摘要
The shear responses of β-SiC are investigated using molecular dynamics simulation with the Tersoff interatomic potential. Results show a clear decreasing trend in critical stress,fracture strain and shear modulus as temperature increases. Above a critical temperature, β-SiC bulk just fractures after the elastic deformation. However, below the critical temperature, an interesting pattern in β-SiC bulk emerges due to the elongation of Si-C bonds before fracture. Additionally, the shear deformation of β-SiC at room temperature is found to be dependent on the strain rate. This study may shed light on the deformation mechanism dependent on temperature and strain rate.
引用
收藏
页码:137 / 144
页数:8
相关论文
共 21 条
[11]  
Simple scheme for deriving atomic force constants:Application to Si C .2 Lee DH,Joannopoulos JD. Phys Rev Lett . 1982
[12]  
A space–time multilevel method for molecular dynamics simulations[J] . Haim Waisman,Jacob Fish.Computer Methods in Applied Mechanics and Engineering . 2006 (44)
[13]   Ultrahigh-temperature materials for jet engines [J].
Zhao, JC ;
Westbrook, JH .
MRS BULLETIN, 2003, 28 (09) :622-630
[14]  
Three strategies to achieve uniform tensile deformation in a nanostructured metal[J] . Y.M. Wang,E. Ma.Acta Materialia . 2003 (6)
[15]  
Characterization of defects in 3C-silicon carbide crystals[J] . William M. Vetter,Michael Dudley.Journal of Crystal Growth . 2003 (1)
[16]   Joining of sintered silicon carbide ceramics for high-temperature applications [J].
Singh, M .
JOURNAL OF MATERIALS SCIENCE LETTERS, 1998, 17 (06) :459-461
[17]  
Atomistic modeling of finite-temperature properties of β-SiC. I. Lattice vibrations, heat capacity, and thermal expansion[J] . Lisa J. Porter,Ju Li,Sidney Yip.Journal of Nuclear Materials . 1997 (1)
[18]  
Penetration of confined silicon carbide targets by tungsten long rods at impact velocities from 1.5 to 4.6 km/s[J] . D.L. Orphal,R.R. Franzen.International Journal of Impact Engineering . 1996 (1)
[19]   FAST PARALLEL ALGORITHMS FOR SHORT-RANGE MOLECULAR-DYNAMICS [J].
PLIMPTON, S .
JOURNAL OF COMPUTATIONAL PHYSICS, 1995, 117 (01) :1-19
[20]   THERMAL-EXPANSION OF THE CUBIC (3C) POLYTYPE OF SIC [J].
LI, Z ;
BRADT, RC .
JOURNAL OF MATERIALS SCIENCE, 1986, 21 (12) :4366-4368