster, U
    Johnson, WL
    [J]. ACTA MATERIALIA, 1999, 47 (08) : 2455 - 2462