Weak Magnetic Internal Signal Characteristics of Pipe Welds under Internal Pressure

被引:3
|
作者
Liu, Bin [1 ]
Fu, Yanduo [1 ]
He, Luyao [1 ]
Geng, Hao [1 ]
Yang, Lijian [1 ]
机构
[1] Shenyang Univ Technol, Sch Informat Sci & Engn, Shenyang 110870, Peoples R China
基金
中国国家自然科学基金;
关键词
pipeline weak magnetic stress; simulation analysis; energy factor; experimental test; DEFECT; STEEL;
D O I
10.3390/s23031147
中图分类号
O65 [分析化学];
学科分类号
070302 ; 081704 ;
摘要
Weak magnetic detection technology is an effective method to identify stress-induced damage to ferromagnetic materials, and it especially possesses great application potential in long-distance oil and gas pipeline weld crack detection. In the process of pipeline operation, due to internal pressure and external loads, local stress concentration may be generated, and partial stress concentration may lead to local cracks and expansion of the pipe. In order to improve the accuracy of magnetic signal analysis for ferromagnetic materials under internal pressure, the causes of magnetic signal generation at pipeline welds were analyzed from a microscopic perspective. The distributions of magnetic signals at pipeline welds, weld cracks, and base metal cracks under different internal pressures were numerically analyzed. The variation trends of magnetic signal characteristics, such as peak values of axial and radial components, gradient K, maximum gradient Kmax, and gradient energy factor S(K), were analyzed. In addition, experiments were carried out to verify the numerical data. It was revealed that with the elevation of internal pressure, the peak values of the axial and radial components, gradient K, maximum gradient Kmax, and gradient energy factor S(K) linearly increased. However, the magnitude and average change of S(K) were larger, which can more directly indicate variations of magnetic signals. The radial growth rate nu(y) of S(K) was 3.24% higher than the axial growth rate nu(x), demonstrating that the radial component of the magnetic signal was more sensitive to variations of stress. This study provided a theoretical and experimental basis for detection of stress-induced damage to long-distance oil and gas pipelines.
引用
收藏
页数:27
相关论文
共 50 条
  • [31] Hoop Membrane Stress Analysis of Elbow-Pipe under Single Internal Pressure
    Hong, Li Xiao
    MECHANICAL AND ELECTRONICS ENGINEERING III, PTS 1-5, 2012, 130-134 : 1785 - 1788
  • [32] Exploring Weak Magnetic Signal Characteristics of Pipeline Welds: Insights into Stress Non-Uniformity Effects
    Fan, Xiangfeng
    Yang, Lijian
    SENSORS, 2024, 24 (15)
  • [33] Fracture mechanics study of cracked pipe bends under internal pressure and bending moments
    Joglekar, Manish. M.
    Joshi, S. G.
    Dutta, B. K.
    Proceedings of the 8th Biennial Conference on Engineering Systems Design and Analysis, Vol 4, 2006, : 89 - 98
  • [34] Plastic collapse of pipe bends under combined internal pressure and in-plane bending
    Robertson, A
    Li, HJ
    Mackenzie, D
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2005, 82 (05) : 407 - 416
  • [35] APPROXIMATE ELASTIC STRESSES IN A TEE BRANCH PIPE CONNECTION UNDER INTERNAL-PRESSURE
    UPDIKE, DP
    JOURNAL OF PRESSURE VESSEL TECHNOLOGY-TRANSACTIONS OF THE ASME, 1981, 103 (01): : 104 - 107
  • [36] A new fluid-structure coupling model: Case of a pipe under internal pressure
    Hicham, Fakiri
    Abdelhamid, Hadjoui
    ADVANCES IN MECHANICAL ENGINEERING, 2023, 15 (05)
  • [37] Development of method of pipe expansion with drawing for improving the fatigue property under internal pressure
    Sumimoto, D
    Ichihara, H
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2001, 87 (10): : 650 - 656
  • [38] Effect of internal pressure on the flexural fatigue behaviour of trenchless internal replacement pipe systems
    Kiriella, Shanika
    Manalo, Allan
    Tien, Cam Minh Tri
    Ahmadi, Hamid
    Karunasena, Warna
    Dixon, Patrick G.
    Salah, Ahmad
    Wham, Brad P.
    TUNNELLING AND UNDERGROUND SPACE TECHNOLOGY, 2024, 154
  • [39] Limiting Plastic Load in a Pressure Vessel with a Branch Pipe under Combined Internal Pressure and Bending Moments
    Skopinskii V.N.
    Berkov N.A.
    Vozhova N.V.
    Smetankin A.B.
    Skopinskii, V. N. (svn46_46@mail.ru), 1600, Springer Science and Business Media, LLC (49): : 549 - 554
  • [40] Sudden Suppression of Internal Magnetic Fields under High Pressure in α-Mn
    Ito, Tomoaki
    Fukazawa, Hideto
    Shioda, Naoki
    Kataoka, Yuki
    Ohama, Tetsuo
    Kohori, Yoh
    JOURNAL OF THE PHYSICAL SOCIETY OF JAPAN, 2021, 90 (08)