Effect of BNNTs/matrix interface tailoring on toughness and fracture morphology of hierarchical SiCf/SiC composites

被引:0
|
作者
Guangxiang ZHU [1 ,2 ,3 ]
Qian FENG [4 ]
Jinshan YANG [1 ,2 ]
Jianbao HU [1 ,2 ]
Hongda WANG [1 ,2 ]
Yudong XUE [1 ,2 ,3 ]
Qingliang SHAN [1 ,2 ,3 ]
Shaoming DONG [1 ,2 ]
机构
[1] State Key Laboratory of High Performance Ceramics and Superfine Microstructure, Shanghai Institute of Ceramics, Chinese Academy of Sciences
[2] Structural Ceramics and Composites Engineering Research Center, Shanghai Institute of Ceramics, Chinese Academy of Sciences
[3] Analysis and Testing Center, Donghua University
[4] University of Chinese Academy of Sciences
基金
中国国家自然科学基金;
关键词
boron nitride nanotubes(BNNTs); interface; nanocomposites; toughness and toughening;
D O I
暂无
中图分类号
TB33 [复合材料];
学科分类号
0805 ; 080502 ;
摘要
A thin BN interphase is applied on BNNTs surface to tailor the interfacial bonding between BNNTs and SiC matrix in hierarchical SiCf/SiC composites. The thickness of BN interphase ranging from 10 to 70 nm can be optimized by chemical vapor deposition after BNNTs are in situ grown on SiC fiber surface. Without BN interphase, the fracture toughness of hierarchical Si Cf/Si C composites can be impaired by 13.6% due to strong interfacial bonding. As long as BN interphase with 30–45 nm thickness is applied, the interfacial bonding can be optimized and fracture toughness of hierarchical composites can be improved by 27.3%. It implies that tailoring BNNTs/matrix interface by depositing a layer of BN interphase is in favor of activating energy dissipation mechanisms at nanoscale induced by BNNTs.
引用
收藏
页码:555 / 563
页数:9
相关论文
共 50 条
  • [31] Effect of irradiation on thermal expansion of SiCf/SiC composites
    Senor, D.J.
    Trimble, D.J.
    Newsome, G.A.
    Woods, J.J.
    Ceramic Engineering and Science Proceedings, 1997, 18 (3 A): : 591 - 598
  • [32] Effect of loading rate on the strength of SiCf/SiC composites
    Stockmann, YJ
    Futakawa, M
    Komiya, S
    Tanabe, Y
    Kogawa, H
    Hino, R
    Mitsuno, S
    CERAMIC MATERIAL SYSTEMS WITH COMPOSITE STRUCTURES: TOWARDS OPTIMUM INTERFACE CONTROL AND DESIGN, 1998, : 357 - 369
  • [33] Effect of PyC Interface Thickness on the Heat-stability of Cansas-Ⅱ SiCf/SiC Composites
    韩笑
    于国强
    张盛
    SHI Jian
    GAO Xiguang
    SONG Yingdong
    WANG Fang
    Journal of Wuhan University of Technology(Materials Science), 2023, 38 (04) : 725 - 734
  • [34] Effect of interface types on the heat-resistance of Cansas-II SiCf /SiC composites
    Han, Xiao
    Chen, Xihui
    Niu, Xuming
    Sun, Zhigang
    Song, Yingdong
    CERAMICS INTERNATIONAL, 2022, 48 (01) : 744 - 753
  • [35] Fracture toughness of SiCf/Ti-6Al-4V composites
    Yang, Yan-Qing
    Luo, Xian
    Huang, Bin
    Li, Jian-Kang
    Chen, Yan
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2010, 31 (09): : 1 - 4
  • [36] Effect of friction between fiber and matrix on the fracture toughness of the composite interface
    Dibenedetto, AT
    Gurvich, MR
    JOURNAL OF MATERIALS SCIENCE, 1998, 33 (16) : 4239 - 4248
  • [37] Effects of silicon ion irradiation on the interface properties of SiCf/SiC composites
    Chai, Yuxin
    Zhang, Huayu
    Zhou, Xingui
    Zhang, Yumin
    CERAMICS INTERNATIONAL, 2018, 44 (02) : 2165 - 2169
  • [38] Effect of friction between fiber and matrix on the fracture toughness of the composite interface
    A. T. Dibenedetto
    M. R. Gurvich
    Journal of Materials Science, 1998, 33 : 4239 - 4248
  • [39] Damage evolution and fracture in SiCf/SiC ceramic matrix composite specimens
    Newton C.D.
    Jones J.P.
    Bache M.R.
    Quiney Z.
    Chamberlain A.L.
    2018, Wiley Blackwell (263): : 297 - 310
  • [40] Interface instability of SiCf-reinforced superalloy matrix composites
    Wang, Fa
    Jiang, He
    Yao, Zhihao
    Dong, Jianxin
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 917