Production of thick-walled hollow glass microspheres for inertial confinement fusion targets by sol-gel technology

被引:1
作者
GAO Cong 1
2 School of Chemical Engineering
机构
关键词
hollow glass microsphere; dried-gel method; inertial confinement fusion; target fabrication;
D O I
暂无
中图分类号
TB302 [工程材料试验];
学科分类号
0805 ; 080502 ;
摘要
To fabricate thick-walled hollow glass microspheres(HGMs)for inertial confinement fusion(ICF)targets by sol-gel technology,we investigated the effects of glass composition,blowing agent,refining temperature,pressure and composition of furnace atmosphere on the wall thickness of HGMs by numerical simulation and experiments.The results showed that the residence times of the thick-walled HGMs in the encapsulating and refining phases decreased with the increase of wall thickness of HGMs.As a response to this challenge,glass composition must be optimized with the object of high surface tension and low viscosity at refining temperature,and the blowing agents with high decomposition temperature should be used,furthermore the concentration of blowing agents in gel particles must also be precisely controlled.The higher volume fraction of argon gas in the furnace atmosphere,the thicker the wall of HGMs.Due to the limited operating range of furnace atmosphere pressure,changing furnace atmosphere pressure could not significantly increase the wall thickness of HGMs.Although increasing refining temperature can improve the yield of high quality HGMs,a higher furnace atmosphere temperature may lead to a decrease in the wall thickness of HGMs.When the volume fraction of argon gas in the furnace atmosphere ranged from 80%to 95%,the furnace atmosphere pressure ranged from 1.0×105Pa to 1.25×105 Pa,and the refining temperature ranged from 1600°C to 1800°C,we produced thick-walled(5–10-m)HGMs with good sphericity,wall thickness uniformity and surface finish.However,the yield of high quality HGMs needs to be further improved.The compressive strength,tensile strength and permeation coefficient to deuterium gas of thick-walled HGMs at ambient temperature decreased with increase of the wall thickness.
引用
收藏
页码:2377 / 2385
页数:9
相关论文
共 13 条
  • [1] 干凝胶法制备空心玻璃微球的炉内成球过程分析
    漆小波
    魏胜
    张占文
    李波
    陈素芬
    师涛
    [J]. 原子能科学技术, 2010, 44 (11) : 1371 - 1375
  • [2] 载气压力对空心玻璃微球炉内成球过程的影响
    漆小波
    李波
    陈素芬
    张占文
    师涛
    [J]. 原子能科学技术, 2010, 44 (09) : 1065 - 1070
  • [3] 载气组份对空心玻璃微球炉内成球过程的影响
    漆小波
    魏胜
    张占文
    李波
    陈素芬
    师涛
    [J]. 强激光与粒子束, 2010, 22 (07) : 1543 - 1547
  • [4] 干凝胶法制备惯性约束聚变靶用大直径空心玻璃微球
    漆小波
    李波
    陈素芬
    张占文
    师涛
    初巧妹
    [J]. 硅酸盐学报, 2010, 38 (04) : 718 - 724
  • [5] 干凝胶法制备空心玻璃微球炉内成球过程的数值模拟
    漆小波
    张占文
    李波
    陈素芬
    师涛
    [J]. 过程工程学报, 2010, 10 (01) : 109 - 114
  • [6] 玻璃微球壁厚和预充气工艺对气体渗透性能的影响
    张占文
    李波
    唐永建
    王朝阳
    漆小波
    陈素芬
    刘一杨
    翟世明
    [J]. 强激光与粒子束, 2006, (06) : 957 - 960
  • [7] 用于ICF靶的空心玻璃微球的干凝胶法制备附视频
    漆小波
    唐永建
    李波
    陈素芬
    师韬
    张占文
    林波
    初巧妹
    [J]. 强激光与粒子束, 2006, (01) : 55 - 60
  • [8] 激光聚变靶用空心玻璃微球的成分设计
    漆小波
    唐永建
    李波
    张占文
    师涛
    [J]. 玻璃与搪瓷, 2005, (06) : 34 - 40
  • [9] Hollow glass microsphere production for laser direct-driven fusion targets on Shen Guang Ⅱ
    邱龙会
    魏芸
    姚书久
    傅依备
    郑永铭
    唐永建
    师韬
    [J]. Science China Mathematics, 2002, (03) : 371 - 377
  • [10] 液滴法制备空心玻璃微球的过程分析
    邱龙会
    魏芸
    唐永建
    傅依备
    郑永铭
    师韬
    [J]. 原子能科学技术, 2001, (01) : 60 - 64