Sulfur-Rich Additive-Induced Interphases Enable Highly Stable 4.6 V LiNi0.5Co0.2Mn0.3O2||graphite Pouch Cells

被引:40
作者
Fan, Ziqiang [1 ,2 ,3 ]
Zhou, Xunzhu [1 ,4 ]
Qiu, Jingwei [2 ,3 ]
Yang, Zhuo [1 ,4 ]
Lei, Chenxi [2 ,3 ]
Hao, Zhiqiang [1 ,4 ]
Li, Jianhui [2 ,3 ,5 ]
Li, Lin [1 ,4 ]
Zeng, Ronghua [2 ,3 ]
Chou, Shu-Lei [1 ,4 ]
机构
[1] Wenzhou Univ, Dept Inst Carbon Neutralizat, Coll Chem & Mat Engn, Wenzhou 325035, Zhejiang, Peoples R China
[2] South China Normal Univ, Engn Res Ctr MTEES, Minist Educ,Sch Chem, Dept Natl & Local Joint Engn, Guangzhou 510006, Guangdong, Peoples R China
[3] South China Normal Univ, Sch Chem, Key Lab ETESPG GHEI, Guangzhou 510006, Guangdong, Peoples R China
[4] Wenzhou Univ Technol Innovat, Inst Carbon Neutralizat, Wenzhou Key Lab Sodium Ion Batteries, Wenzhou 325035, Zhejiang, Peoples R China
[5] South China Normal Univ, Sch Mat & New Energy, Shanwei 516600, Guangdong, Peoples R China
基金
中国国家自然科学基金;
关键词
Electrode-Electrolyte Interface; High Energy Density; High-Voltage; Lithium-Ion Batteries; Sulfur-Rich Additive; HIGH-VOLTAGE PERFORMANCE; METHYLENE METHANEDISULFONATE; LICOO2/GRAPHITE BATTERIES; ELECTROLYTE ADDITIVES; FUNCTIONAL ADDITIVES; PROPYLENE CARBONATE; LITHIUM; OXIDE; SULTONE; IMPACT;
D O I
10.1002/anie.202308888
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
High-voltage lithium-ion batteries (LIBs) have attracted great attention due to their promising high energy density. However, severe capacity degradation is witnessed, which originated from the incompatible and unstable electrolyte-electrode interphase at high voltage. Herein, a robust additive-induced sulfur-rich interphase is constructed by introducing an additive with ultrahigh S-content (34.04 %, methylene methyl disulfonate, MMDS) in 4.6 V LiNi0.5Co0.2Mn0.3O2 (NCM523)||graphite pouch cell. The MMDS does not directly participate the inner Li+ sheath, but the strong interactions between MMDS and PF6- anions promote the preferential decomposition of MMDS and broaden the oxidation stability, facilitating the formation of an ultrathin but robust sulfur-rich interfacial layer. The electrolyte consumption, gas production, phase transformation and dissolution of transition metal ions were effectively inhibited. As expected, the 4.6 V NCM523||graphite pouch cell delivers a high capacity retention of 87.99 % even after 800 cycles. This work shares new insight into the sulfur-rich additive-induced electrolyte-electrode interphase for stable high-voltage LIBs.
引用
收藏
页数:9
相关论文
共 61 条
[61]   High-voltage performance of LiCoO2/graphite batteries with methylene methanedisulfonate as electrolyte additive [J].
Zuo, Xiaoxi ;
Fan, Chengjie ;
Xiao, Xin ;
Liu, Jiansheng ;
Nan, Junmin .
JOURNAL OF POWER SOURCES, 2012, 219 :94-99