Evaluation of the Healing Performance of Hot-Mix Asphalt Containing Waste Steel Shavings under Different Microwave Induction Healing Cycles

被引:2
作者
Alikhani, Hadi [1 ]
Latifi, Manouchehr [2 ]
机构
[1] Univ Tehran, Coll Engn, Sch Civil Engn, Tehran 1417954495, Iran
[2] Univ Tehran, Coll Engn, Sch Civil Engn, Tehran 1417613131, Iran
关键词
Asphalt healing; Microwave heating induction; Waste steel shavings (WSS); Overheating in healing; Intermittent heating; CONCRETE; MIXTURES; VISCOSITY; FRACTURE; BITUMEN; SLAG;
D O I
10.1061/JCEMD4.COENG-13904
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Increasing the temperature affects the healing potential of asphalt mixtures significantly. However, it can lead to overheating in some parts of the specimens and cause damage. Thus, the healing temperature should be decreased in order to reduce the risk of overheating, which can affect the healing performance adversely. This research aims to investigate the probability of local overheating in asphalt mixtures during the induction heating of the mixtures containing different percentages of waste steel shavings (WSS). The healing procedure of the mixtures was simulated by placing the fractured hot-mix asphalt samples in a microwave so that the fractured surfaces are healed and stuck together. The healing resistance was evaluated by conducting the fracture test on the healed specimens and comparing the results to those of the intact specimens. The results showed that increasing the healing temperature to more than 70 degrees C and the existence of WSS additives increase the probability of overheating in asphalt mixtures. The results indicated that the intermittent heating is effective to reduce the risk of overheating. As the healing procedure accelerates when the temperature increases to more than the softening point, it is recommended that, during intermittent heating, the samples should be cooled down to the temperature of the softening point during the rest period so that the temperature of the sample does not fall below the softening point of the bitumen during healing. By doing this, in addition to reducing the risk of overheating, the healing performance improves without increasing energy consumption.
引用
收藏
页数:10
相关论文
共 63 条
  • [1] AASHTO, 2022, T84 AASHTO
  • [2] AASHTO, 2015, Standard method of test for determining the fracture energy of asphalt mixtures using the semi-circular bend geometry (SCB)
  • [3] AASHTO, 2022, Standard practice for laboratory conditioning of asphalt mixtures
  • [4] AASHTO, 2019, AASHTO T 96-02
  • [5] AASHTO, 2022, AASHTO t 85, standard method of test for specific gravity and absorption of coarse aggregate
  • [6] AASHTO, 2022, Standard method of test for soundness of aggregate by use of sodium sulfate or magnesium sulfate
  • [7] AASHTO, 2022, AASHTO T 228
  • [8] AASHTO, 2022, Standard practice for superpave volumetric design for asphalt mixtures
  • [9] Self-Healing of Dense Asphalt Concrete by Two Different Approaches: Electromagnetic Induction and Infrared Radiation
    Ajam, H.
    Lastra-Gonzalez, P.
    Gomez-Meijide, B.
    Airey, G.
    Garcia, A.
    [J]. JOURNAL OF TESTING AND EVALUATION, 2017, 45 (06) : 1933 - 1940
  • [10] Mechanical and healing properties of asphalt mixes reinforced with different types of waste and commercial metal particles
    Ajam, Harith
    Gomez-Meijide, Breixo
    Artamendi, Ignacio
    Garcia, Alvaro
    [J]. JOURNAL OF CLEANER PRODUCTION, 2018, 192 : 138 - 150