Tribology of WC reinforced SiC ceramics: Influence of counterbody

被引:0
|
作者
Sandan Kumar SHARMA [1 ]
B.Venkata MANOJ KUMAR [1 ]
Young-Wook KIM [2 ]
机构
[1] Department of Metallurgical and Materials Engineering,Indian Institute of Technology (IIT) Roorkee
[2] TriboCeramics Laboratory,Department of Materials Science and Engineering,the University of Seoul
基金
新加坡国家研究基金会;
关键词
silicon carbide; tungsten carbide; composites; steel; sliding wear; counterbody;
D O I
暂无
中图分类号
TB33 [复合材料];
学科分类号
0805 ; 080502 ;
摘要
Hot pressed silicon carbide(SiC) composites prepared with 0, 10, 30 or 50 wt% tungsten carbide(WC) are subjected to dry sliding wear against WC-Co and steel ball. In particular an attempt has been made to answer the following important questions:(i) How does the load(from 5 to 20 N) effect sliding wear behaviour of SiC-ceramics against WC-Co and steel counterbodies?(ii) Is there any effect of WC content on friction and wear characteristics of SiC ceramics?(iii) Does the dominant material removal mechanism of SiC ceramics change with the addition of WC or counterbody?(iv) What is the influence of mechanical properties on the sliding wear? Experimental results indicated that coefficient of friction(COF) for the SiC ceramics varied between 0.66 and 0.33 with change in load and counterbodies. Wear volume for SiC ceramics found approximately 6-10 times more against WC-Co as compared against steel. Wear volume changes from 2.0 × 10mm~3 to 1.2 × 10mm~3 with change in counterbodies for SiC -(10, 30 or 50 wt%) WC composite at 20 N. SiC ceramics indicated abrasion and composites reveal tribochemical wear as major material removal mechanisms. Wear is influenced by the hardness of counterbody and fracture toughness of SiC -WC composites.
引用
收藏
页码:129 / 142
页数:14
相关论文
共 50 条
  • [41] Enhanced electromagnetic microwave absorption of SiC nanowire-reinforced PDC-SiC ceramics catalysed by rare earth
    Feng, Pei
    Wei, Hanjun
    Shang, Peng
    Shi, Yuhua
    Wei, Xiaolong
    Luo, Sihai
    Liang, Xiaoqiang
    Zhang, Wenyuan
    Yu, Yaping
    He, Weifeng
    CERAMICS INTERNATIONAL, 2022, 48 (17) : 24915 - 24924
  • [42] Preparation and characterization of high hard and high tough ultrafine WC ceramics containing hybrid graphene and SiC nanowire
    Shen, Xue-hui
    Xu, Nan
    Su, Hao
    He, Xiang-ping
    He, Jian-qun
    JOURNAL OF CENTRAL SOUTH UNIVERSITY, 2024, 31 (01) : 114 - 126
  • [43] Influence of microstructural variation on fracture toughness of LPS-SiC ceramics
    Strecker, K
    Ribeiro, S
    Oberacker, R
    Hoffmann, MJ
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2004, 22 (4-5) : 169 - 175
  • [44] SLIDING WEAR BEHAVIOR OF SIC WHISKER-REINFORCED ALUMINUM COMPOSITE
    IWAI, Y
    YONEDA, H
    HONDA, T
    WEAR, 1995, 181 : 594 - 602
  • [45] Effects of Cr3C2 and V8C7 on the Microstructure and Mechanical Properties of WC-SiC Whisker Ceramics
    Taimatsu, Hitoshi
    Sugiyama, Shigeaki
    Komatsu, Masanori
    MATERIALS TRANSACTIONS, 2009, 50 (10) : 2435 - 2440
  • [46] Influence of SiC addition on tribological properties of SiAlON
    Mallik, Awadesh Kumar
    Reddy, K. Madhav
    Acikbas, Nurcan Calis
    Kara, Ferhat
    Mandal, Hasan
    Basu, Debabrata
    Basu, Bikramjit
    CERAMICS INTERNATIONAL, 2011, 37 (07) : 2495 - 2504
  • [47] Study of tribological properties of polymer derived ZrB2-SiC ceramics
    He, Jiabei
    Cao, Yejie
    Li, Zhenbao
    Wang, Yiguang
    CERAMICS INTERNATIONAL, 2018, 44 (13) : 15627 - 15630
  • [48] Self lubrication of pressureless sintered SiC ceramics
    Zhang, Wei
    Yamashita, Seiji
    Kita, Hideki
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2020, 9 (06): : 12880 - 12888
  • [49] Microstructure and mechanical properties of SiC/SiC joints reinforced by in-situ growth SiC nanowires
    Tang, Mao
    Liu, Yan
    Liu, Leimin
    Lin, Tiesong
    Liu, Xuejian
    MATERIALS CHARACTERIZATION, 2021, 179
  • [50] Sliding wear resistance of biomorphic SiC ceramics
    Vera, M. C.
    Ramirez-Rico, J.
    Martinez-Fernandez, J.
    Singh, M.
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2015, 49 : 327 - 333